journal article·2024-06

Chemical resistance and corrosion mechanism of aluminophosphate-based low temperature enamel (LTE) in H2SO4 and NaOH solutions

Dongming Yan, Shenhao Ye, Hao Qian, Peng Guo, Yi Liu

Ceramics International· Volume 50· Issue 11
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition · Dental materials and restorations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (69)

Show source-provided references
1. The cost of corrosion in China10.1038/s41529-017-0005-2 ↗
3. Lunt · 1977
4. Anti-corrosion coatings for protection of steel railway structures exposed to atmospheric environments: a review10.1016/j.conbuildmat.2021.123115 ↗
5. Metallurgy of galvanized coatings10.1179/095066079790136327 ↗
6. Cathodic protection with sacrificial anodes10.1515/CORRREV.2006.24.3-4.231 ↗
7. The Cr-Ni (Chromium-Nickel) system10.1007/BF02867812 ↗
8. Sastri · 1998
9. Durability of vitreous enamel coatings and their resistance to abrasion, chemicals, and corrosion: a review10.1007/s11998-020-00415-3 ↗
10. Nanoindentation and SEM/EDX characterization of the geopolymer-to-steel interfacial transition zone for a reactive porcelain enamel coating10.1016/j.compositesb.2015.03.011 ↗
11. Evaluation of the abrasion resistance of enamel coatings10.1016/j.cep.2012.10.009 ↗
12. Influence of graphene addition on the mechanical and surface properties of vitreous enamel coatings10.1016/j.surfcoat.2020.126071 ↗
13. Abrasion and chemical resistance of composite vitreous enamel coatings with hard particles10.1002/sia.5849 ↗
14. The aesthetic and functional properties of enamel coatings on steel10.1016/j.matdes.2010.04.030 ↗
15. Low-melting chemically resistant enamel for steel kitchenware10.1023/A:1023886032228 ↗
16. Glass enamel and glass-ceramic coatings for chemical apparatus10.1007/BF01154564 ↗
17. Corrosion resistances of steel pipes internally coated with enamel10.5006/2497 ↗
18. Corrosion resistance of transmission pipeline steel coated with five types of enamels10.1007/s40195-017-0554-y ↗
19. Torsional guided-wave attenuation in coal-tar-enamel-coated, buried piping10.1016/j.ndteint.2004.05.003 ↗
20. Corrosion resistance and mechanism of steel rebar coated with three types of enamel10.1016/j.corsci.2012.02.024 ↗
21. Microstructure and corrosion resistance of enamel coatings applied to smooth reinforcing steel10.1016/j.conbuildmat.2012.04.059 ↗
22. Microstructural and mechanical characterization of the interface between concrete and chemically reactive enamel (CRE) coated rebar10.1016/j.conbuildmat.2020.120676 ↗
23. The roles of H2S gas in behavior of carbon steel corrosion in oil and gas environment: a review10.22441/jtm.v7i1.2279 ↗
24. Koteeswaran · 2010
25. Study of corrosion control effect of H2S scavengers in multiphase systems
26. Rate and mechanism of the reaction of silicates with cement pore fluids10.1016/0169-1317(92)90026-J ↗
27. The chemistry of the pore fluid of silica fume-blended cement systems10.1016/0008-8846(90)90095-F ↗
28. Ubertazzi · 2002
29. Andrews · 1961
30. Chemical durability of glasses; a thermodynamic approach10.1007/BF00552247 ↗
31. Blue enamel pigment—chemical and morphological characterization of its corrosion process10.1016/j.corsci.2018.05.005 ↗
32. Corrosion of SiO2–B2O3–Al2O3–CaF2-R2O (R=Na and K) enamels with different content of ZrO2 in H2SO4 and NaOH solutions10.1016/j.ceramint.2019.04.232 ↗
33. Simulating sulfuric acid dew point corrosion of enamels with different contents of silica10.1016/j.corsci.2017.08.012 ↗
34. Effect of glass powder on acid resistance of enamel coating10.1142/S0218625X17500366 ↗
35. Xu · 2020
36. Enamel coatings mill additives optimization for sulfuric acid corrosion10.1111/ijac.14538 ↗
37. Effect of bentonite content on the suspension stability of a glaze slurry and final enamel performance10.1016/j.ceramint.2022.11.116 ↗
