Abstract In this study, 2.5 dimensional KD-II silicon carbide fiber-reinforced silicon dioxide (2.5D (SiC f /SiO 2 )) ceramic matrix composites with zirconium dioxide (ZrO 2 ) coating were successfully fabricated by sol–gel process. Effects of ZrO 2 coating on the flexural strength of the composites were comprehensively investigated. Results showed that the flexural strength of the ZrO 2 -coated SiC f /SiO 2 composites was approximately twice that of composites without coating. Moreover, the strength of the composites tested at 1200 °C increased approximately by 12% than that of the samples tested at room temperature. Further, the oxidation behavior of the composites was also investigated at high temperatures corresponding to 1300 and 1500 °C, which showed an increase in the bonding strength between SiC fibers and SiO 2 matrix. The evolution of microstructure revealed that ZrO 2 coating led to an increase in the surface roughness of fibers owing to the effective bonding between fibers and matrix.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Silicon carbide fibers and their potential for use in composite materials, Part 110.1016/0010-4361(84)90956-X ↗
2. Research development of fabrication techniques and properties of SiCf/SiC ceramic matrix composite (in Chinese)
3. Fabrication of SiCf/SiO2 composites and the influence of interface on the mechanical properties (in Chinese)
4. Mechanical performance of SiCf/SiO2 composite fabricated by impregnation method (in Chinese)
5. Fabrication of SiCf/SiC composites by chemical vapor infiltration and vapor silicon infiltration10.1016/j.matlet.2010.05.013 ↗
6. Dielectric properties of the SiC fiber-reinforced SiC matrix composites with the CVD SiC interphases10.1016/j.jallcom.2009.09.163 ↗
7. Strength enhancement of 2D-SiCf/SiC composites after static fatigue at room temperature10.1016/j.jeurceramsoc.2007.02.180 ↗
8. Synthesis of boron nitride coatings on quartz fibers: thickness control and mechanism research
9. Application of sol–gel processing techniques for the manufacture of fiber-reinforced ceramics10.1111/j.1151-2916.1993.tb03992.x ↗
10. The influence of the interphase and associated interfaces on the deflection of matrix cracks in ceramic matrix composites10.1016/S1359-835X(00)00095-6 ↗
11. Mechanical properties of 3D KD-I SiCf/SiC composites with engineered fiber–matrix interfaces10.1016/j.compscitech.2011.01.014 ↗
12. The concept of a strong interface applied to SiC/SiC composites with a BN interphase10.1016/S1359-6454(00)00247-0 ↗
13. Deposition of BN interphase coatings from B-trichloroborazine and its effects on the mechanical properties of SiC/SiC composites10.1016/j.apsusc.2010.08.047 ↗
14. Oxidation mechanisms and kinetics of 1D-SiC/C/SiC composite materials: i, experimental approach10.1111/j.1151-2916.1994.tb07015.x ↗
15. Boron nitride interphase in ceramic matrix composites10.1111/j.1151-2916.1991.tb06789.x ↗
16. Oxidation of BN-coated SiC fibers in ceramic matrix composites10.1111/j.1151-2916.1996.tb08163.x ↗
17. R.L.CallenderA.R.Barron, Novel route to alumina and aluminate interlayer coatings for SiC, carbon and Kevlar1 fiber reinforced ceramic matrix composites using carboxylate-alumoxane nanoparticles, Journal of material research, 15, 2000, pp. 2228–223710.1557/JMR.2000.0320 ↗
18. Microstructure and mechanical behavior of an hibonite interphase in alumina-based composites10.1002/9780470314784.ch4 ↗
19. Preparation and characterization of chemically vapor deposited ZrO2 coating on nickel and ceramic fiber substrates10.1111/j.1151-2916.1997.tb03022.x ↗
20. Multilayered oxide interphase concept for ceramic-matrix composites10.1111/j.1151-2916.1998.tb02396.x ↗
21. Morphological evolution and weak interface development within chemical-vapor-deposited zirconia coating deposited on Hi-NicalonTM fiber10.1111/j.1151-2916.2002.tb00312.x ↗
22. Effects of oxygen partial pressure on the nucleation behavior and morphology of chemically-vapor-deposited zirconia on Hi-Nicalon fiber and Si10.1111/j.1151-2916.2003.tb03604.x ↗
23. Tensile and stress-rupture behavior of SiC/SiC minicomposite containing chemically vapor deposited zirconia interphase10.1111/j.1551-2916.2004.01726.x ↗
24. The yttria stabilized zirconia interfacial coating on NicalonTM fiber10.1016/j.jeurceramsoc.2005.03.241 ↗
25. The oxidation resistance of the oxide-coated NicalonTM fibers10.4028/www.scientific.net/KEM.287.477 ↗
26. Micro-oxidation treatment to improve bonding strength of Sr and Na co-substituted hydroxyapatite coatings for carbon/carbon composites10.1016/j.apsusc.2016.03.216 ↗
27. Mechanical and dielectric properties of SiCf/SiC composites fabricated by PIP combined with CIP process10.1016/j.ceramint.2016.01.057 ↗
28. Effect of intermediate heat treatment on mechanical properties of SiCf/SiC composites with BN interphase prepared by ICVI10.1016/j.jeurceramsoc.2010.12.018 ↗
29. Processing and properties of a porous oxide matrix composite reinforced with continuous oxide fibers10.1111/j.1151-2916.2003.tb03548.x ↗
30. Effects of thermal aging on the mechanical properties of a porous-matrix ceramic composite10.1111/j.1151-2916.2002.tb00138.x ↗
31. AlPO4-coated mullite/alumina fiber reinforced reaction-bonded mullite composites10.1016/j.jeurceramsoc.2008.05.032 ↗
32. Developments in oxide fiber composites10.1111/j.1551-2916.2006.01342.x ↗
33. Oxidation behavior of oxidation protective coatings for PIP–C/SiC composites at 1500°C10.1016/j.ceramint.2011.06.063 ↗
34. Fabrication and high-temperature properties of SiO2f/SiO2 composites by sol–gel10.1016/j.ceramint.2016.05.043 ↗