journal article·2014-01

Microstructure and strength of needle coke modified ceramic casting molds

Fei Wang, Fei Li, Bo He, Baode Sun

Ceramics International· Volume 40· Issue 1
Publisher page

Abstract

Abstract Properties of an investment casting mold using needle coke additions have been investigated in this work. The use of needle coke increases the mold thickness by a factor of 30% on flat section and 60% at sharp edges over that of a comparable full fused silica system. The extra mold thickness in the needle coke modified system, especially at edges, gives a higher load bear capacity. Ceramic molds modified with needle coke exhibit higher “green, dry” strength, and show less reduction in “green, wet” strength. The extra volume of cavity left after needle coke combustion is not acting as a significant defect which would reduce the hot strength of the mold.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Pigment Synthesis and Properties · Recycling and utilization of industrial and municipal waste in materials production · Injection Molding Process and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Role of silica binders in investment casting
2. Advances in shell molding for investment casting10.1016/S0924-0136(02)00907-X ↗
3. Properties of ceramic casting molds produced with two different binders10.1016/j.ceramint.2004.10.004 ↗
4. Jones · 1993
5. Kline · 2010
6. D. Kline, S. Lekakh, C. Mahimkar, V. Richards, Crack formation in ceramic shell during foam pattern firing, in: Proceedings of the Technical and Operating Conference, Chicago, Illinois, USA, 2009.
7. Corner strength of investment casting shells10.1007/BF03355541 ↗
8. J. Vandermeer, Aunique silica binder for investment shell systems, in: Proceedings of 10th World Conference on Investment Casting, Monte Carlo, 2000, Paper 3.
9. S. Jones, S. Leyland, The use of conductivity as a means of assessing the extent of wet back in an investment casting mold, in: Proceedings of 22nd BICTA Conference on Investment Casting, Bath, 1995, Paper 4.
10. T. Branscomb, The importance of green MOR for autoclave cracking, in: Proceedings of 50th Investment casting Institute (ICI) Technical Meeting, Chicago, 2002, Paper 21.
11. Investigation of fiber modified ceramic molds for investment casting, J10.1016/S0955-2219(02)00153-X ↗
12. The influence of autoclave steam on polymer and organic fiber modified ceramic shells10.1016/j.jeurceramsoc.2004.04.011 ↗
13. R.S. Doles, D.S. Viers, Filler component for investment casting slurries, US Patent no. 7588633 B2, 2009.
14. An EVS (electrochemical voltage spectroscopy) study for the comparison of graphitization behaviors of two petroleum needle cokes10.1016/S0008-6223(99)00262-6 ↗
15. Electrochemical characteristics of needle coke refined by molten caustic leaching as an anode material for a lithium-ion battery10.1016/j.jpowsour.2005.03.139 ↗
16. M.J. Hendricks, M.J.P. Wang, Ceramic shell green strength—how is it measured and what does it mean, in: Proceedings of 10th World Conference on Investment Casting, Monte Carlo, 2000, Paper 5.
17. J. Vandermeer, A unique silica binder for investment shell systems, in: Proceedings of 10th World Conference on Investment Casting, Monte Carlo, Monaco, 2000, Paper 3.
18. Developments in investment casting process-A review10.1016/j.jmatprotec.2012.06.003 ↗
19. S.P. Leyland, R. Hyde, P.A. Withey, The fitness for purpose of investment casting shells, in: Proceedings of 8th International Symposium on Investment Casting (Precast 95), Czech Republic, Brno,1995, pp. 62–68.
20. R. Hyde, S.P. Leyland, P.A. Withey, S. Jones, Evaluation of the mechanical properties of investment casting shells, in: Proceedings of the 22nd BICTA Conference, Bath, September 1995, Paper 7.
21. T. Branscomb, The importance of green MOR for autoclave cracking, in: Proceedings of 50th Investment casting Institute (ICI) Technical Meeting, Chicago, 2002, Paper 21.