38. Evaluation of 316L stainless mill additives on microstructure and alkali corrosive behavior of enamel coatings10.1111/jace.19115 ↗
39. Glass coatings on stainless steels for high-temperature oxidation protection: mechanisms10.1016/j.corsci.2014.01.033 ↗
40. Effect of high temperature exposure and strain rate on mechanical properties of high-strength steel rebars10.1061/(ASCE)MT.1943-5533.0002906 ↗
41. Phase Structure and corrosion resistance of multilayer low-temperature sintered chemically reactive enamel coatings10.1061/(ASCE)MT.1943-5533.0003334 ↗
42. Study of lower temperature–sintered enamel coating on steel bars: effect of coating cycles10.1061/(ASCE)MT.1943-5533.0003346 ↗
43. Thermal-spray deposition of enamel on aluminium alloys10.1016/j.surfcoat.2013.04.065 ↗
44. Silicon carbide/enamel composite coatings for steel corrosion protection: microstructure, thermal expansion behavior, and anti-corrosion performance10.1016/j.surfcoat.2022.128172 ↗
45. Substrate surface roughening improves the interfacial properties between steel rebar and low temperature enamel (LTE) coating10.1016/j.ceramint.2023.06.224 ↗
46. Silicon nitride modified enamel coatings enable high thermal shock and corrosion resistances for steel protection10.1016/j.surfcoat.2021.127474 ↗
47. Long-term corrosion of silicon carbide/enamel composite coatings on steel rebars: a microstructure-dependent corrosion behavior10.1016/j.jobe.2023.107007 ↗
48. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
49. Vibrational characteristics of aluminum–phosphate compounds by an experimental and theoretical approach10.1038/s41598-022-22432-5 ↗
50. Uncovering the phase transition of berlinite (α-AlPO4) under high pressure: insights from first-principles calculations10.1007/s11595-021-2402-1 ↗
51. The thermodynamics of the system CaSO4—H2O10.1524/zpch.1977.104.1-3.041 ↗
52. Spectra structure correlations in hydroxy and fluorapatite10.1016/0371-1951(66)80133-9 ↗
53. Crystal imperfection studies of pure and silicon substituted hydroxyapatite using Raman and XRD10.1007/s10856-005-4721-8 ↗
54. Micro-Raman and FTIR studies of synthetic and natural apatites10.1016/j.biomaterials.2007.02.028 ↗
55. Octacalcium phosphate and hydroxyapatite: crystallographic and chemical relations between octacalcium phosphate and hydroxyapatite10.1038/1961050a0 ↗
56. Raman spectroscopy of some natural hydrotalcites with sulphate and carbonate in the interlayer10.1002/jrs.1050 ↗
57. Application of thermo-Raman spectroscopy to study dehydration of CaSO4 2H2O and CaSO4 0.5H2O10.1016/S0254-0584(98)00239-9 ↗
58. Clarification of phosphorus fractions and phosphorus release enhancement mechanism related to pH during waste activated sludge treatment10.1016/j.biortech.2016.10.010 ↗
59. Laudise · 1970
60. Conversion of calcium fluorapatiteinto calcium hydroxyapatite under alkaline hydrothermal conditions10.1006/jssc.1999.8623 ↗
61. AlPO4‐containing glass‐crystalline materials in the system Li2O‐Al2O3‐P2O510.1002/bbpc.19961000919 ↗
62. J. Zeng, and L. Hu, Progress for Preparation and Application of Nano-Aluminate Phosphate.
63. Recovery of sodium phosphate from incinerated ash of sewage sludge by gel formation
64. Anaerobic digestion of hydrothermally pretreated dewatered sewage sludge: effects of process conditions on methane production and the fate of phosphorus10.1007/s11356-023-26990-7 ↗
65. Electronic and crystallographic structure of apatites10.1103/PhysRevB.67.134106 ↗
66. A structural model for phosphate glasses10.1016/0022-3093(95)00524-2 ↗
67. Review: the structure of simple phosphate glasses10.1016/S0022-3093(99)00620-1 ↗
68. Synthesis and characterization of rare-earth doped aluminium phosphate glasses10.1016/j.pnucene.2022.104372 ↗
69. Raman imaging as a useful tool to describe crystallization of aluminum/iron-containing polyphosphate glasses10.1016/j.jeurceramsoc.2021.03.028 ↗