Abstract

Abstract The influence of sintering temperature and soaking time on fracture toughness of Al 2 O 3 ceramics has been investigated. The samples were prepared by solid state sintering at 1500, 1600 and 1700 °C for different soaking time periods. The fracture toughness of the sintered samples was determined by inducing cracks using Vickers indentation technique. Microstructural investigations on fracture surfaces obtained by three point bend test mode were made and correlated with fracture toughness. Crack deflection in the samples sintered at 1500 and 1600 °C for which ranges of fracture toughness are 5.2–5.4 and 5.0–5.6 MPa m 1/2 respectively, are found. The samples sintered at 1700 °C have lower fracture toughness ranging between 4.6 and 5.0 MPa m 1/2 . These samples have larger grains and transgranular fracture mode is predominant. The crack deflection has further been revealed by SEM and AFM observations on fracture surface and fracture surface roughness respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Effects of rare earth dopants on grain boundary bonding in alumina–silicon carbide composites10.1016/S0955-2219(03)00198-5 ↗
2. Effect of second phase on mechanical properties and toughening of Al2O3 based ceramic composites10.1016/0961-9526(95)00069-Y ↗
3. The effect of rare earth dopants on grain boundary cohesion in alumina10.1016/j.jeurceramsoc.2006.07.001 ↗
4. Research on toughening mechanisms of alumina matrix ceramic composite materials improved by rare earth additive10.1016/S1002-0721(08)60097-6 ↗
5. Toughening and strengthening of alumina with silver inclusions10.1016/0955-2219(95)90351-I ↗
6. Influence factors on wear resistance of two alumina matrix composites10.1016/j.wear.2007.08.011 ↗
7. Crack stability and strength variability in alumina ceramics with rising toughness-curve behavior10.1016/S1359-6454(99)00350-X ↗
8. Fracture toughness and crack bridging of a silicon nitride ceramic10.1016/0955-2219(91)90028-X ↗
9. Microstructural design of toughened ceramics10.1111/j.1151-2916.1991.tb06872.x ↗
10. Influence of a liquid phase on the microstructure development of Al2O310.1007/BF00592716 ↗
11. Synthesis, evaluation and characterization of alumina ceramics with elongated grains10.1016/j.ceramint.2004.10.008 ↗
12. Fracture toughness enhancement for alumina systems: a review10.1111/j.1744-7402.2008.02224.x ↗
13. Grain size dependences of Vickers microhardness and fracture toughness in A12O3 and Y2O3 ceramics10.1016/S0272-8842(86)80007-4 ↗
14. Fracture surface roughness of Al2O3–plateler reinforced glass matrix composites10.1016/S1359-835X(01)00080-X ↗
15. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
16. Hardness-grain size relation in ceramics10.1111/j.1151-2916.1994.tb04641.x ↗
17. Temperature and porosity effects on the fracture of fine grain size MgO10.1007/BF00553244 ↗
18. The temperature-dependence of the strength of polycrystalline MgO10.1007/BF00550995 ↗
19. Microstructure and mechanical properties of Al2O3–MgB2 composites10.1016/j.ceramint.2004.03.040 ↗
20. Effect of grain boundary dopants and mean grain size on tribomechanical behavior of highly purified α-alumina in the mild wear regime10.1016/0043-1648(94)07043-1 ↗
21. Fracture-mode change in alumina-silicon carbide composites doped with rare-earth impurities10.1111/j.1151-2916.2003.tb03556.x ↗
22. Microstructure and fracture toughness of liquid-phase-sintered β-SiC containing β-SiC whiskers as seeds10.1023/A:1022812427677 ↗
23. Toughening of SiC ceramics by a bimodal grain size distribution produced by hiping ultrafine and coarse grained SiC powders10.1016/0965-9773(95)00202-2 ↗