Microstructure and current–voltage characteristics of ZnO–V2O5–MnO2 varistor system

H.H. Hng, P.L. Chan

Ceramics International· Volume 30· Issue 7
Publisher page

Abstract

Abstract The effects of sintering temperature and time on the microstructure and the electrical properties have been studied in a ZnO–0.5 mol%V2O5–2 mol%MnO2 system. The microstructure of the samples consists mainly of ZnO grains with Zn3(VO4)2 as the minority secondary phase. This minor secondary phase disappears for samples sintered at 1200 °C and above. An increase in sintering temperature also brings about a deleterious effect on the non-linear coefficient and the breakdown electric field. An optimum sintering time of 4 h at 900 °C gives the best electrical properties, with the non-linear coefficient α attaining a highest value of 31.8. Grain growth process is also investigated in terms of the phenomenological kinetic grain growth expression: G n =K o t exp (− Q RT ) . The kinetic grain growth exponent n is observed to be 4, while the apparent activation energy Q is 193±19 kJ / mol .
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: ZnO doping and properties · Gas Sensing Nanomaterials and Sensors · Transition Metal Oxide Nanomaterials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Microstructural engineering through donor and acceptor doping in the grain and grain boundary of a polycrystalline semiconducting ceramic10.1557/JMR.1992.3280 ↗
2. Non-ohmic properties of zinc oxide ceramics10.1143/JJAP.10.736 ↗
3. Sintering and varistor characteristics of ZnO–Bi2O3 ceramics10.1063/1.328266 ↗
4. Non-ohmic properties of ZnO–rare earth metal oxide–Co3O4 ceramics10.1143/JJAP.16.1361 ↗
5. The effect of liquid-phase sintering on the properties of Pr6O11-based ZnO varistors10.1063/1.349812 ↗
6. Non-ohmic characteristics of ZnO–V2O5 ceramics10.1063/1.357254 ↗
7. Microstructure and non-ohmic properties of ZnO–V2O5 ceramics10.1143/JJAP.34.6452 ↗
8. Microstructure and non-ohmic properties of binary ZnO–V2O5 ceramics sintered at 900°C10.1016/0167-577X(95)00217-0 ↗
9. Microstructure and electrical properties of V2O5-based multicomponent ZnO varistors prepared by microwave sintering process10.1143/JJAP.36.1169 ↗
10. Microstructure and non-linear properties of microwave-sintered ZnO–V2O5 varistors: I. Effect of V2O5 doping10.1111/j.1151-2916.1998.tb02717.x ↗
11. Microstructure and non-linear properties of microwave-sintered ZnO–V2O5 varistors: II. Effect of Mn3O4 doping10.1111/j.1151-2916.1998.tb02718.x ↗
12. Characterisation of Zn3(VO4)2 phases in V2O5-doped ZnO varistors10.1016/S0955-2219(98)00303-3 ↗
13. Microstructure and current–voltage characteristics of multi-component vanadium-doped zinc oxide varistors10.1111/j.1151-2916.2000.tb01576.x ↗
14. Zinc vanadates in vanadium oxide-doped zinc oxide varistors10.1111/j.1151-2916.2001.tb00673.x ↗
15. Effects of MnO2 doping in V2O5-doped ZnO varistor system10.1016/S0254-0584(02)00031-7 ↗
16. Average grain size in polycrystalline ceramics10.1111/j.1151-2916.1969.tb11975.x ↗
17. Reactions between ZnO and selected oxides of elements of Groups IV and V
18. Grain growth in sintered ZnO and ZnO–Bi2O3 ceramics10.1111/j.1151-2916.1990.tb05099.x ↗
19. Grain growth of ZnO in binary ZnO–V2O5 ceramics10.1023/A:1023988631228 ↗
20. Grain growth of ZnO during Bi2O3 liquid-phase sintering10.1111/j.1151-2916.1992.tb05607.x ↗
21. Zinc oxide varistor—a review