Hot corrosion resistance of air plasma sprayed ceramic Sm2SrAl2O7 (SSA) thermal barrier coatings in simulated gas turbine environments
Source abstract
Abstract
Abstract Samarium strontium aluminate (Sm 2 SrAl 2 O 7 -SSA) and Yttria-stabilized zirconia (YSZ) thermal barrier coatings (TBCs) were developed on NiCrAlY bond coated Inconel 718 superalloy substrate using air plasma spray process. The hot corrosion study was conducted in simulated gas turbine environments (molten mixtures of 50 wt% Na 2 SO 4 + 50 wt% V 2 O 5 and 90 wt% Na 2 SO 4 + 5 wt% V 2 O 5 + 5 wt% NaCl) for two different temperatures of 700 and 900 °C. A developed SSA TBCs showed about 8% and 22% lower lifetime at 700 and 900 °C, respectively than YSZ TBCs in 50 wt% Na 2 SO 4 + 50 wt% V 2 O 5 (vanadate). The hot corrosion life of SSA TBCs being found about 13% and 39% lower than YSZ TBCs in 90 wt% Na 2 SO 4 + 5 wt% V 2 O 5 + 5 wt% NaCl (chloride) at 700 and 900 °C, respectively. X-ray diffraction results showed the formation of SmVO 4 , SrV 2 O 6 , and SrSO 4 as a major hot corrosion product in 50 wt% Na 2 SO 4 + 50 wt% V 2 O 5 and 90 wt% Na 2 SO 4 + 5 wt% V 2 O 5 + 5 wt% NaCl environments respectively for SSA TBCs. Similarly, YSZ TBCs also showed YVO 4 as hot corrosion product in vanadate and chloride environments. Both the TBCs suffer a more severe hot corrosion attack in chloride environment at 900 °C. The leaching of Sr 2+ and Y 3+ ions from SSA and YSZ respectively play a vital role in the destabilization of coating in vanadate and chloride environments at 700 and 900 °C. In both SSA and YSZ TBCs, the leaching of ion has significantly low influence as compared to attack by chloride ions at the bond coat-top coat interface in the presence of chloride environment. The hot corrosion resistance of SSA TBCs was improved three times higher in the presence of MgO and NiO inhibitor in vanadate environment at 900 °C mainly due to the formation of a stable Ni 3 V 2 O 8 phase at the surface.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Catalytic Processes in Materials Science · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Common failures in gas turbine blades10.1016/j.engfailanal.2004.07.004 ↗
2. Hot corrosion in gas turbine components10.1016/S1350-6307(00)00035-2 ↗
3. Hot corrosion of materials: a fluxing mechanism?10.1016/S0010-938X(01)00057-9 ↗
4. Hot corrosion behavior of plasma sprayed YSZ/LaMgAl11O19 composite coatings in molten-sulfate vanadate salts10.1016/j.corsci.2011.03.019 ↗
5. Some aspects of the hot corrosion thermal barrier coatings10.1007/BF02646315 ↗
6. Hot corrosion behavior of rare earth zirconates and yttria partially stabilized zirconia thermal barrier coatings10.1016/j.surfcoat.2010.04.044 ↗
7. Hot corrosion behavior of LaTi2Al9O19 ceramic exposed to vanadium oxide at temperatures of 700–950 °C in air10.1016/j.corsci.2015.12.024 ↗
8. Hot corrosion behavior of plasma sprayed functionally graded thermal barrier coatings in the presence of Na2SO4 + V2O5 salt10.1016/j.surfcoat.2017.07.058 ↗
9. Hot corrosion behavior of overlay-clad yttria stabilized zirconia coatings in contact with vandate-sulfate salts10.1016/j.jeurceramsoc.2009.10.017 ↗
10. Thermal conductivity of rare earth strontium aluminates10.1111/j.1551-2916.2009.03594.x ↗
