Fracture toughness of ZrO2–SiC/MoSi2 composite ceramics prepared by powder metallurgy
Source abstract
Abstract
Abstract ZrO2–SiC/MoSi2 composite ceramics were prepared by powder metallurgy. The room temperature and high temperature fracture toughness of 10 vol%ZrO2+MoSi2, 10 vol%ZrO2+10 vol%SiC + MoSi2, 20 vol%ZrO2+10 vol%SiC + MoSi2, 10 vol%ZrO2+20 vol%SiC + MoSi2 composite ceramics were studied. The room temperature fracture toughness was calculated by Vickers indentation crack. High temperature fracture toughness is measured by wavefront interference principle of moire interferometry and non-contact measurement of in-plane displacement. The synergistic effects mechanism of nano-ZrO2 and SiC particles on the fracture toughness of MoSi2 nanocomposite ceramics was discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. UHTC–carbon fibre composites: preparation, oxyacetylene torch testing and characterization10.1016/j.jeurceramsoc.2012.08.018 ↗
2. Effects of Ti/Al addition on the microstructures and ablation properties of Cf/C–MoSi2–SiC composites10.1016/j.jeurceramsoc.2015.10.039 ↗
3. Effects of SiC or MoSi2 second phase on the oxide layers structure of HfB2-based composites10.1016/j.ceramint.2017.08.031 ↗
4. SiC/MoSi2 based coatings for Cf/C composites by two step pack cementation10.1016/j.jeurceramsoc.2018.01.024 ↗
5. Silicide-matrix materials for high-temperature applications
6. A comparative overview of molybdenum disilicide composites10.1016/0921-5093(92)90308-N ↗
7. Oxidation of MoSi2 and comparison with other silicide materials10.1016/0921-5093(92)90324-T ↗
8. Synthesis of dense mullite/MoSi2 composite for high temperature applications10.1016/j.ijrmhm.2014.03.006 ↗
9. Production of silicon carbide reinforced molybdenum disilicide composites using high-pressure sintering10.1016/j.ceramint.2020.06.137 ↗
10. Synthesis of molybdenum disilicide on molybdenum substrates10.1016/0257-8972(95)02524-3 ↗
11. High temperature oxidation and pesting of Mo(Si,Al)210.1016/S0921-5093(97)00673-4 ↗
12. One step synthesis of dense MoSi2–SiC composite by high-frequency induction heated combustion and its mechanical properties10.1016/j.jallcom.2004.10.072 ↗
13. Intrinsic second-phase particles in powder-processed MoSi210.1016/0921-5093(91)90235-F ↗
14. Effects of carbon additions on the high temperature mechanical properties of molybdenum disilicide10.1016/0921-5093(92)90323-S ↗
15. Carbon additions to molybdenum disilicide: improved high-temperature mechanical properties10.1111/j.1151-2916.1991.tb06829.x ↗
16. The intermediate and high-temperature oxidation behaviour of Mo(Si1−xAlx)2 intermetallic alloys10.1016/S0966-9795(96)00068-4 ↗
17. First principles study on the phase stability and mechanical properties of MoSi2 alloyed with Al, Mg and Ge10.1016/j.intermet.2015.07.008 ↗
18. Microstructure and oxidation resistance of Mo-Si and Mo-Si-Al alloy coatings prepared by electro-thermal explosion ultrahigh speed spraying10.1016/j.msea.2009.04.026 ↗
19. High temperature oxidation of Mo-Si-X intermetallics (X=Al, Ti, Ta, Zr and Y)10.1016/0966-9795(95)98935-2 ↗
20. On the ductile-to-brittle transition temperature in MoSi210.1016/0956-716X(92)90224-3 ↗
21. Oxidation behavior of Mo-Si-B alloys in wet air10.1016/j.msea.2003.12.025 ↗
22. Structure and properties of ultrafine-grained MoSi2 + Si3N4 composites synthesized by mechanical alloying10.1016/j.msea.2007.07.021 ↗
23. Development and characterization of SiC(f)/MoSi2–Si3N4(p) hybrid composites10.1016/S0921-5093(98)01046-6 ↗
24. Properties and densification of nanocrystalline MoSi2-Si3N4 composite from mechanically alloyed powders by pulsed current-activated sintering10.1016/j.jallcom.2010.04.120 ↗
25. Consolidation and mechanical properties of nanostructured MoSi2-SiC-Si3N4 from mechanically activated powder by high frequency induction heated sintering10.1016/j.msea.2010.10.063 ↗
26. Effect of nano-ZrO2 on the microstructure and high temperature tribological properties of MoSi2 coating10.1007/s11666-013-9924-9 ↗
27. Manufacturing of composite coatings by atmospheric plasma spraying using different feed-stock materials as YSZ and MoSi210.1007/s11666-017-0537-6 ↗
28. Thermal cycling and reactivity of a MoSi2/ZrO2 composite designed for self-healing thermal barrier coatings10.1016/j.matdes.2016.01.054 ↗
29. Prediction of the mechanical properties of MoSi2 doped with Cr, Nb and W from first-principles calculations10.1016/j.jallcom.2017.04.271 ↗
30. A Si-Mo-W coating to protect SiC-coated carbon/carbon composites against oxidation10.1111/j.1551-2916.2009.03144.x ↗
