journal article·2014-11

Strength and toughness improvement in a C/SiC composite reinforced with slurry-prone SiC whiskers

Hui Mei, Huwei Wang, Hui Ding, Nan Zhang, Yuetang Wang, Shanshan Xiao, Qianglai Bai, Laifei Cheng

Ceramics International· Volume 40· Issue 9
Publisher page

Abstract

Abstract The present paper reports on the strength and toughness improvement in carbon-fiber reinforced silicon carbide (C/SiC) composites as a result of slurry-prone SiC whisker presence at varying concentrations. For whisker contents of 5 and 15 wt%, the SiC w –C/SiC composite flexural strength was found to increase by 98.5% and 64.3%, respectively, from the whisker-free case while work of fracture increased by 209.8% and 179.0%, respectively. For the same respective whisker concentrations, porosity was found to decrease by 4.9% and increase by 19.4% compared to plain samples. The composites’ interlaminar shear strength exhibited similar non-monotonic response with the property value for 5 wt% whisker-reinforced composites being higher by 12.5 MPa than the plain specimens and higher by 14.9 MPa than the composites with 15 wt% whisker content. Fiber pullout in SiC w –C/SiC composites was considerably more prominent than in the whisker-free material and the corresponding mean pullout lengths were significantly longer than in plain specimens. The improvements in strength and toughness were attributed to the energy dissipation mechanisms of crack deflection, whisker bridging and pullout coupled with conventional fiber pullout.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Innovative concrete reinforcement materials · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Composite thermostructures: an overview of the French experience
2. Preparation and characterization of 2D SiC/SiC composites with composition-graded C(B) interphase10.1016/S0955-2219(96)00216-6 ↗
3. Microstructure and mechanical properties of ZrB2–SiC–ZrO2f ceramic10.1016/j.scriptamat.2011.01.019 ↗
4. Dry sliding wear behaviors of La2O3–WSi2–MoSi2 composite against alloy steel10.1016/j.wear.2005.06.014 ↗
5. Influence of SiC whisker morphology and nature of SiC/Al2O3 interface on thermomechanical properties of SiC reinforced Al2O3 composites10.1016/j.jeurceramsoc.2004.09.026 ↗
6. High-resolution TEM characterization of SiC nanowires as reinforcements in a nanocrystalline Mg-matrix10.1016/j.matchar.2013.01.003 ↗
7. Thermal conductivity of SiC ceramic fabricated by liquid infiltrating molten Si into mesocarbon microbeads-based perform10.1016/j.matchar.2013.04.011 ↗
8. Morphological evolution of one-dimensional SiC nanomaterials controlled by sol–gel carbothermal reduction10.1016/j.matchar.2011.11.018 ↗
9. Interfacial microstructure and mechanical properties of TiAl and C/SiC joint brazed with TiH2–Ni–B brazing powder10.1016/j.matchar.2013.02.010 ↗
10. Fabrication of laminated SiCw/SiC ceramic composites by CVI10.1016/j.jeurceramsoc.2013.02.019 ↗
11. Fabrication and characterization of SiC whisker reinforced reaction bonded SiC composite10.1016/j.ceramint.2012.06.047 ↗
12. Microstructure and growth mechanism of SiC whiskers on carbon/carbon composites prepared by CVD10.1016/j.matlet.2005.02.088 ↗
13. Effect of SiC whiskers on microstructure and mechanical properties of the MoSi2–SiCw composites10.1016/j.ijrmhm.2013.06.007 ↗
14. Silicon carbide whisker reinforced silicon carbide composites by chemical vapor infiltration10.1016/j.msea.2006.05.050 ↗
15. Processing of ceramic matrix composites by pulsed-CVI and related techniques10.4028/www.scientific.net/KEM.159-160.359 ↗
16. A review of the pull-out mechanism in the fracture of brittle-matrix fibre-reinforced composites10.1177/096369350701600102 ↗
17. Crack deflection processes—I. Theory10.1016/0001-6160(83)90046-9 ↗
18. Direct measurement of fiber bridging in notched glass-ceramic-matrix composites10.1557/jmr.2006.0132 ↗
19. Debonding of interfaces between beta-silicon nitride whiskers and Si–Al–Y oxynitride glasses10.1016/S1359-6454(96)00069-9 ↗
20. On the toughening of ceramics by strong reinforcements10.1016/0001-6160(86)90146-X ↗
21. Toughening behavior in whisker-reinforced ceramic matrix composites10.1111/j.1151-2916.1988.tb05791.x ↗
22. Fabrication and fracture behavior of novel SiC ceramics having rodlike grains10.1111/j.1151-2916.1992.tb04224.x ↗
23. Intrinsic parameters in the fracture of carbon/carbon composites, Compos10.1016/j.compscitech.2004.10.021 ↗