Densification, microstructure and mechanical properties of SiO2–cBN composites by spark plasma sintering

Jianfeng Zhang, Rong Tu, Takashi Goto

Ceramics International· Volume 38· Issue 1
Publisher page

Abstract

Abstract SiO 2 –cBN composites were consolidated by spark plasma sintering at 1473–1973 K. The effects of cBN content and sintering temperature on the relative density, phase transformation, microstructure and mechanical properties of the SiO 2 –cBN composites were investigated. The relative density of the SiO 2 –cBN composites increased with increasing SiO 2 content. The phase transformation of cBN to hBN in SiO 2 –cBN composites was identified at 1973 K, showing the highest transformation temperature in cBN-containing composites. The SiO 2 –20 vol% cBN composites sintered at 1673 K showed the highest hardness and fracture toughness of 12.5 GPa and 1.5 MPa m 1/2 , respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Bioactive glass ceramics: properties and applications10.1016/0142-9612(91)90194-F ↗
2. Structure and properties of amorphous silica and its related materials: recent developments and future directions10.2109/jcersj.113.17 ↗
3. A survey of energy and environmental applications of glass10.1016/j.jeurceramsoc.2008.08.011 ↗
4. Sintered superhard materials10.1126/science.208.4446.873 ↗
5. Pierson · 1996
6. Densification and phase transformation of β-SiAlON–cubic boron nitride composites prepared by spark plasma sintering10.1111/j.1551-2916.2009.03098.x ↗
7. Densification: phase transformation and hardness of mullite–cubic BN composites prepared by spark plasma sintering10.2109/jcersj2.118.157 ↗
8. Preparation and microstructure of a ZrB2–SiC composite fabricated by the spark plasma sintering–reactive synthesis (SPS–RS) method10.1111/j.1551-2916.2007.02050.x ↗
9. Microstructure and densification of ZrB2–SiC composites prepared by spark plasma sintering10.1016/j.jeurceramsoc.2009.01.011 ↗
10. Highly transparent lutetium titanium oxide produced by spark plasma sintering
11. Formation of a unique glass by spark plasma sintering of a zeolite10.1557/jmr.2009.0385 ↗
12. Influence of iron powder particle size on the microstructure and properties of Fe3Al intermetallics prepared by mechanical alloying and spark plasma sintering10.1016/j.msea.2006.05.024 ↗
13. JCPDS, International Centre for Diffraction Data, No. 27-0605.
14. JCPDS, International Centre for Diffraction Data, No. 25-1033.
15. Equilibrium penny-like cracks in indentation fracture10.1007/BF00557479 ↗
16. Elastic/plastic indentation hardness and indentation fracture toughness: the inclusion core model10.1007/BF01233154 ↗
17. Spark plasma sintering of Al2O3–cBN composites assisted by precipitating Ni nanoparticle precipitated by rotary chemical vapor deposition10.1016/j.jeurceramsoc.2011.05.019 ↗
18. Hot isostatic pressing of cubic boron nitride–tungsten carbide/cobalt (cBN–WC/Co) composites: effect of cBN particle size and some processing parameters on their microstructure and properties10.1111/j.1551-2916.2006.01426.x ↗
19. Densification and microstructure of Al2O3–cBN composites prepared by spark plasma sintering10.2109/jcersj2.116.744 ↗
20. Spark plasma sintering of TiN–cubic BN composites10.2109/jcersj2.118.137 ↗
21. Spark plasma sintering of βSiAlON–cBN composite10.4028/www.scientific.net/MSF.561-565.599 ↗
22. Stoer silica particle size effect on the hardness and brittleness of silica monoliths10.1016/j.colsurfa.2007.02.061 ↗