journal article·2014-06

Microstructure and mechanical properties of Si3N4/42CrMo joints brazed with TiNp modified active filler

Tianpeng Wang, Jie Zhang, Chunfeng Liu, Guochao Wang

Ceramics International· Volume 40· Issue 5
Publisher page

Abstract

Abstract Si 3 N 4 ceramic/42CrMo steel joints were obtained by employing TiNp modified Ag–Cu–Ti active filler and subsequently the effect of TiNp content on the microstructure and mechanical properties of the joints was investigated. Microstructural examination revealed that TiN+Ti 5 Si 3 reaction layer was adjacent to the Si 3 N 4 ceramic while a TiC reaction layer was close to the steel substrate. With the increase of TiNp content, more fine grains and less Ag–Cu eutectic appeared in the joint and the reaction layers near the two base materials became thinner. The flexural strength of the joint obtained by four-point bending test climbed about 100% with the optimum TiNp content of 5 vol%, comparing with the case without TiNp. Thermal stress distributions in the joint were analyzed using finite element modeling computations, which accorded well with the bending test results.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Joining of engineering ceramics10.1179/174328009X461078 ↗
2. Interface microstructure of alumina mechanically metallized with Ti brazed to Fe–Ni–Co using different fillers10.1016/j.msea.2007.02.033 ↗
3. Formation of interfacial microstructure in brazing of Si3N4 with Ti-activated Ag–Cu filler alloys10.1016/0956-716X(95)00127-H ↗
4. Interfacial characterization of silicon nitride/silicon nitride joints brazed using Cu-base active metal interlayers10.1016/j.ceramint.2011.11.050 ↗
5. Improving the strength of brazed joints to alumina by adding carbon fibres10.1023/A:1018666827969 ↗
6. Microstructure and mechanical properties of Si3N4/Si3N4 joint brazed with Ag–Cu–Ti+SiCp composite filler10.1016/j.msea.2010.01.065 ↗
7. Relief of the residual stresses in ceramic-metal joints by a layered braze structure10.1002/adem.200500233 ↗
8. Microstructure evolution of Si3N4/Si3N4 joint brazed with Ag–Cu–Ti+SiCp composite filler10.1016/j.ceramint.2010.02.010 ↗
9. Effect of brazing temperature on microstructure and mechanical properties of Si3N4/Si3N4 joints brazed with Ag–Cu–Ti+Mo composite filler10.1007/s10853-010-5154-4 ↗
10. Brazing of silicon nitride ceramic composite to steel using SiC-particle-reinforced active brazing alloy10.1016/j.ceramint.2006.03.010 ↗
11. An analysis of deformation mechanism in the Si3N4–AgCuTi+SiCp–Si3N4 joints by digital image correlation10.1016/j.jeurceramsoc.2012.07.038 ↗
12. Microstructure and mechanical properties of the Si3N4/42CrMo steel joints brazed with Ag–Cu–Ti+Mo composite filler10.1016/j.jeurceramsoc.2010.07.005 ↗
13. Nanostructure of wetting triple line in a Ag–Cu–Ti/Si3N4 reactive system10.1016/S1359-6454(98)00375-9 ↗
14. Lattice parameters and thermal expansion of Ti(CxN1−x), Zr(CxN1−x), Hf(CxN1−x) and TiN1−x from 298K to 1473K as investigated by high-temperature X-ray diffraction10.1016/0925-8388(94)90828-1 ↗
15. Studies of residual stresses in planar solid oxide fuel cells10.1016/j.jpowsour.2008.04.035 ↗
16. Microstructural and mechanical characterization of the Si3N4/Si3N4 joint brazed using Au–Ni–V filler alloys10.1016/j.jeurceramsoc.2009.08.015 ↗
17. Effect of Si3N4-particles addition in Ag–Cu–Ti filler alloy on Si3N4/TiAl brazed joint10.1016/j.msea.2011.03.032 ↗
18. Al2O3/Al2O3 joint brazed with Al2O3-particulate-contained composite Ag–Cu–Ti filler material
19. Thermodynamic assessment of the Cu–Ti–Zr system I. Cu–Ti system10.1007/s11106-008-9026-2 ↗
20. Influence of TiX (X=B(2) or N) addition on the interfacial microstructure features of CBN grains and AgCuTi composite filler10.1007/s11595-010-0047-6 ↗
21. Brazing mechanism and infiltration strengthening of CC composites to TiAl alloys joint10.1016/j.scriptamat.2010.06.035 ↗
22. Strain energy distribution in ceramic-to-metal joints10.1016/S1359-6454(01)00352-4 ↗
23. Characterisation of TiN thin films using the bulge test and the nanoindentation technique10.1016/S0040-6090(97)00566-X ↗
24. Enhanced Young's modulus of Al–Si alloys and reinforced matrices by Co-continuous structures10.1177/0021998309347649 ↗
25. Thermal expansion coefficients of composite materials based on energy principles10.1177/002199836800200308 ↗
26. An analytical study on strengthening of particulate reinforced metal matrix composites10.1016/1359-6454(95)00150-9 ↗
27. Thermal expansion of the Ti5Si3 and Ti6Si2B phases investigated by high-temperature X-ray diffraction10.1016/j.intermet.2005.05.007 ↗