journal article·2025-09

Effect of SiC interlayer on microstructure and flexural strength of C/C-SiC-(Zr,Hf,Ti)C composites prepared by reactive melt infiltration

Junwen Liu, Yalei Wang, Zhiwei Qiao, Xiang Xiong, Zhiyong Ye, Zaidong Liu

Ceramics International· Volume 51· Issue 23
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Strength improvement by densification of C/C composites10.1016/S0008-6223(00)00083-X ↗
2. Interfacial shear strength of C/C composites10.1016/S0008-6223(03)00144-1 ↗
3. Effect of pyrocarbon content on thermal and frictional properties in C/C preforms of C/C-SiC composites10.1016/j.wear.2010.03.017 ↗
4. Improving flexural performance of repaired C/C composites through Ti addition: mechanism analysis
5. Influence of the pore structure of carbon fibers on the oxidation resistance of C/C composites10.1016/S0008-6223(01)00274-3 ↗
6. Oxidation behavior of C/C composites with the fibre/matrix interface modified by carbon nanotubes grown in situ at low temperature10.1016/j.corsci.2011.09.024 ↗
7. Ablative and mechanical properties of C/C-SiC-ZrC composites modified with PyC/SiC and PyC/BN interface layers10.1111/ijac.14613 ↗
8. Influence of high temperature treatment of C/C porous preform on friction and wear behavior of C/C-SiC composites10.15541/jim20220555 ↗
9. High temperature corrosion of carbon/carbon composites in Zr-Ti melts during liquid metal infiltration10.1016/j.corsci.2015.05.014 ↗
10. Oxidation behavior of non-stoichiometric (Zr,Hf,Ti)C carbide solid solution powders in air10.1007/s40145-021-0469-y ↗
11. Effect of ZrC amount and distribution on the thermomechanical properties of Cf/SiC-ZrC composites10.1111/ijac.13217 ↗
12. Ablation of advanced C/C-ZrC-SiC leading edge composites10.1016/j.corsci.2023.111648 ↗
13. Formation mechanism of (Ti, Zr, Hf)C medium-entropy carbide derived from polymer precursors and its modification on the ablative mechanism of C/C-SiC composites10.1016/j.corsci.2024.111935 ↗
14. C/C-HfC-ZrC composites with excellent long-term ablation performance prepared by combining PIP and RMI10.1016/j.ceramint.2024.01.308 ↗
15. Nb- and Ta-doped (Hf,Zr,Ti)C multicomponent carbides with enhanced oxidation resistance at 2500 °C10.26599/JAC.2024.9220856 ↗
16. Advances in ultra-high temperature ceramics, composites, and coatings10.1007/s40145-021-0550-6 ↗
17. Mechanical and ablation properties of a C/C-HfB2-SiC composite prepared by high-solid-loading slurry impregnation combined with precursor infiltration and pyrolysis10.1016/j.jeurceramsoc.2021.06.055 ↗
18. Elevated temperature performance: Arc-jet testing of carbon fiber reinforced ZrB2 bars up to 2200 °C for strength retention assessment10.26599/JAC.2024.9221022 ↗
19. C/C-ZrC composite prepared by chemical vapor infiltration combined with alloyed reactive melt infiltration10.1016/j.ceramint.2012.04.017 ↗
20. Effect of pyrolytic carbon content on microstructure and tribological properties of C/C-SiC brake composites fabricated by isothermal chemical vapor infiltration10.1016/j.solidstatesciences.2011.10.010 ↗
21. Processing and performance of ultra high temperature ceramic matrix composite (UHTCMCs) using radio frequency assisted chemical vapour infiltration (RF-CVI)10.1016/j.compositesa.2024.108358 ↗
22. Effect of ZrC particle distribution on the ablation resistance of C/C-SiC-ZrC composites fabricated using precursor infiltration pyrolysis10.1016/j.ceramint.2020.03.157 ↗
