Effect of interface types on the heat-resistance of Cansas-II SiCf /SiC composites

Xiao Han, Xihui Chen, Xuming Niu, Zhigang Sun, Yingdong Song

Ceramics International· Volume 48· Issue 1
Publisher page

Abstract

Abstract The heat-resistance of the Cansas-II SiC/CVI-SiC mini-composites with a PyC and BN interface was studied in detail. The interfacial shear strength of the SiC/PyC/SiC mini-composites decreased from 15 MPa to 3 MPa after the heat treatment at 1500 °C for 50 h, while that of the SiC/BN/SiC mini-composites decreased from 248 MPa to 1 MPa, which could be mainly attributed to the improvement of the crystallization degree of the interface and the decomposition of the matrix. Aside from the above reasons, the larger declined fraction of the interfacial shear strength of the SiC/BN/SiC mini-composites might also be related to the gaps in the BN interface induced by the volatilization of B2O3·SiO2 phase, leading to a significant larger declined fraction of the tensile strength of the SiC/BN/SiC mini-composites due to the obvious expansion of the critical flaws on the fiber surface. Therefore, compared with the CVI BN interface, the CVI PyC interface has better heat-resistance at high temperatures up to 1500 °C due to the fewer impurities in PyC.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. A review of third generation SiC fibers and SiCf/SiC composites10.1016/j.jmst.2019.07.020 ↗
3. Effect of heat treatment on microstructure and mechanical properties of PIP-SiC/SiC composites10.1016/j.msea.2012.09.027 ↗
4. Effect of heat treatment on the mechanical properties of PIP–SiC/SiC composites fabricated with a consolidation process10.1016/j.ceramint.2013.08.029 ↗
5. Effect of heat treatment on the microstructure and mechanical behavior of SiC/SiC mini-composites10.1016/j.msea.2018.12.118 ↗
6. Effect of intermediate heat treatment on mechanical properties of SiCf/SiC composites with BN interphase prepared by ICVI10.1016/j.jeurceramsoc.2010.12.018 ↗
7. Effect of heat treatment on the mechanical properties of SiCf/BN/SiC fabricated by CVI10.1016/j.ceramint.2015.11.030 ↗
8. Microstructure and damage evolution of SiCf/PyC/SiC and SiCf/BN/SiC mini-composites: a synchrotron X-ray computed microtomography study10.1016/j.ceramint.2019.03.004 ↗
9. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
10. A methodology to measure the interface shear strength by means of the fiber push-in test10.1016/j.compscitech.2012.08.011 ↗
11. A family of weakest link models for fiber strength distribution10.1016/j.compositesa.2006.06.004 ↗
12. Effect of heat treatment on the microstructure and tensile strength of KD-II SiC fibers10.1016/j.msea.2016.07.066 ↗
13. Structural evolution and mechanical properties of Cansas-III SiC fibers after thermal treatment up to 1700 °C10.1016/j.jeurceramsoc.2020.12.003 ↗
14. Thermal stability of a PCS-derived SiC fibre with a low oxygen content (Hi-Nicalon)10.1023/A:1018541030308 ↗
15. Effects of temperature and atmosphere on microstructural evolution and mechanical properties of KD-II SiC fibers10.1016/j.ceramint.2020.06.225 ↗
16. Effect of composition and heat treatment conditions on the tensile strength and creep resistance of SiC-based fibers10.1016/S0955-2219(99)00114-4 ↗
17. The effect of heat treatment on the strength and toughness of carbon fiber/silicon carbide composites with different pyrolytic carbon interphase thicknesses10.1016/j.carbon.2013.01.076 ↗
18. Recent developments in fibers and interphases for high temperature ceramic matrix composites10.1016/S1359-835X(98)00131-6 ↗
19. Characterization of boron nitride films deposited from BCl3-NH3-H2 mixtures in chemical vapour infiltration conditions10.1007/BF00368905 ↗
20. Effects of heat treatment on microstructure and mechanical properties of 2.5D Cf/BN/pyrocarbon composites by chemical vapor infiltration10.1016/j.surfin.2021.100951 ↗
21. Boron-bearing species in ceramic matrix composites for long-term aerospace applications10.1016/j.jssc.2003.03.005 ↗
22. A pervasive mode of oxidative degradation in a SiC-SiC composite10.1111/j.1151-2916.1998.tb02696.x ↗
23. Raman study of SiC fibres made from polycarbosilane10.1007/BF01160751 ↗
24. Effect of different thickness h-BN coatings on interface shear strength of quartz fiber reinforced SiOCN composite10.1016/j.apsusc.2013.12.067 ↗
25. Effect of PyC interphase thickness on mechanical behaviors of SiBC matrix modified C/SiC composites fabricated by reactive melt infiltration10.1016/j.carbon.2014.05.092 ↗
26. Tensile and stressed-oxidation behavior of 2D SiC/BN/SiC composites at intermediate temperatures in air10.1016/j.ceramint.2021.06.082 ↗
27. Damage and failure of SiC fiber tows during environment activated slow crack growth: residual behavior and Strength-Probability-Time diagrams10.1016/j.actamat.2017.03.073 ↗
28. Failure of fiber bundles10.1016/j.compscitech.2003.07.003 ↗