Anti-oxidation performance of carbon aerogel composites with SiCO ceramic inner coating
Source abstract
Abstract
Abstract To improve the oxidative-resistant ability of carbon fibre-reinforced carbon aerogel composites (C/CAs), C/CAs were impregnated with a silicon oxycarbide (SiCO) precursor sol several times. After gelating, aging, solvent exchanging, ambient drying, and pyrolyzing, the SiCO precursor sol infiltrated the nanoporous C/CA, and anti-oxidation carbon aerogel composites with a SiCO ceramic inner coating (C/CA-SiCO) were prepared. It was found that the density of the material increases with the number of times that impregnation and pyrolysis were carried out. The mechanical properties and the anti-oxidant performance were significantly improved after the deposition with different numbers of the SiCO coating cycles. The bending strength increased from 2.2 MPa to 10.8–32.3 MPa and the compressive strength (10%e) increased from 0.4 MPa to 3.6–44.4 MPa. The weight loss for the as-prepared composites after heating at 1600 °C for 60 min in air was only 7.6%, and the in-plane shrinkage was less than 2%. Additionally, after the oxidation resistance test, the surface of the C/CA-SiCO had abundant β-SiO2 crystalline, whereas its inner region of the composite remained amorphous.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aerogels and thermal insulation · Advanced ceramic materials synthesis · Silicone and Siloxane Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Ultralow density carbon aerogels with low thermal conductivity up to 2000 °C10.1016/j.matlet.2011.07.114 ↗
2. The preparation of carbon aerogels based upon the gelation of resorcinol-furfural in isopropanol with organic base catalyst10.1016/j.jnoncrysol.2003.12.051 ↗
3. Thermal conductivity of carbon aerogels as a function of pyrolysis temperature10.1007/s10765-006-0086-6 ↗
4. A machinable carbon aerogel composite with a low thermal conductivity and enhanced mechanical properties
5. Shrinkage and pore structure in preparation of carbon aerogels10.1007/s10971-011-2514-8 ↗
6. Determination of the anisotropic thermal conductivity of a carbon aerogel-fiber composite by a non-contact thermographic technique10.1007/s10765-006-0145-z ↗
7. Carbon fiber reinforced carbon aerogel composites for thermal insulation prepared by soft reinforcement10.1016/j.matlet.2011.09.076 ↗
8. Pores in carbon materials-importance of their control10.1016/S1872-5805(08)60048-7 ↗
9. Carbon aerogel-based high-temperature thermal insulation10.1007/s10765-009-0595-1 ↗
10. A MoSi2-SiOC-Si3N4/SiC anti-oxidation coating for C/C composites prepared at relatively low temperature10.1016/j.ceramint.2016.11.151 ↗
11. Microstructure and ablation behavior of double anti-oxidation protection for carbon-bonded carbon fiber composites10.1016/j.ceramint.2016.10.009 ↗
12. A phosphate-based antioxidation coating for carbon/carbon composites10.1016/S1872-5805(07)60004-3 ↗
13. The anti-oxidation coatings of carbon/carbon composites
14. A MoSi2-SiC-Si oxidation protective coating for carbon/carbon composites10.1016/j.surfcoat.2007.03.013 ↗
15. SiC-MoSi2/ZrO2-MoSi2 coating to protect C/C composites against oxidation10.1016/S1003-6326(13)62704-1 ↗
16. Preparation and ablation propertiesof Hf(Ta)C Co-deposition coating for carbon/carbon composites10.1016/j.corsci.2012.09.016 ↗
17. TaB2-SiC-Si multiphase oxidation protective coating for SiC-coated carbon/carbon composites10.1016/j.jeurceramsoc.2013.06.028 ↗
18. Multi-layer CVD-SIC/MoSi2-CrSi2-Si/B-modified SiC oxidation protective coating for carbon/carbon composites10.1016/j.vacuum.2013.03.012 ↗
19. High-temperature behavior of Cf/SiOC composites in inert atmosphere10.1016/j.msea.2011.09.084 ↗
20. Processing of polysiloxane-derived porous ceramics: a review
21. Silicon carbonitride ceramics derived from polysilazane Part II. Investigation of electrical properties10.1016/S0955-2219(00)00009-1 ↗
22. Amorphous Si(Al)OC ceramic from polysiloxanes: bulk ceramic processing, crystallization behavior and applications10.1016/j.jeurceramsoc.2003.10.016 ↗
23. Amorphous silicoboron carbonitride ceramic with anomalously high resistance to creep10.1111/j.1151-2916.1998.tb02780.x ↗
24. A silicoboron carbonitride ceramic stable to 2000°C10.1038/382796a0 ↗
25. Microstructural and dielectric characterization of sol-gel derived silicon oxycarbide glass sheets10.1023/A:1008740218534 ↗
26. Formation of carbon fiber-reinforced ceramic matrix composites with polysiloxane/silicon derived matrix10.1016/j.msea.2006.08.102 ↗
27. Evaluation of oxidation resistance of thin continuous silicon oxycarbide fiber derived from silicone resin with low carbon content10.1007/s10853-010-4629-7 ↗
28. Oxidation resistance improvement of carbon aerogel composites by pyrolyzed sioc ceramic inner coating
29. Synthesis and characterization of novel phenolic resin/silicone hybrid aerogel composites with enhanced thermal, mechanical and ablative properties10.1016/j.compositesa.2017.07.012 ↗
30. Advanced silicon oxycarbide-carbon composites for high temperature resistant friction systems10.1016/j.jeurceramsoc.2016.03.012 ↗
31. Carbon fiber/ceramic matrix composites: processing, oxidation and mechanical properties10.1007/s10853-006-0688-1 ↗
32. Synthesis and characterization of carbon-enriched silicon oxycarbides10.1016/j.jeurceramsoc.2004.07.019 ↗
33. Mechanical property and microstructure evolutions of Cf/SiOC composites with increasing annealing temperature in reduced pressure environment10.1016/j.ceramint.2011.07.049 ↗