Abstract

Abstract By using nano-infiltration and transient eutectic (NITE) phase with nanosized SiC and the addition of CeO2–Al2O3 as joining material, liquid-phase-sintered SiC ceramics were joined at the relatively low temperature of 1500 °C and 1700 °C. For comparison purpose, Al2O3–Y2O3 and SiO2–Al2O3–Y2O3 were used as the additives to join SiC ceramics. The shear strength of SiC assembly with the interlayer thickness of ~70 μm and addition of CeO2–Al2O3 after joining at 1700 °C was measured to be 163.9 MPa but decreased to 57.4 MPa when joining at 1500 °C. It was revealed that the joining status could be improved by decreasing the thickness of the interlayer to ~35 μm and SiC joint finishing at 1500 °C possessed the comparatively high shear strength of 113.2 MPa. NITE phase containing other additives (Al2O3–Y2O3 and SiO2–Al2O3–Y2O3) showed the much lower shear strength after joining at 1500 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Creep and microstructural evolution at high temperature of liquid phase-sintered silicon carbide10.1111/j.1551-2916.2006.01350.x ↗
2. Thermal shock resistance and fracture toughness of liquid-phase-sintered SiC-based ceramics10.1016/j.jeurceramsoc.2009.01.021 ↗
3. Current status of SiC/SiC composites R & D10.1016/S0022-3115(98)00303-1 ↗
4. Design and material issues for high performance SiCf/SiC-based fusion power cores10.1016/S0920-3796(01)00181-8 ↗
5. High temperature mechanical behaviour of liquid phase sintered silicon carbide10.1016/S0955-2219(97)00163-5 ↗
6. Advanced LWR nuclear fuel cladding system development trade-off study
7. Development of joining and coating technique for SiC and SiC/SiC composites utilizing NITE processing10.1002/9780470291221.ch47 ↗
8. Bonding mechanism between silicon carbide and thin foils of reactive metals10.1007/BF00552387 ↗
9. Joining of SiC ceramic-based materials with ternary carbide Ti3SiC210.1016/j.mseb.2010.09.002 ↗
10. Joining machined SiC/SiC composites for thermonuclear fusion reactors10.1016/j.jnucmat.2008.02.020 ↗
11. Fabrication and characterization of joined silicon carbide cylindrical components for nuclear applications10.1016/j.jnucmat.2014.11.071 ↗
12. A heat-resistant preceramic polymer with broad working temperature range for silicon carbide joining10.1016/j.jeurceramsoc.2017.08.033 ↗
13. Residual thermal stress of SiC/Ti3SiC2/SiC joints calculation and relaxed by postannealing10.1111/ijac.12900 ↗
14. The influence of sintering additives on the irradiation resistance of NITE SiC10.1016/j.jnucmat.2010.12.181 ↗
15. Effects of neutron irradiation on mechanical properties of silicon carbide composites fabricated by nano-infiltration and transient eutectic-phase Process10.1016/j.jnucmat.2013.10.005 ↗
16. Joining of silicon carbide composites for fusion energy applications10.1016/S0022-3115(00)00247-6 ↗
17. M3FT-16OR020202112-Report on viability of hydrothermal corrosion resistant SiC/SiC Joint development
18. R&D of joining technology for SiC components with channel10.1016/j.jnucmat.2008.12.263 ↗
19. Pressureless sintering of β-SiC with Al2O3 additions10.1007/BF00351412 ↗
20. Low temperature spark plasma densification of nano-SiC powder with novel Al2O3-Ho2O3 additives for SiC/SiC applications10.1016/j.ceramint.2016.05.019 ↗
21. Sintering and oxidation resistance of compositions in the SiC-La2O3-Al2O3-Cr2O3 system. I. Pressureless sintering of compositions in the SiC-La2O3-Al2O3-Cr2O3 system at low temperatures10.1016/S0272-8842(99)00080-2 ↗
22. Low temperature pressureless sintering of ɑ-SiC with Al2O3 and CeO2 as additives10.1016/j.jeurceramsoc.2013.09.015 ↗
23. Electric current activated/assisted sintering (ECAS): a review of patents 1906-200810.1088/1468-6996/10/5/053001 ↗
24. Effects of additives on densification, microstructure and properties of liquid-phase sintered silicon carbide10.1023/A:1004881430804 ↗
25. Recent advances in joining of SiC-based materials (monolithic SiC and SiCf/SiC composites): joining processes, joint strength, and interfacial behaviour10.1007/s40145-018-0297-x ↗