Abstract

Abstract The low fracture toughness of ceramic coatings has always hindered their wide application. In this study, an in-situ nanocomposite coating was prepared by the atmospheric plasma spraying of a 50 wt% Ti3AlC2-50 wt% Cu mixed powder. The in-situ nanocomposite coating was found to have an unusual microstructure with a nano-micrometre phase synergistic enhancement, which consisted of submicrometre-thick layers of Cu and nanoparticles of Cu(Al), Ti4O5, TiO2, and Al2TiO5. Thus, in the spraying process, Al was delinked out of Ti3AlC2, forming a large amount of plastic Cu(Al) with Cu. The delinked channel provided a path for Cu to diffuse into Ti3AlC2, which a spatial Cu network structure was formed in the coating. The in-situ nanocomposite coating has high fracture toughness and crack growth resistance by a three-point bending test. This paper reports a new method to prepare a high-fracture-toughness composite ceramic coating.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Indentation properties of plasma sprayed Al2O3–13%TiO2 nanocoatings10.1016/j.actamat.2009.03.020 ↗
2. Effects of critical plasma spray parameter and spray distance on wear resistance of Al2O3–8wt.%TiO2 coatings plasma-sprayed with nanopowders10.1016/j.surfcoat.2008.01.002 ↗
3. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
4. A sintering model for plasma-sprayed zirconia thermal barrier coatings. Part II: coatings bonded to a rigid substrate10.1016/j.actamat.2008.10.058 ↗
5. Hot corrosion behaviour of La2(Zr0.7Ce0.3)2O7 thermal barrier coating ceramics exposed to molten calcium magnesium aluminosilicate at different temperatures10.1016/j.corsci.2015.08.031 ↗
6. Calcium-magnesium-alumino-silicate induced degradation and failure of La2(Zr0.7Ce0.3)2O7/YSZ double-ceramic–layer thermal barrier coatings prepared by electron beam-physical vapor deposition10.1016/j.jeurceramsoc.2017.10.057 ↗
7. Ceramic top coats of plasma-sprayed thermal barrier coatings: materials, processes, and properties10.1007/s11666-017-0597-7 ↗
8. On the compatibility of single crystal superalloys with a thermal barrier coating system10.1016/j.actamat.2007.07.057 ↗
9. Comparison of flame sprayed Al2O3/TiO2 coatings: their microstructure, mechanical properties and tribology behavior10.1016/j.surfcoat.2006.02.011 ↗
10. Effects of micro-grooves on tribological behaviour of plasma-sprayed alumina-13%titania coatings10.1016/j.ceramint.2017.02.052 ↗
11. Strong, tough and stiff bioinspired ceramics from brittle constituents10.1038/nmat3915 ↗
12. The conflicts between strength and toughness10.1038/nmat3115 ↗
13. Fibrous monolithic ceramics10.1111/j.1151-2916.1997.tb03148.x ↗
14. Surface engineering design of alumina/molybdenum fibrous monolithic ceramic to achieve excellent lubrication in a high vacuum environment10.1007/s11249-018-1021-2 ↗
15. Plastic metallic-barrier layer for crack propagation within plasma-sprayed Cu/ceramic coatings10.1016/j.surfcoat.2018.12.124 ↗
16. Escape from the strength-to-toughness paradox: bulk ceramics through dual composite architectures10.1016/j.jeurceramsoc.2018.02.003 ↗
17. Enhanced interface adhesion by in-situ oxidation within metal-ceramic coatings10.1016/j.ceramint.2018.08.332 ↗
18. Heat-induced interface-coupling behaviour of thermally sprayed Cu/ceramic coatings10.1016/j.ceramint.2018.03.212 ↗
19. Effects of the metal-ceramic transition region on the mechanical properties and crack propagation behavior of an Al2O3-40wt%TiO2 coating10.1016/j.surfcoat.2017.04.058 ↗
20. Fracture behaviour of ceramic–metallic glass gradient transition coating
21. Fabrication and properties of plasma-sprayed Al2O3/TiO2 composite coatings: a role of nano-sized TiO2 addition10.1016/j.surfcoat.2009.10.052 ↗
22. Influence of composite powders' microstructure on the microstructure and properties of Al2O3–TiO2 coatings fabricated by plasma spraying10.1016/j.matdes.2014.09.078 ↗
23. Microstructural evolution during high-temperature oxidation of Ti2AlC ceramics10.1016/j.actamat.2011.03.035 ↗
24. Substitution behavior of Si atoms in the Ti2AlC ceramics10.1016/j.actamat.2017.11.002 ↗
25. TEM study of the initial oxide scales of Ti2AlC10.1016/j.actamat.2011.04.058 ↗
26. Interfacial microstructure of Ti3AlC2 and Al2O3 oxide scale10.1016/j.scriptamat.2006.01.030 ↗
27. TEM study of the early stages of Ti2AlC oxidation at 900°C10.1016/j.scriptamat.2012.07.045 ↗
28. Structure stability of Ti3AlC2 in Cu and microstructure evolution of Cu–Ti3AlC2 composites10.1016/j.actamat.2007.03.033 ↗
29. EBSD image quality mapping10.1017/S1431927606060090 ↗
30. A prominent driving force for the spallation of thermal barrier coatings: chemistry dependent phase transformation of the bond coat10.1016/j.actamat.2017.06.037 ↗
31. Thermal stability of Ti3AlC2/Al2O3 composites in high vacuum10.1016/j.matchemphys.2007.02.091 ↗
32. Microstructural characterization and compression properties of TiC0.61/Cu(Al) composite synthesized from Cu and Ti3AlC2 powders10.1016/j.jallcom.2014.02.159 ↗
33. Sintering and properties of mechanical alloyed Ti3AlC2-Cu composites10.1016/j.msea.2017.01.003 ↗
34. Probing the oxidation behavior of Ti2AlC MAX phase powders between 200 and 1000°C10.1016/j.jeurceramsoc.2016.08.004 ↗
35. Evolution of cracks within an Al2O3–40 wt%TiO2/NiCoCrAl gradient coating10.1016/j.ceramint.2018.08.081 ↗
36. Determination of interface toughness of functionally graded tungsten/EUROFER multilayer at 550 °C by analytical and experimental methods10.1016/j.engfracmech.2018.09.016 ↗
37. Reddy · 2003
38. A methodology, based on sintering-induced stiffening, for prediction of the spallation lifetime of plasma-sprayed coatings10.1016/j.actamat.2012.09.079 ↗
39. Prolong the durability of La2Zr2O7/YSZ TBCs by decreasing the cracking driving force in ceramic coatings10.1016/j.jeurceramsoc.2018.08.033 ↗