31. Interaction in the MoSi2-W system at 1500 to 1800°C10.1007/s11106-009-9092-0 ↗
32. Kinetics and oxidation mechanism of MoSi2–MoB ceramics in the 600–1200 °C temperature range10.1016/j.ceramint.2017.05.093 ↗
33. Improvement of MoSi2 oxidation resistance via boron addition: fabrication of MoB/MoSi2 composite by mechanical alloying and subsequent reactive sintering10.1016/j.powtec.2014.01.034 ↗
34. Self-propagating high-temperature synthesis of advanced ceramics MoSi2-HfB2-MoB10.1016/j.ceramint.2018.09.138 ↗
35. High-temperature oxidation and plasma torch testing of MoSi2-HfB2-MoB ceramics with single-level and two-level structure10.1016/j.corsci.2019.07.001 ↗
36. Influence of mechanical activation of reactive mixtures on the microstructure and properties of SHS-ceramics MoSi2-HfB2-MoB10.1016/j.ceramint.2019.07.009 ↗
37. Oxidation-resistance of ZrB2-MoSi2 composite coatings prepared by atmospheric plasma spraying
38. Mechanical and electrical properties of MoSi2-based ceramics with various ZrB2-20vol% SiC as additives for ultra high temperature heating element10.1016/j.ceramint.2017.10.043 ↗
39. Effects of microstructures and flaw evolution on the fracture strength of ZrB2-MoSi2 composites under high temperatures10.1016/j.jallcom.2015.05.027 ↗
40. An investigation on the in situ synthesis–sintering and mechanical properties of MoSi2–xSiC composites prepared by spark plasma sintering10.1016/j.ijrmhm.2014.09.020 ↗
41. Enhanced bonding strength and thermal cycling performance of MoSi2–CrSi2–SiC–Si coating for carbon/carbon composites by surface modification via blasting treatment10.1016/j.ceramint.2016.06.008 ↗
42. Formation mechanism and oxidation behavior of MoSi2–SiC protective coating prepared by chemical vapor infiltration/reaction10.1016/S1003-6326(13)62702-8 ↗
43. Microstructure, sintering behavior and mechanical properties of SiC/MoSi2 composites by spark plasma sintering10.1016/S1003-6326(18)64730-2 ↗
44. Effect of SiC whiskers on microstructure and mechanical properties of the MoSi2-SiCw composites10.1016/j.ijrmhm.2013.06.007 ↗
45. Synthesis and properties of MoSi2-MoB-SiC ceramics10.1111/jace.14163 ↗
46. Mechanical and electrical properties of MoSi2-based ceramics with various ZrB2-20vol% SiC as additives for ultra high temperature heating element10.1016/j.ceramint.2017.10.043 ↗
47. Advanced materials for ultrahigh temperature structural applications
48. Toughening strategies for MoSi2-based high temperature structural silicides10.1016/S0966-9795(00)00044-3 ↗
49. Creep behaviour of MoSi2–SiC and MoSi2–HfO210.1016/S0167-577X(01)00340-8 ↗
50. Moire interferometry near the theoretical limit10.1364/AO.21.001621 ↗
51. Microstructure and mechanical properties of spark plasma sintered zirconia-hydroxyapatite nano-composite powders10.1016/j.actamat.2005.01.039 ↗
52. Recent applications of moiré interferometry10.1007/s11340-010-9404-9 ↗
53. Study of effect of 90° domain switching on ferroelectric ceramics fracture using the moiré interferometry10.1016/j.actamat.2007.03.005 ↗
54. Comprehensive handbook of ternary alloy phase diagrams10.1007/BF02881177 ↗
55. Dense layered molybdenum disilicide-silicon carbide functionally graded composites formed by field-activated synthesis10.1111/j.1151-2916.2001.tb00775.x ↗
56. Structure and properties of MoSi2–MeB2–SiC (Me = Zr, Hf) ceramics produced by combination of SHS and HP techniques10.1016/j.ceramint.2020.08.033 ↗
57. Electrical percolation and infrared emissivity of pressureless sintered SiC-MoSi2 composites tailored by sintering temperature10.1016/j.jeurceramsoc.2019.05.019 ↗
58. Materials discovery at high pressures10.1038/natrevmats.2017.5 ↗
59. Combustion wave structure during the MoSi2 synthesis by mechanically-activated self-propagating high-temperature synthesis (MASHS): in situ time-resolved investigations10.1016/j.intermet.2005.09.001 ↗
60. Effect of thermodynamically metastable components on mechanical and oxidation properties of the thermal-sprayed MoSi2 based composite coating10.1016/j.corsci.2019.04.041 ↗
61. Synthesis, microstructure and properties of MoSi2–5 vol%Al2O3 composites10.1016/j.ceramint.2014.07.142 ↗
62. In-situ preparation of nano MoSi2-SiC composite by melt infiltration of silicon method10.1016/j.matchemphys.2017.05.052 ↗
63. Effect of starting composition on formation of MoSi2-SiC nanocomposite powder via ball milling10.1007/s12034-012-0342-2 ↗
64. In situ pressureless sintering of SiC/MoSi2 composite10.1016/j.ceramint.2011.11.046 ↗
65. Microstructure, sintering behavior and mechanical properties of SiC/MoSi2 composites by spark plasma sintering10.1016/S1003-6326(18)64730-2 ↗