Abstract Unidirectional carbon fiber-reinforced zirconium diboride based composites were fabricated by hot pressing. The fiber–matrix interface was tailored by pre-coating the as-received carbon fibers with pyrolytic carbon (PyC) coatings of various thickness or silicon carbide (SiC) coating. The effects of the interfacial characteristics on mechanical properties and microstructure of the composites were studied. The results indicated that both the composites reinforced with as-received carbon fibers and SiC coated carbon fibers showed inferior flexural strength and fracture toughness. With optimized PyC coating thickness, the mechanical properties of the composites had been remarkably improved, i.e. a flexural strength of 309.6 MPa was achieved when the thickness of PyC coating was 0.1 μm, and a fracture toughness of 6.72 MPa m 1/2 was obtained when the PyC coating was 0.7 μm thick.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Zirconium diboride
2. Materials for ultrahigh temperature structural applications
3. Evaluation of ultra-high temperature ceramics for aeropropulsion use10.1016/S0955-2219(02)00140-1 ↗
4. Fabrication, mechanical properties and thermal shock resistance of a ZrB2–graphite ceramic10.1016/j.ijrmhm.2010.12.014 ↗
5. Mechanical properties of short carbon fiber reinforced ZrB2–SiC ceramic matrix composites10.1016/j.matlet.2008.01.076 ↗
6. Thermal and electrical properties of hot-pressed short pitch-based carbon fiber-reinforced ZrB2–SiC matrix composites10.1016/j.ceramint.2012.12.091 ↗
7. Microstructure and toughening mechanisms in spark plasma-sintered ZrB2 ceramics reinforced by SiC whiskers or SiC-chopped fibers10.1111/j.1551-2916.2010.03730.x ↗
8. Toughened ZrB2-based ceramics through SiC whisker or SiC chopped fiber additions10.1016/j.jeurceramsoc.2009.11.012 ↗
9. Influence of milling time on the synthesis, microstructure and mechanical properties of ZrB2–SiC–ZrO2f ceramic composites10.1016/j.ceramint.2012.11.003 ↗
10. Microstructure and mechanical properties of silicon carbide monofilament reinforced zirconium diboride matrix composites10.1016/j.ceramint.2012.07.018 ↗
11. Preparation and characterization of C/SiC–ZrB2 composites by precursor infiltration and pyrolysis process10.1016/j.ceramint.2009.11.015 ↗
12. Oxidation behavior of ZrB2–MoSi2–SiC composites in air at 1500°C10.1016/j.ceramint.2010.09.034 ↗
13. Fabrication of SiCw reinforced ZrB2-based ceramics10.1016/j.ceramint.2010.03.006 ↗
14. Elastic properties of spark plasma sintered (SPSed) ZrB2–ZrC–SiC composites10.1016/j.ceramint.2007.06.010 ↗
15. The mechanical-behavior of ceramic matrix composites10.1016/0001-6160(89)90291-5 ↗
16. The role of interfaces in fiber-reinforced brittle matrix composites10.1016/0266-3538(91)90010-M ↗
17. The influence of the interphase and associated interfaces on the deflection of matrix cracks in ceramic matrix composites10.1016/S1359-835X(00)00095-6 ↗
18. Influence of fiber coating thickness on fracture behavior of continuous woven Nicalon® fabric-reinforced silicon-carbide matrix ceramic composites10.1016/S0921-5093(01)01184-4 ↗
19. Influence of pyrolytic carbon interface thickness on microstructure and mechanical properties of SiC/SiC composites by NITE process10.1016/j.compscitech.2007.05.037 ↗
20. Strong interface in CMCs, a condition for efficient multilayered interphases
21. The design of the fibre–matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
22. Reinforcing effect of carbon short fibers coated with pyrolytic carbon in ceramic matrix composites10.1177/0021998307075437 ↗
23. Mechanical properties of thin pyrolitic carbon interphase SiC-matrix composites reinforced with near-stoichiometric SiC fibers10.1111/j.1551-2916.2005.00546.x ↗
24. Boron-nitride interphase in ceramic–matrix composites10.1111/j.1151-2916.1991.tb06789.x ↗
25. Evaluating the effect of oxygen content in BN interfacial coatings on the stability of SiC/BN/SiC composites10.1016/S1359-835X(98)00135-3 ↗
26. Coating of carbon short fibers with thin ceramic layers by chemical vapor deposition10.1016/j.tsf.2006.02.001 ↗
27. Mechanical properties of 3D KD-I SiCf/SiC composites with engineered fibre–matrix interfaces10.1016/j.compscitech.2011.01.014 ↗
28. Carbon with high thermal conductivity, prepared from ribbon-shaped mesosphase pitch-based fibers10.1016/j.carbon.2006.01.015 ↗
29. Chemical vapour deposition of coatings10.1016/S0079-6425(01)00009-3 ↗
30. Interfaces and interfacial mechanics-influence on the mechanical-behavior of ceramic–matrix composites (CMC)10.1051/jp4:19937252 ↗