Abstract

Abstract Al alloy/Ti3SiC2 composites with compressive strengths ranging from 743 to 932 MPa have been successfully fabricated by a new two-step pressureless infiltration method. 6061 Al alloy ribbons prepared by melt spinning were employed as the Al alloy matrix for melt infiltration. Shifts in phase constitution and reaction mechanisms of Ti3SiC2 preforms in molten Al at 950 °C were investigated, and the compression performance of Al alloy/Ti3SiC2 composites was tested. The Vickers hardness of the composites was enhanced to a maximum of 751 HV by increasing the Al content.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · MXene and MAX Phase Materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. In situ production of Al-TiB2 nanocomposite by double-step mechanical alloying10.1007/s10853-009-3335-9 ↗
2. Influence of ultrasonic assisted stir casting on mechanical properties of Al6061-nano Al2O3 composites
3. Enhanced thermal conductive 3D-SiC/Al-Si-Mg interpenetrating composites fabricated by pressureless infiltration10.1016/j.ceramint.2016.10.104 ↗
4. Improvement of particles distribution of in-situ 5vol% TiB2 particulates reinforced Al-4.5Cu alloy matrix composites with ultrasonic vibration treatment10.1016/j.jallcom.2016.09.013 ↗
5. Fabrication process and bending properties of carbon fibers reinforced Al-alloy matrix composites10.1016/j.jmatprotec.2016.01.007 ↗
6. Powder metallurgy processing and compressive properties of Ti3AlC2/Al composites10.1016/j.msea.2011.09.068 ↗
7. Compressive performance and crack propagation in Al alloy/Ti2AlC composites10.1016/j.msea.2016.06.073 ↗
8. Microstructure and mechanical properties of porous Ti3SiC210.1016/j.actamat.2005.05.034 ↗
9. Fabrication of Al2O3-Al composites by infiltration method and their characteristic10.1016/j.jmatprotec.2005.04.046 ↗
10. Wetting kinetics and bonding of Al and Al alloys on α-SiC10.1016/0921-5093(95)09896-8 ↗
11. Microstructures and properties of Al2O3/Al-AlN composites by pressureless infiltration of Al-alloys10.1016/S0921-5093(99)00180-X ↗
12. Microstructural characterization and compression properties of TiC0.61/Cu(Al) composite synthesized from Cu and Ti3AlC2 powders10.1016/j.jallcom.2014.02.159 ↗
13. Effect of rapid solidification on mechanical properties of a lead-free Sn-3.5Ag solder10.1016/j.jallcom.2010.05.179 ↗
14. Brazing of Si3N4 with amorphous Ti40Zr25Ni15Cu20 filler10.1016/j.msea.2008.11.056 ↗
15. Reaction of Al with Ti3SiC2 in the 800–1000°C temperature range10.1016/S0921-5093(00)01281-8 ↗
16. Wetting of TiC by molten Al at 1123–1323K10.1016/j.actamat.2010.11.055 ↗
17. Effect of excess silicon content on the formation of nano-layered Ti3SiC2 ceramic via infiltration of TiC preforms10.1016/j.jeurceramsoc.2016.09.004 ↗
19. Phase equilibria in the Al-Si-C system10.1007/BF02647073 ↗
20. Phase relations associated with the aluminum blast furnace: aluminum oxycarbide melts and Al-C-X (X=Fe, Si) liquid alloys10.1007/BF02656164 ↗
21. Phase stability of Ti3SiC2 at high pressure and high temperature10.1016/j.ceramint.2013.04.111 ↗
22. Experimental evidence of copper insertion in a crystallographic structure of Ti3SiC2 MAX phase10.1016/j.scriptamat.2015.03.015 ↗
23. A new aluminum silicon carbide formed in laser processing10.1023/A:1018653030270 ↗