Preparation and cutting performance of textured SiAlON ceramic brazing composite tool
Source abstract
Abstract
Three types of textured SiAlON ceramics (one-dimensional C-axis-oriented, two-dimensional randomly textured, and two-dimensional centripetally textured) were prepared using plastic deformation through extrusion, and then brazed to commercial cemented carbide substrates using vacuum brazing with a commercial Ag-Cu-Ti active brazing alloy to fabricate SiAlON brazed composite cutting tools for superalloy machining, simultaneously non-texture SiAlON cutting tools was prepared. The wear mechanisms of the cutting tools during superalloy machining include adhesive wear , oxidation wear, abrasive wear, and chipping. Among the four tools, the two-dimensional centripetally textured SiAlON composite tool, with rod-like grains oriented parallel to both the rake and flank faces, exhibited the best cutting performance. The reason is that the rod-like grains on its flank face are oriented toward the tool tip, providing enhanced fracture toughness and excellent resistance to chipping in the direction of the workpiece motion.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced machining processes and optimization · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Improvement of cutting performance of high x value α/β-SiAlON ceramic cutting inserts via tailoring microstructure and oxidation behavior10.1016/j.ijrmhm.2022.106087 ↗
2. Suitability of the full body ceramic end milling tools for high speed machining of nickel based alloy Inconel 71810.1016/j.procir.2018.08.190 ↗
3. The effect of cation type, intergranular phase amount and cation mole ratios on z value and intergranular phase crystallization of SiAlON ceramics10.1016/j.ceramint.2012.10.013 ↗
4. Pressureless sintering of β-SiAlON ceramic compositions using fluorine and oxide additive system10.1016/j.jeurceramsoc.2011.05.016 ↗
5. Thermal shock behaviour of α:β-SiAlON-TiN composites10.1016/j.ceramint.2013.09.064 ↗
6. Sintering and characterization of a hard-to-hard configured composite: spark plasma sintered WC reinforced α-SiAlON10.1016/j.jpcs.2020.109548 ↗
7. The property characterization of α-Sialon/Ni composites synthesized by spark plasma sintering10.3390/nano9121682 ↗
8. Sialon ceramic with gradient microstructures10.1016/S0257-8972(97)00641-5 ↗
9. Spark plasma sintering of α/β-SiAlON ceramic end mill rods: electro–Thermal simulation, microstructure, mechanical properties, and machining performance10.26599/JAC.2023.9220786 ↗
10. Hot forging Nb4AlC3 ceramics with enhanced properties10.26599/JAC.2023.9220805 ↗
11. Improvement of cutting performance of SiAlON ceramic by texture engineering in turning superalloys10.1016/j.ceramint.2023.06.254 ↗
12. Enhancing the strength of the PCBN/M42 joint via a solid solution brazed seam design involving a pre-melted CuNi layer and a Ti interlayer10.1016/j.ijrmhm.2024.106640 ↗
13. Effect of Ti content in Ag-Cu-Ti activated filler metal on dissimilar joint formation of sialon and WC-Co alloy by laser brazing10.1179/1362171814Y.0000000217 ↗
14. Brazing mechanism and shear strength of SiAlON/WC‐Co joint using Ag–Cu–Ti active filler10.1111/ijac.14881 ↗
15. Textured silicon nitride: processing and anisotropic properties10.1088/1468-6996/9/3/033001 ↗
16. Phase transformation kinetics and grain orientation of multi-cation doped (Yb, Sm) α/β-SiAlON ceramic tool materials10.1016/j.ceramint.2023.06.041 ↗
17. Preferential orientation of SiAlON grains in reversible α'↔β' phase transformations10.4028/www.scientific.net/KEM.237.163 ↗
18. Phase relationships and stability of α′-SiAlON10.1111/j.1151-2916.1999.tb01869.x ↗
19. Effect of crystal orientation, structure and dimension on vickers microhardness anisotropy of β-, α-Si3N4, α-SiO2 and α-SiC single crystals10.1016/0025-5408(82)90003-4 ↗
20. Evaluation of fracture toughness for ceramic materials10.2355/isijinternational.29.717 ↗
21. Microstructural design of silicon nitride with improved fracture toughness: I, effects of grain shape and size10.1111/j.1151-2916.1998.tb02702.x ↗
22. Wear and failure mechanisms of SiAlON ceramic tools during high-speed turning of nickel-based superalloys
23. Wear mechanisms and notch formation of whisker-reinforced alumina and sialon ceramic tools during high-speed turning of Inconel 71810.3390/ma15113860 ↗
24. Friction behaviors in the metal cutting process: state of the art and future perspectives10.1088/2631-7990/ac9e27 ↗
25. Temperature calculation in cutting zones10.1016/j.cirp.2018.03.009 ↗
26. 1993
27. Temperature distribution of cubic boron nitride-coated cutting tools by finite element analysis10.1007/s00170-019-04498-0 ↗
28. Cutting performance and wear mechanism of Sialon ceramic cutting inserts with TiCN coating10.1016/j.surfcoat.2016.08.069 ↗
29. A comparative study on characteristics of cutting tool materials based on SiAlON ceramics10.4150/KPMI.2021.28.6.502 ↗
30. Chip formation and wear mechanisms of SiAlON and whisker-reinforced ceramics when turning Inconel 718
31. Thermal effects in orthogonal cutting10.1007/s11740-013-0451-9 ↗