journal article·2023-06

Modification of low-melting phase monticellite (CMS) by La2O3

Yan Cui, Dianli Qu, Xudong Luo, Yu Zheng, Peng Wang

Ceramics International· Volume 49· Issue 11
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Magnesium Oxide Properties and Applications · Advanced ceramic materials synthesis · Microwave Dielectric Ceramics Synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Comparison of ferrous calcium silicate slag and calcium ferrite slag interactions with magnesia-chrome refractories10.1007/s11663-011-9499-0 ↗
2. Strength behavior of magnesia-based refractories after thermal cycling10.1111/ijac.12027 ↗
3. Use of magnesia sand for optimal design of high performance magnesium potassium phosphate cement mortar10.1016/j.conbuildmat.2017.07.099 ↗
4. Modification of matrix for magnesia material by in situ nitridation10.1016/j.ceramint.2019.06.013 ↗
5. Comparison study of slag corrosion resistance of MgO-MgAl2O4, MgO-CaO and MgO-C refractories under electromagnetic field10.1007/s42243-020-00421-0 ↗
6. Influence of pre-synthesized Al2O3-SiC composite powder from clay on properties of low-carbon MgO-C refractories10.1007/s42243-021-00653-8 ↗
7. Enhanced oxidation resistance of low-carbon MgO-C refractories with ternary carbides: a review10.1007/s42243-022-00804-5 ↗
8. Recent progress in synthesis of composite powders and their applications in low-carbon refractories10.1007/s42243-022-00806-3 ↗
9. A study of commercial periclases10.1111/j.1151-2916.1960.tb13668.x ↗
10. Composition of periclase and calcium silicate phases in magnesia refractories derived from natural microcrystalline magnesite10.1111/j.1551-2916.2005.00263.x ↗
11. Effect of zirconia on densification and properties of natural Indian magnesite10.1016/j.minpro.2015.09.006 ↗
12. From magnesite directly to lightweight closed-pore MgO ceramics: the role of Si and Si/SiC10.1016/j.ceramint.2021.07.287 ↗
13. Effect of titania on the microstructure evolution of sintered magnesite in correlation with its properties10.1016/j.ceramint.2015.03.236 ↗
14. Facile synthesis of MgO-Mg2SiO4 composite ceramics with high strength and low thermal conductivity10.1016/j.ceramint.2021.03.331 ↗
15. Phase equilibrium relations in the specific region of CaO-SiO2-La2O3 system10.1016/j.jeurceramsoc.2017.12.011 ↗
16. Designing low-carbon MgO-Al2O3-La2O3-C refractories with balanced performance for ladle furnaces10.1016/j.jeurceramsoc.2022.03.051 ↗
17. ZrO2 and MxOy (M=La, Ce, and Nb) synergistically reinforced porous cordierite ceramics synthesized via a facile solid-state reaction10.1016/j.ceramint.2022.05.249 ↗
18. The effects of pre-sintering temperature and La2O3 addition on sinterability and corrosion resistance of stoichiometric magnesium aluminate spinel10.1016/j.ceramint.2022.07.193 ↗
19. Synthesis and densification behaviour of magnesium aluminate spinel: effect of Dy2O310.1016/j.ceramint.2009.02.011 ↗
20. Fundamentals and applications on in situ spinel formation mechanisms in Al2O3-MgO refractory castables10.1016/j.ceramint.2011.10.074 ↗
21. The effect of Y2O3 addition on thermal shock behavior of magnesium aluminate spinel10.2298/SOS0901075P ↗
22. Effects of processing parameters and rare earths additions on preparation of Al2O3-SiC composite powders from coal ash10.1016/j.ceramint.2017.05.362 ↗
23. Effect of CeO2 on the crystalline structure of forsterite synthesized from low-grade magnesite10.1007/s11148-013-9595-6 ↗
24. Improvement in thermo-mechanical properties of off-grade natural magnesite by addition of Y2O310.1111/ijac.12736 ↗
25. Structure and properties of periclase ceramics dopped with rare-earth oxides10.1007/BF00682548 ↗
26. Microstructure, properties, and application of low carbon Al2O3‐C refractories used as submerged entry nozzles10.1111/ijac.13388 ↗
27. Effect of YSZ with different Y2O3 contents on toughening behavior of Al2O3/Ba-β-Al2O3/ZrO2 composites10.1016/j.ceramint.2019.06.023 ↗
28. Elastic moduli and refractive indices of aluminosilicate glasses containing Y2O3, La2O3, and TiO210.1111/j.1151-2916.1978.tb09291.x ↗
29. Phase stability and equilibria in the La2O3-TiO2 system10.1016/S0955-2219(99)00270-8 ↗
30. Effect of La2O3 addition on the microstructural evolution and thermomechanical property of sintered low-grade magnesite10.1016/j.ceramint.2020.09.150 ↗
31. Study of the filamentary growth of silicon crystals from the vapor10.1063/1.1713143 ↗
32. Growth mechanism of crystalline SiAlON microtubes prepared by combustion synthesis10.1039/c2ce25525a ↗
33. Relations between crystal structure and growth morphology of β-Si3N410.1016/0022-0248(94)90509-6 ↗
34. Grain growth studies of silicon nitride dispersed in an oxynitride glass10.1111/j.1151-2916.1993.tb04015.x ↗
35. Morphology of silicon nitride grown from a liquid phase10.1111/j.1151-2916.1998.tb02676.x ↗
36. Modeling and simulation of grain growth in Si3N4: I, anisotropic ostwald ripening10.1016/S1359-6454(98)00290-0 ↗
37. Modeling and simulation of grain growth in Si3N4: III, tip shape evolution10.1016/S1359-6454(00)00250-0 ↗