23. Fabrication and properties of 3-dimensional 4-directional Cf/HfC-SiC composites by precursor impregnation and pyrolysis process10.1016/j.jallcom.2017.12.059 ↗
24. Preparation, microstructure and properties of C/Ta4HfC5-SiC composite fabricated by PIP method based on a new liquid precursor10.1016/j.jeurceramsoc.2025.117281 ↗
25. Microstructure, interfacial and mechanical properties of SiC interphase modified C/C-SiC composites prepared by reactive melt infiltration10.1016/j.jeurceramsoc.2024.116785 ↗
26. Microstructure and ablation behavior of carbon/carbon composites infiltrated with Zr-Ti10.1016/j.carbon.2012.11.042 ↗
27. Addressing high processing temperatures in reactive melt infiltration for multiphase ceramic composites10.1016/j.jeurceramsoc.2022.09.002 ↗
28. Application of carbon fiber-reinforced ceramic composites in active thermal protection of advanced propulsion systems: a review
29. Advances in processing and ablation properties of carbon fiber reinforced ultra-high temperature ceramic composites
30. Laser ablation behavior and mechanism of Cf/SiC-ZrC ultra-high temperature ceramic matrix composite prepared by PIP method10.1016/j.ceramint.2021.05.080 ↗
31. Efficient fabrication and properties of 2D Cf/(Ti0.2Zr0.2Hf0.2Nb0.2Ta0.2) C-SiC high-entropy ceramic matrix composites via slurry infiltration lamination combined with precursor infiltration and pyrolysis10.1016/j.jeurceramsoc.2023.07.080 ↗
32. Ablation resistant C/C-HfC-ZrC-TaC-SiC composites prepared by reactive melt infiltration10.1016/j.ceramint.2024.07.146 ↗
33. Reaction mechanism and microstructure development of Zr-Si alloyed melt-infiltrated ZrC-Modified C/C composite10.1111/jace.13595 ↗
34. Microstructure evolution and properties of Hf/Zr-based UHTCs modified C/C composites prepared by reactive melt infiltration method10.1016/j.jeurceramsoc.2023.12.078 ↗
35. Influence of graphitization treatment on microstructure and flexural strength of C/C-ZrC-SiC composites fabricated via reactive melt infiltration10.1016/j.ceramint.2023.05.139 ↗
36. Structure evolution and ablative mechanism of C/C-ZrC-ZrxCuy composites with low porosity fabricated by pressure assisted reactive melt infiltration10.1016/j.corsci.2022.110801 ↗
37. Effect of fiber architecture and density on the ablation behavior of carbon/carbon composites modified by Zr-Ti-C10.1016/j.carbon.2013.06.043 ↗
38. Interphase degradation of three-dimensional Cf/SiC-ZrC-ZrB2 composites fabricated via reactive melt infiltration10.1111/jace.14983 ↗
39. Construction of sandwich-structured C/C-SiC and C/C-SiC-ZrC composites with good mechanical and anti-ablation properties10.1016/j.jeurceramsoc.2021.12.006 ↗
40. Effects of SiC interphase on the mechanical and ablation properties of C/C-ZrC-ZrB2-SiC composites prepared by precursor infiltration and pyrolysis10.1016/j.matdes.2017.02.086 ↗
41. Infiltration mechanism and factors influencing carbon/carbon-Zr-Ti-C composites prepared by liquid metal infiltration10.1016/j.jmatprotec.2014.07.021 ↗
42. Excellent oxyacetylene ablation performance of C/C-Me-Zr-Hf-C (Me=Ta Si) composites prepared by a novel two-step molten salt infiltration10.1016/j.jeurceramsoc.2023.12.001 ↗
43. Microstructure and flexural strength of C/HfC-ZrC-SiC composites prepared by reactive melt infiltration method10.1016/j.jeurceramsoc.2022.12.015 ↗
44. Increasing the strength and toughness of a carbon fiber/silicon carbide composite by heat treatment10.1016/j.carbon.2012.11.001 ↗
45. Mechanical, oxidation and ablation properties of C/(C-SiC)CVI-(ZrC-SiC)PIP composites10.1016/j.corsci.2019.108200 ↗