journal article·2023-10

Effect of surface grain structure on reaction of residual glass phase with hydrofluoric acid in glass-ceramics

Yuxuan Zhang, Tiezhu Zhang, Hangren Li, Gang Han, Yu Li, Wence Xu, Rui Ma, Nannan Wu, Shunli Ouyang

Ceramics International· Volume 49· Issue 19
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Glass properties and applications · Building materials and conservation · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Transparent glass-ceramics functionalized by dispersed crystals10.1016/j.pmatsci.2018.02.006 ↗
2. Advances in transparent glass–ceramic phosphors for white light-emitting diodes—a review10.1016/j.jeurceramsoc.2014.10.002 ↗
3. Strengthened surface crystallized 19.6Li2O·11.0ZrO2·69.4SiO2 and 20.0Li2O·6.7ZrO2·68.9SiO2·4.4Al2O3 glass-ceramics10.1016/j.msea.2019.02.055 ↗
4. Raman spectroscopic study of irregular network in the process of glass conversion to CaO-MgO-Al2O3-SiO2 glass-ceramics10.1016/j.jnoncrysol.2021.120701 ↗
5. Effect of milling, fitting adjustments, and hydrofluoric acid etching on the strength and roughness of CAD-CAM glass-ceramics: a systematic review and meta-analysis
6. HF etching effect on sandblasted soda-lime glass properties10.1016/j.jeurceramsoc.2009.03.020 ↗
7. Effects of HF etching on nanoindentation response of ion-exchanged aluminosilicate float glass on air and tin sides10.1007/s10853-016-0684-z ↗
8. A study of the dissolution of SiO2 in acidic fluoride solutions10.1149/1.2407835 ↗
9. The dissolution of Na2O-MgO-CaO-SiO2 glass in aqueous HF solutions10.1007/BF01132419 ↗
10. Stress-corrosion mechanisms in silicate glasses10.1088/0022-3727/42/21/214006 ↗
11. Fatigue failure load of zirconia-reinforced lithium silicate glass ceramic cemented to a dentin analogue: effect of etching time and hydrofluoric acid concentration10.1016/j.jmbbm.2017.09.028 ↗
12. Morphology and chemical termination of HF-etched Si3N4 surfaces10.1063/1.4905282 ↗
13. Structural and 57Fe Mössbauer spectroscopic characterization of the synthetic NaFeSi2O6 (aegirine) - CaMgSi2O6 (diopside) solid solution series10.1524/zkri.2012.1514 ↗
14. Growth of diopside crystals in CMAS glass-ceramics using Cr2O3 as a nucleating agent10.1111/jace.15700 ↗
15. Modeling of the coadsorption of chloride and hydrogen ions on copper electrode surface10.1149/2.0061901jes ↗
16. Raman identification of glassy silicates used in ceramics, glass and jewellery: a tentative differentiation guide10.1002/jrs.1515 ↗
17. Measurement of microscale residual stresses in multi-phase ceramic composites using Raman spectroscopy10.1016/j.actamat.2017.03.015 ↗
18. The phenomena of rupture and flow in solids
19. Crack propagation in silicon nitride ceramics under various temperatures and grain boundary toughness10.1016/j.msea.2015.02.061 ↗
20. Effect of melting temperature on the crystal growth of diopside
21. The mechanism of the crystalline characteristics of spinel-induced epitaxial growth of diopside in CMAS glass-ceramics10.1016/j.jeurceramsoc.2020.09.037 ↗
22. Stress corrosion and static fatigue of glass10.1111/j.1151-2916.1970.tb15962.x ↗
23. Molecular mechanisms for corrosion of silica and silicate-glasses10.1016/0022-3093(94)90708-0 ↗
24. Stress-corrosion mechanisms in silicate glasses10.1088/0022-3727/42/21/214006 ↗
25. Environmentally enhanced fracture of glass: a historical perspective10.1111/j.1551-2916.2009.03097.x ↗
26. Formation of embedded patterns in glasses using femtosecond irradiation10.1007/s00339-004-2845-1 ↗
27. Strength of brittle materials in moderately corrosive environments10.1111/jace.15307 ↗
28. Piezo-Raman measurements and anharmonic parameters in silicon and diamond10.1103/PhysRevB.41.7529 ↗
29. Effects of microstructures on the mechanical properties of lithium disilicate glass-ceramics for the SiO2–Li2O–P2O5–K2O–ZnO system10.1016/j.msea.2020.140564 ↗
30. Impact of oral fluids on dental ceramics: what is the clinical relevance?10.1016/j.dental.2013.08.199 ↗
31. A study of mechanical property and corrosion resistance of modified silica glass
32. Real-time in situ observations of reaction and transport phenomena during silicate glass corrosion by fluid-cell Raman spectroscopy10.1038/s41563-019-0293-8 ↗
33. Aqueous corrosion of borosilicate glass under acidic conditions: a new corrosion mechanism10.1016/j.jnoncrysol.2010.04.033 ↗
34. The mechanism of borosilicate glass corrosion revisited10.1016/j.gca.2015.02.039 ↗
35. Dean · 1999
36. Su · 2015