11. Anisotropic elastic and thermal properties of the double perovskite slab-rock salt layer Ln2SrAl2O7 (Ln˭La, Nd, Sm, Eu, Gd or Dy) natural superlattice structure10.1016/j.actamat.2012.03.004 ↗
12. Thermal expansion of MCrAlY alloys10.1016/j.surfcoat.2003.05.001 ↗
13. Role of thermally grown oxide and oxidation resistance of samarium strontium aluminate based air plasma sprayed ceramic thermal barrier coatings10.1016/j.surfcoat.2017.07.049 ↗
14. Influence of ceramic top coat and thermally grown oxide microstructures of air plasma sprayed Sm2SrAl2O7 thermal barrier coatings on the electrochemical impedance behavior10.1016/j.surfcoat.2018.03.058 ↗
15. Solid-liquid phase equilibria for the ternary systems V2O5-Na2O-Fe2O3, V2O5-Na2O-Cr2O3, and V2O5-Na2O-MgO10.1139/v73-153 ↗
16. Mechanisms and mitigation of volcanic ash attack on yttria stabilized zirconia thermal barrier coatings10.1016/j.surfcoat.2014.09.015 ↗
17. W.R. May, M.J. Zetlmeisl, R.R. Annand, D.F. Laurence, High temperature corrosion in gas turbines and steam boilers by fuel impurities. III. Evaluation of the effects of manganese, calcium and several heavy metals on corrosion and slag formation, in: Symposium on Heavy Fuel Oil Additives, New York City, New York, April, 1976.10.1115/1.3446229 ↗
18. Evaluation of sulfidation corrosion inhibitors by small burner rig tests
19. Revisiting the inhibition of vanadium induced hot corrosion in gas turbines10.1115/1.1456095 ↗
20. Hot corrosion of stabilized thermal barrier coatings and the role of Mg inhibitor10.1111/jace.13631 ↗
21. Effects of chromate and vanadate anions on the hot corrosion of pre-oxidized Ni by a thin fused Na2SO4 film at 900 °C10.1149/1.2086437 ↗
22. On the cyclic hot corrosion behavior of atmospheric plasma sprayed Lanthanum Zirconate based coatings in contact with a mixture of sodium sulfate and vanadate salts: a comparison with the traditional YSZ duplex and NiCrAlY bond coats10.1016/j.vacuum.2013.03.020 ↗
23. Hot corrosion behaviors of solution precursors and atmospheric plasma sprayed thermal barrier coatings10.1016/j.corsci.2015.05.034 ↗
24. ASTM E 1920-03 · 2014
25. ASTM B214-16 · 2016
26. Microstructure and properties of plasma-sprayed segmented thermal barrier coatings10.1111/j.1551-2916.2005.00912.x ↗
27. Effect of pores and interfaces on effective properties of plasma sprayed zirconia coatings10.1016/S1359-6454(03)00390-2 ↗
28. Correlation between young's modulus and porosity in porous materials10.1023/A:1006669914946 ↗
29. Comparison of hot corrosion resistance of Sm2Zr2O7 and (Sm0.5Sc0.5)Zr2O7 ceramics in Na2SO4 + V2O5 molten salt10.1016/j.ceramint.2016.05.190 ↗
30. Evaluation of hot corrosion behavior of SrHfO3 ceramic in the presence of molten sulfate and vanadate salt10.1016/j.jallcom.2017.08.279 ↗
31. Phase stability and hot corrosion behavior of ZrO2-Ta2O5 compound in Na2SO4-V2O5 mixtures at elevated temperatures10.1016/j.ceramint.2013.08.062 ↗
32. Zhu · 2011
33. Ropp · 2013 · 701
34. Degradations of yttria-stabilized zirconia thermal barrier coatings by vanadium pentoxide, phosphorous pentoxide, and sodium sulfate10.1111/j.1551-2916.2007.01941.x ↗
35. A comparative study on hot corrosion resistance of three types of thermal barrier coatings: YSZ, YSZ + Al2O3 and YSZ/Al2O310.1016/j.msea.2007.06.001 ↗
36. Evaluation of laser-glazed plasma-sprayed thermal barrier coatings under high temperature exposure to molten salts10.1016/j.surfcoat.2005.10.011 ↗