Abstract The WC-8Ni powder was prepared by the ball milling method, then consolidated via a vacuum sintering technique. The influence of sintering temperature varying from 1375 °C up to 1500 °C on microstructure and mechanical properties of WC-8Ni cemented carbide was investigated. The best mechanical properties of the samples have been achieved at sintering temperature of 1450 °C. At which the relative density, hardness and fracture toughness (KIC) of the samples are 99.81%, 13.23 GPa and 24.22 MPa m1/2, respectively. The effect of η-phase identified by Murakami etching method and XRD technique on the mechanical properties was also discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Powder Metallurgy Techniques and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Potentials of nanostructured WC-Co cemented carbide as reference material for Vickers hardness10.1016/j.ijrmhm.2014.12.006 ↗
2. J. Lammle, W. Ferstl, G. Knunz, A. Lackner, Hardmetal in the toolmaking is a question of confidence, Plansee TIZIT AG Newsletter Edition, 2000.
3. Trends in the P/M hard metal industry10.1016/j.ijrmhm.2014.07.007 ↗
4. Toxicity of tungsten carbide and cobalt-doped tungsten carbide nanoparticles in mammalian cells in vitro10.1289/ehp.0800121 ↗
5. Anodic polarization and corrosion of cemented carbides with cobalt and nickel binders10.1007/BF01153988 ↗
6. Some aspects of the structure of cobalt and nickel binder phases in hardmetals10.1016/j.actamat.2010.12.004 ↗
7. Ultrafine WC–Ni cemented carbides fabricated by spark plasma sintering10.1016/j.msea.2011.10.119 ↗
8. WC grain growth and grain growth inhibition in nickel and iron binder hardmetals10.1016/S0263-4368(01)00070-1 ↗
9. Comparison of the friction and wear behaviour of WC–Ni–Co–Cr and WC–Co hardmetals in contact with steel at high temperatures10.1016/j.wear.2012.01.015 ↗
10. Microstructure and mechanical properties of WC Ni–Si based cemented carbides developed by powder metallurgy10.1016/j.ijrmhm.2010.04.003 ↗
11. Investigations on kinetics of formation of FCC-free surface layers on cemented carbides with Fe–Ni–Co binders10.1016/j.ijrmhm.2010.12.007 ↗
12. Microstructural evolution and its correlation with hardening of WC-Ni cemented carbides irradiated by high-intensity pulsed ion beam10.1016/j.surfcoat.2012.04.011 ↗
13. Influence of electrical discharge machining on sliding friction and wear of WC–Ni cemented carbide10.1016/j.triboint.2010.08.008 ↗
14. Corrosion and wear behavior of laser cladded Ni–WC coatings10.1016/j.surfcoat.2015.06.039 ↗
15. Mechanics and mechanisms of fatigue in a WC–Ni hardmetal and a comparative study with respect to WC–Co hardmetals10.1016/j.ijfatigue.2014.09.011 ↗
16. Microstructure and formation process of Ni-pool defect in WC–8Ni cemented carbides10.1016/S1003-6326(15)63676-7 ↗
17. Laser cladding assisted by induction heating of Ni–WC composite enhanced by nano-WC and La2O310.1016/j.ceramint.2014.06.097 ↗
18. Effect of high energy milling on the microstructure and properties of WC-Ni composite10.1590/S1516-14392010000300004 ↗
19. Hardness to toughness relationship of fine-grained WC-Co hardmetals10.1016/S0263-4368(98)00028-6 ↗
20. Upadhyaya · 1998
21. Grain growth, phase evolution and properties of NbC carbide-doped WC-10AISI304 hardmetals produced by pseudo hot isostatic pressing10.1016/j.jallcom.2012.10.060 ↗