journal article·2024-12

Sealing Ni-Cr/Ni-Al alloys with borosilicate glass: Bonding strength, sealing interface, and fracture behavior

Zheng Liu, Chao Zhou, Keqian Gong, Yanfei Sun, Cheng Ren, Zifeng Song, Zhangjing Shi, Yong Zhang

Ceramics International· Volume 50· Issue 24
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced materials and composites · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Textile-integrated thermocouples for temperature measurement10.3390/ma13030626 ↗
2. In situ embedment of type K sheathed thermocouples with directed energy deposition10.1007/s00170-023-11624-6 ↗
3. Improving the water-resistance of MgO-based metal–insulator–metal capacitors by inserting a BeO thin film grown via atomic layer deposition10.1039/D2TC00595F ↗
4. Influence of moisture absorption on the synthesis and properties of Y2O3–MgO nanocomposites10.1016/j.ceramint.2016.08.117 ↗
5. Characterization of potting epoxy resins performance parameters based on a viscoelastic constitutive model10.3390/polym16070930 ↗
6. Physical aging of an epoxy/cycloaliphatic amine resin10.1016/S0014-3057(98)00132-3 ↗
7. The hygrothermal aging process and mechanism of the novolac epoxy resin10.1016/j.compositesb.2016.09.067 ↗
8. Review on silicate and borosilicate‐based glass sealants and their interaction with components of solid oxide fuel cell10.1002/er.7161 ↗
9. Non-crystallising glass sealants for SOFC: effect of Y2O3 addition10.1016/j.ceramint.2019.10.266 ↗
10. Kinetics of crack healing and self‐repair behaviors in a sealant glass for SOFC applications10.1111/ijac.14143 ↗
11. Glass fiber reinforced sealants for solid oxide fuel cells10.1016/j.ijhydene.2019.05.116 ↗
12. Optimized sealing process and real-time monitoring of glass-to-metal seal structures
13. Donald · 2009
14. Recent developments in the preparation, characterization and applications of glass- and glass–ceramic-to-metal seals and coatings10.1007/s10853-010-5095-y ↗
15. Fundamentals of glass-to-metal bonding: III, Temperature and pressure dependence of wettability of metals by glass10.1111/j.1151-2916.1957.tb12618.x ↗
16. Chemical compatibility of barium-calcium-aluminosilicate-based sealing glasses with the ferritic stainless steel interconnect in SOFCs10.1149/1.1590325 ↗
17. Photoluminescence spectroscopy to detect microregion stress distribution in glass‐to‐metal seals10.1111/jace.19769 ↗
18. Investigation of glass sintering to improve strength and interfacial interactions in glass‐to‐AISI 316L metal joints10.1111/ijag.16617 ↗
19. Shear strength and interfacial characterization of borosilicate glass-to-metal seals10.1016/j.jallcom.2020.154275 ↗
20. Surface alloy depletion and martensite formation during glass to metal joining of austenitic stainless steels10.1179/1362171812Y.0000000011 ↗
21. The effects of pre-oxidation and alloy chemistry of austenitic stainless steels on glass/metal sealing10.1007/s11085-009-9181-y ↗
22. Zinc diffusion affects the chemical stability of the borosilicate glass and AISI 304 interface10.1016/j.matchar.2020.110792 ↗
23. Morphological evolution of oxide layer and its effect on glass-to-metal seal10.1016/j.jnoncrysol.2020.120355 ↗
24. High temperature wettability studies for development of unmatched glass-metal joints in solar receiver tube10.1016/j.renene.2017.12.020 ↗
25. Fundamentals of glass‐to‐metal bonding: VII, wettability of iron by molten sodium silicate containing iron oxide10.1111/j.1151-2916.1961.tb13751.x ↗
26. Fundamentals of glass-to-metal bonding: V, wettability of iron by molten sodium disilicate10.1111/j.1151-2916.1961.tb13749.x ↗
27. Fundamentals of glass-to-metal bonding: VI, reaction between metallic iron and molten sodium disilicate10.1111/j.1151-2916.1961.tb13750.x ↗
28. Adhesion of borosilicate glass and Fe-Ni-Co alloy joined by direct fusion
29. Microscopy and strength of borosilicate glass-to-Kovar alloy joints10.1016/j.msea.2007.04.016 ↗
30. A new adhesion process of glass to metal using the redox reaction10.1007/BF00355877 ↗
31. Internal residual stresses in glass-ceramics: a review10.1016/j.jnoncrysol.2012.01.040 ↗
32. Sealing glass‐ceramics with near‐linear thermal strain, part III : stress modeling of strain and strain rate matched glass‐ceramic to metal seals10.1111/jace.14821 ↗
33. Development and interface characterization of unmatched glass-metal joint10.1016/j.jmapro.2017.12.027 ↗
34. Interface degradation of glass-to-metal seals during thermo-oxidative aging10.1016/j.corsci.2022.110189 ↗
35. Calibration for determination of compressive stress in glass‐to‐metal seals via photoluminescence spectroscopy10.1111/jace.19528 ↗
36. Joining of sintered SiC ceramics at a lower temperature using borosilicate glass with laser cladding Si modification layer10.1016/j.jeurceramsoc.2020.11.044 ↗
37. A microstructural study of preferential oxidation at the grain boundaries of Ni–Cr alloys10.1023/A:1014818117073 ↗
38. Kinetics of high temperature oxidation and chromia volatilization for a binary Ni–Cr alloy10.1007/s11085-005-6562-8 ↗
39. Studies of interface reactions between glass ceramic coatings and metals10.1016/0022-3093(89)90553-X ↗
40. The oxidation of three Ni–6Si–xAl alloys in 1atm O2 at 1000°C10.1016/j.corsci.2005.05.032 ↗
41. The synergistic effect of cavitation erosion and corrosion of nickel-aluminum copper surface layer on nickel-aluminum bronze alloy10.1016/j.jallcom.2018.03.103 ↗
42. Cavitation erosion behavior of Hastelloy C-276 nickel-based alloy10.1016/j.jallcom.2014.08.248 ↗
43. Interfacial reactions between lithium silicate glass-ceramics and Ni-based superalloys and the effect of heat treatment at elevated temperatures10.1023/B:JMSC.0000011517.36767.a0 ↗
44. Strength, microstructure and bonding mechanism of borosilicate glass-to-SA105 carbon steel seals10.1088/2053-1591/ad6b00 ↗
45. Sintering of glass matrix composites with small rigid inclusions10.1016/j.jeurceramsoc.2009.02.007 ↗
46. Effect of compaction on the sintering of borosilicate glass/alumina composites10.1016/S0955-2219(02)00422-3 ↗
47. Fracture study of glass with bubbles: multiscale finite element method and experimental facts10.1016/j.mtla.2023.101746 ↗
48. Contributions of mechanical bonding and chemical bonding to high-temperature hermeticity of glass-to-metal compression seals10.1016/j.matdes.2021.109579 ↗
49. Multiphase microstructure formation and its effect on fracture behavior of medium carbon high silicon high strength steel10.1016/j.jmst.2020.09.034 ↗
50. Effect of grain size on the ductile-brittle fracture behavior of commercially pure titanium sheet metals