Abstract

Abstract The 3D carbon fiber-reinforced mullite matrix (3D-Cf/mullite) composites were fabricated via sol–gel process, using mullite sols with high solid content as precursor. The mullitizaiton process of mullite sols was investigated with XRD and TEM. The results showed that the sol was transformed into orthorhombic mullite at 1300 °C with a trace of amorphous SiO 2 between crystals of mullite. The flexural strength, fracture toughness and interlaminar shear strength of 3D-Cf/mullite composites were 277.6 MPa, 12.3 MPa m 1/2 and 36.3 MPa, respectively. The 3D-Cf/mullite composites exhibited a significant tough fracture behavior. The oxidation resistance of 3D-Cf/mullite composites was examined. It can be found that the strength retentions of 3D-Cf/mullite composites were 62.9%, 84.8% and 13.6% after oxidation at 1300 °C, 1500 °C and 1700 °C, respectively. The strength transformation was interpreted with the microstructure analysis of oxidized 3D-Cf/mullite composites at different temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Processing and performance of an all-oxide ceramic composite10.1111/j.1151-2916.1998.tb02590.x ↗
2. Mechanical properties and oxidation resistance of SiCf/CVI-SiC composites with PIP-SiC interphase10.1016/j.ceramint.2012.01.045 ↗
3. Processing, structure, and properties of mullite fiber/mullite matrix composites10.1016/0955-2219(95)00136-0 ↗
4. Interface engineering in mullite fiber/mullite matrix composites10.1016/j.jeurceramsoc.2007.03.008 ↗
5. Effects of matrix porosity on the mechanical properties of a porous-matrix, all-oxide ceramic composite10.1111/j.1151-2916.2001.tb01059.x ↗
6. Effects of pyrolysis temperatures on the microstructure and mechancial properties of 2D-Cf/SiC composites using polycarbosilane10.1016/j.ceramint.2005.07.017 ↗
7. Mechanical property and microstructure evolutions of Cf/SiOC composites with increasing annealing temperature in reduced pressure environment10.1016/j.ceramint.2011.07.049 ↗
8. Continuous fibre reinforced mullite matrix composites by sol–gel processing: part I fabrication and microstructures10.1023/A:1018604229535 ↗
9. Microstructure and properties of Cf/SiC composites with thin SiCN layer as fiber-protecting coating10.1016/j.ceramint.2013.02.050 ↗
10. Continuous fibre reinforced mullite matrix composites by sol–gel processing: part II properties and fracture behaviour10.1023/A:1018630429960 ↗
11. Developments in oxide fiber composites10.1111/j.1551-2916.2006.01342.x ↗
12. Processing of oxide composites with three-dimensional fiber architectures10.1111/j.1551-2916.2009.03036.x ↗
13. Preparation of silicon–titanium–carbon–oxygen fabric/mullite filler/polytitanocarbosilane laminates by polymer impregnation and pyrolysis method10.1111/j.1551-2916.2004.00996.x ↗
14. A new concept for thermal protection of all-mullite composites in combustion chambers10.1016/S0955-2219(99)00265-4 ↗
15. Properties and microstructure of Nextel 720/SiC composites10.1016/j.ceramint.2004.06.024 ↗
16. Effects of combustor rig exposure on a porous-matrix oxide composite10.1111/j.1744-7402.2005.02015.x ↗
17. Performance of four ceramic-matrix composite divergent flap inserts following ground testing on an F110 turbofan engine10.1111/j.1151-2916.2000.tb01457.x ↗
18. Ceramics for future power generation technology: fiber reinforced oxide composites10.1016/S1359-0286(01)00017-1 ↗
19. Structure and properties of mullite – a review10.1016/j.jeurceramsoc.2007.03.017 ↗
20. Mechanical characterisation of mullite-based ceramic matrix composites at test temperatures up to 1200°C10.1016/S0955-2219(99)00250-2 ↗
21. High temperature behaviour of polycrystalline aluminosilicate fibres with mullite bulk composition. I. Microstructure and strength properties10.1016/0955-2219(95)00152-2 ↗
22. Thermal degradation of an oxide fibre (Nextel 720)/aluminosilicate composite10.1016/S0955-2219(03)00250-4 ↗
23. Effects of thermal aging on the mechanical properties of a porous-matrix ceramic composite10.1111/j.1151-2916.2002.tb00138.x ↗
24. Inorganic fibers – a literature review10.1111/j.1151-2916.1991.tb04289.x ↗
25. Al2O3–mullite–SiC–Al4SiC4 multi-composition coating for carbon/carbon composites10.1016/j.matlet.2004.03.046 ↗
26. Development and environmental durability of mullite and mullite/YSZ dual layer coatings for SiC and Si3N4 ceramics10.1016/S0257-8972(96)03074-5 ↗
27. Mullite based oxidation protection for SiC–C/C composites in air at temperatures up to 1900K10.1016/S0955-2219(98)00242-8 ↗
28. Characterisation of sol–gel derived alumina–silica matrices for continuous fibre reinforced composites10.1016/0955-2219(95)00183-2 ↗
29. Sol–gel control of matrix net-shape sintering in 3D fibre reinforced ceramic matrix composites10.1016/S0955-2219(97)89406-X ↗
30. Sol–gel mullite matrix–SiC and mullite 2D woven fabric composites with or without zirconia containing interphase: elaboration and properties10.1016/0955-2219(95)00189-1 ↗
31. Low temperature pressureless sintering of sol–gel derived mullite10.1016/S0921-5093(98)01094-6 ↗
32. Effect of precursor pH and sintering temperature on synthesizing and morphology of sol–gel processed mullite10.1016/S0272-8842(02)00077-9 ↗
33. Improvement of sintering and microstructural homogeneity of a diphasic mullite10.1016/S0955-2219(00)00280-6 ↗
34. Effect of carbon fiber pre-heat-treatment on the microstructure and properties of Cf/SiC composites10.1016/j.msea.2006.06.060 ↗
35. Properties and microstructure of KD-I/SiC composites by combined process of CVI/RB/PIP
36. Review of mullite synthesis routes by sol–gel method10.1007/s10971-010-2222-9 ↗
37. Correlation of the precursor type with densification behavior and microstructure of sintered mullite ceramics10.1016/S0955-2219(02)00176-0 ↗
38. Effect of composition on the sintering and microstructure of diphasic mullite gels10.1016/S0272-8842(99)00051-6 ↗
39. Formation of mullite from precursor powder: sintering, microstructure and Mechanical properties10.1016/S0921-5093(03)00049-2 ↗
40. SiC material produced by carbothermal reduction of a freeze gel silica–carbon artefact10.1016/S0955-2219(98)00223-4 ↗