journal article·2023-01

Damage mechanism of Al2O3f/Al2O3 composites by acoustic emission technology

Xiang Yang, Chen Kun, Zheng Zhou, Zhang Wen, Peng Zhi-hang, Sun Chen-cheng, Wu Wen-jun, Cao Jian-hui

Ceramics International· Volume 49· Issue 2
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced Surface Polishing Techniques · High-Velocity Impact and Material Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Creep and microstructure of NextelTM720 fiber at elevated temperature in air and in steam[J]10.1016/j.actamat.2013.06.053 ↗
2. Advances in processing of NiAl intermetallic alloys and composites for high temperature aerospace applications[J]10.1016/j.paerosci.2015.09.003 ↗
3. Oxidation protection of C/C composites: coating development with thermally stabile SiC@PyC nanowires and an interlocking TaB_2-SiC structure[J]10.1016/j.corsci.2018.12.024 ↗
4. Degradation of CVD-SiC coated C/SiC composites exposed to the monopropellant combustion products based on Hydroxylammonium nitrate[J]10.1016/j.corsci.2013.04.036 ↗
5. Degradation of CVD-SiC coated PIP-C/SiC composites exposed to the hot firing test based on MMH/N2O4 bipropellants[J]10.1016/j.ceramint.2014.03.001 ↗
6. High-temperature properties of 2.5D SiO2f/SiO2 composites by sol–gel[J]10.1016/j.ceramint.2016.05.043 ↗
7. Effects of ZrO2 coating on the strength improvement of 2.5D SiCf/SiO2 composites[J]10.1016/j.ceramint.2016.09.164 ↗
8. Sol-gel process and high-temperature property of SiO2/ZrO2-SiO2 composites[J]
9. Effects of sintering temperature on mechanical properties of 3D mullite fiber (ALF FB3) reinforced mullite composites[J]10.1016/j.ceramint.2013.05.030 ↗
10. Microstructure and room temperature mechanical properties of mullite fibers after heat-treatment at elevated temperatures[J]
11. Mechanical behavior of oxide–oxide fiber-reinforced CMCs at elevated temperature: environmental effects[J]
12. Assessment of three oxide/oxide ceramic matrix composites: mechanical performance and effects of heat treatments[J]10.1016/j.compositesa.2014.09.013 ↗
13. Nielsen · 1980 · vol. 15 · 80
14. The velocity and attenuation of acoustic emission waves in SiC/SiC composites loaded in tension[J]10.1016/S0266-3538(02)00065-9 ↗
15. Modal acoustic emission of damage accumulation in a woven SiC/SiC composite[J]10.1016/S0266-3538(98)00121-3 ↗
16. Study on interfacial debonding stress and damage mechanisms of C/SiC composites using acoustic emission[J]10.1016/j.ceramint.2020.10.013 ↗
17. Effects of sintering temperature on mechanical properties of alumina fiber reinforced alumina matrix composites[J]10.1007/s10971-019-05192-z ↗
18. Interlaminar shear behaviors of 2D needled C/SiC composites under compressive and tensile loading[J]10.1016/j.ceramint.2020.10.071 ↗
19. On acoustic emission for damage detection and failure prediction in fiber reinforced polymer rods using pattern recognition analysis[J]
20. Effects of matrix porosity on the mechanical properties of a porous-matrix, all-oxide ceramic composite[J]10.1111/j.1151-2916.2001.tb01059.x ↗
21. Acoustic emission characterization of damage in hybrid fiber-reinforced polymer rods[J]10.1061/(ASCE)1090-0268(2004)8:1(70) ↗
22. The velocity and attenuation of acoustic emission waves in SiC/SiC composites loaded in tension[J]10.1016/S0266-3538(02)00065-9 ↗
23. Acoustic emission as a screening tool for ceramic matrix composites[J]
24. On the identification of the failure mechanisms in oxide/oxide composites using acoustic emission[J]10.1016/S0963-8695(03)00068-9 ↗