journal article·2025-09

Ultra-fast laser scanning achieves high-strength joining of glass and Al/Al-Alloys

Youfu Wang, Longfei Mi, Xiaowen Qi, Xiaolong Fang, Chengling Liu, Hongtao Cui

Ceramics International· Volume 51· Issue 22
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. In situ characterization of residual stress in glass-to-metal seal10.1016/j.ceramint.2019.06.259 ↗
2. Glass to aluminum joining by forming a mechanical pin structure using femtosecond laser10.1016/j.jmatprotec.2022.117504 ↗
3. Design, contributions of mechanical bonding and chemical bonding to high-temperature hermeticity of glass-to-metal compression seals10.1016/j.matdes.2021.109579 ↗
4. Towards high-temperature applications of aluminium alloys enabled by additive manufacturing10.1080/09506608.2021.1951580 ↗
5. Mechanical performance and design of aluminium alloy beam string structures10.1016/j.tws.2024.111798 ↗
6. Aluminium alloys as structural material: a review of research10.1016/j.engstruct.2020.111372 ↗
7. Tensile and fatigue properties of single lap joints of aluminium alloy/glass fibre reinforced composites fabricated with different joining methods10.1016/j.compstruct.2018.06.003 ↗
8. Recent developments in advanced aircraft aluminium alloys10.1016/j.matdes.2013.12.002 ↗
9. Laser lap joining of dissimilar materials: a review of factors affecting joint strength
10. TiO2-SiO2 mixed oxide deposited by low pressure PECVD: insights on optical and nanoscale electrical properties10.1016/j.apsusc.2020.148510 ↗
11. Optimized solder alloy for glass-to-metal joints by simultaneous soldering and anodic bonding10.1016/j.jmatprotec.2016.05.017 ↗
12. Active metal brazing for joining glass-ceramic to Titanium—A study on silver enrichment10.1007/BF00134327 ↗
13. High-strength joining of silica glass and 2024 aluminum alloy by ultrasonic-assisted soldering with Sn-Bi low temperature solder10.1016/j.jmapro.2023.07.010 ↗
14. A new sealing technology for ultra-thin glass to aluminum alloy by laser transmission welding method10.1007/s00170-021-07226-9 ↗
15. Direct microwelding of dissimilar glass and kovar alloy without optical contact using femtosecond laser pulses10.1007/s11771-022-5091-9 ↗
16. Enhanced joint through significant diffusion and molten pool regions in fused silica to aluminum alloy welding by femtosecond mJ-pulses10.1007/s00170-023-12325-w ↗
17. The characteristics and dynamics of fused silica-aluminum alloy welding during mJ-level femtosecond laser10.1016/j.matdes.2024.112790 ↗
18. Transmission laser welding of similar and dissimilar semiconductor materials10.1002/lpor.202200208 ↗
19. Picosecond laser seal welding of glasses with a large gap10.1364/OE.27.030297 ↗
20. Direct joining of quartz glass and copper by nanosecond laser10.1016/j.ceramint.2023.08.285 ↗
21. Mechanism and optimization of femtosecond laser welding fused silica and aluminum10.1016/j.apsusc.2023.158327 ↗
22. Microstructures and mechanical properties of copper-to-glass laser transmission welding employing a nanosecond pulsed laser10.1016/j.ceramint.2024.03.291 ↗
23. Effects of laser power on the interfacial intermetallic compounds and mechanical properties of dual-spot laser welded-brazed Ti/Al butt joint10.1016/j.optlastec.2019.105987 ↗
24. Investigation of laser welding on butt joints of Al/steel dissimilar materials10.1016/j.matdes.2015.05.069 ↗
25. Migration behavior of IMC layer in twin-spot laser welding-brazing of aluminum to steel10.1016/j.matdes.2020.108489 ↗
26. Microstructural evolution and its effect on joint strength during laser welding of dual phase steel to aluminium alloy10.1016/j.jmapro.2020.08.004 ↗
27. Effect of activating flux Cr2O3 on microstructure and properties of laser welded 5083 aluminum alloys10.1016/j.optlastec.2022.107930 ↗
28. Glass to aluminum joining by forming a mechanical pin structure using femtosecond laser10.1016/j.jmatprotec.2022.117504 ↗
29. An experimental study of the effects of surface roughness and coating of Cr2O3 layer on the laser-forming process10.1016/j.optlastec.2018.07.064 ↗
30. Effect of high-temperature oxidation on laser transmission welding of high borosilicate glass and TC4 titanium alloy
31. Capacity fading mechanism of Li2O loaded NiFe2O4/SiO2 aerogel anode for lithium-ion battery: ex-Situ XPS analysis10.1016/j.apsusc.2020.147677 ↗
32. Preparation and characterization of chromium oxide thin films: the response of morphology, crystal structure, and electrical properties to oxygen pressure under magnetron sputtering10.1016/j.vacuum.2024.113518 ↗
33. Effect of annealing on the structural, optical and surface properties of chromium oxide (Cr2O3) thin films deposited by e-beam evaporation for plasma etching applications10.1016/j.jallcom.2021.160087 ↗
34. Exploring the effect of Si content in Cr coating on its microstructure and properties10.1016/j.surfcoat.2024.131253 ↗
35. Welding reinforcement between silica glass and stainless steel using nanosecond fiber laser with chromium interlayer10.1016/j.optlaseng.2023.107877 ↗
36. Effects of different oxidation methods on the wetting and diffusion characteristics of a high-alumina glass sealant on 304 stainless steel
37. Investigation of metal mixing in laser keyhole welding of dissimilar metals10.1016/j.matdes.2020.109056 ↗
38. Laser powder-bed fusion additive manufacturing: physics of complex melt flow and formation mechanisms of pores, spatter, and denudation zones10.1016/j.actamat.2016.02.014 ↗
39. Influence of the thermal-fluid behavior on the microstructure evolution during the process of selective laser melting of Ti6Al4V10.1016/j.heliyon.2022.e11725 ↗
40. Sub-surface thermal measurement in additive manufacturing via machine learning-enabled high-resolution fiber optic sensing
41. Thermodynamic assessments of the Cr-Si and al-cr-si systems10.1016/j.jallcom.2017.03.042 ↗
42. Review on laser directed energy deposited aluminum alloys10.1088/2631-7990/ad16bb ↗
43. Aluminum and silicon diffusion in fe-cr-al alloys10.1016/S1359-6462(98)00498-9 ↗
44. Welding between rough copper foil and silica glass using green femtosecond laser10.1016/j.optlastec.2024.111804 ↗
45. The influence of anodization on laser transmission welding between high borosilicate glass and TC4 titanium alloy