Abstract
Abstract A 90TiC–10ZrC (mol%) solid solution was consolidated by spark plasma sintering at 2373 K and decomposed into Zr0.94Ti0.06C nodules and Ti0.97Zr0.03C matrix by heat treatment at 1573 K. The Zr0.94Ti0.06C nodules were precipitated in the Ti0.97Zr0.03C matrix with Ti0.97Zr0.03C {100} // Zr0.94Ti0.06C {100}. The Vickers hardness and fracture toughness increased with increasing heat treatment time up to 36 ks and exhibited the maximum values of 25.9 GPa and 3.3 MPa m1/2, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Ultra High Temperature Ceramic Composite
2. Densification and mechanical properties of TiC by SPS-effects of holding time, sintering temperature and pressure condition10.1016/j.jeurceramsoc.2012.04.017 ↗
3. Effects of ZrC on microstructure, mechanical properties and thermal shock resistance of TiC−ZrC−Co−Ni cermets10.1016/j.msea.2012.11.003 ↗
4. Microstructure and fracture toughness of TiC−ZrC−WC−Mo−Ni cermets10.1016/j.ijrmhm.2007.08.008 ↗
5. Synthesis of titanium carbide and TiC–SiO2 nanocomposite powder using rutile and Si by mechanically activated sintering10.1016/j.apt.2014.02.008 ↗
6. Preparation of Al2O3–TiC nanocomposite by mechano-chemical reduction of TiO2 with aluminum and graphite10.1016/j.jallcom.2009.02.122 ↗
7. Fabrication and characterization of Al–Al2O3–ZrC composite produced by accumulative roll bonding (ARB) process10.1016/j.jallcom.2014.08.136 ↗
8. The effect of Ti substitution by Zr on the microstructure and mechanical properties of the cermet Ti1−xZrxC sintered by SPS10.1016/j.ijrmhm.2011.10.002 ↗
9. Mechanical properties of nanocrystalline TiC–ZrC solid solutions fabricated by spark plasma sintering10.1016/j.ceramint.2014.03.024 ↗
10. Consolidation of titanium carbide with zirconium carbide by spark plasma sintering10.4028/www.scientific.net/KEM.616.52 ↗
11. Spark plasma sintering of TiC−ZrC composites10.1016/j.ceramint.2015.02.019 ↗
12. First-principles study of elastic and stability properties of ZrC–ZrN and ZrC–TiC alloys
13. Calculation of phase diagrams of pseudobinary systems based on high-melting carbides of titanium, zirconium, hafnium, and vanadium
14. First-principles phase diagram calculations for the HfC−TiC, ZrC−TiC, and HfC−ZrC solid solutions10.1103/PhysRevB.80.134112 ↗
15. Structure and properties of precipitation-hardening ceramic Ti−Zr−C and Ti−Ta−C materials10.1134/S0031918X10010102 ↗
16. On spinodal decomposition in magnetron-sputtered (Ti, Zr) nitride and carbide thin films10.1016/0040-6090(89)90868-7 ↗
17. Synthesis and phase separation of (Ti, Zr)C10.1016/j.actamat.2013.11.074 ↗
18. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
19. Material selection for hard coatings10.1116/1.573700 ↗
20. Shackelford · 2000
21. Fracture toughness improvement of TiC by Nb and Mo precipitates10.1023/A:1006735624221 ↗
22. Nanocrystalline hydroxyapatite with simultaneous enhancements in hardness and toughness10.1016/j.biomaterials.2009.08.048 ↗
23. Processing and properties of nanophase non-oxide ceramics10.1016/S0921-5093(00)01389-7 ↗