Comparative study of Ti-C-Ni-Al, Ti-C-Ni-Fe, and Ti-C-Ni-Al/Ti-C-Ni-Fe coatings produced by magnetron sputtering, electro-spark deposition, and a combined two-step process
Source abstract
Abstract
Abstract Comparative study of Ti-C-Ni-Fe, Ti-C-Ni-Al, and Ti-C-Ni-Al/Ti-C-Ni-Fe coatings obtained by electro-spark deposition (ESD) using TiCNi electrode, magnetron sputtering (MS) of TiCNiAl target, and a combination of these methods (MS-ESD) was carried out. The coating microstructures and elemental compositions were studied by means of X-ray diffraction, scanning electron microscopy, energy-dispersive spectroscopy, and glow discharge optical emission spectroscopy. The materials were tested in terms of their hardness, elastic modulus, elastic recovery, crack resistance, friction coefficient, and wear resistance under sliding, impact and abrasive conditions, as well as corrosion- and oxidation resistance. The work demonstrated that the utilization of a combined two-step MS-ESD technology permits to obtain bilayers made of Ti-C-Ni-Al/Ti-C-Ni-Fe coatings with improved crack-, wear- and oxidation resistance compared with their single-layered Ti-C-Ni-Al counterparts deposited by MS, and with reduced friction coefficient and enhanced corrosion resistance compared with ESD Ti-C-Ni-Fe coatings.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Surface Treatment and Coatings · Metal and Thin Film Mechanics · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Fretting causes failure of a WC-Co-coated slide bearing10.1016/0043-1648(65)90249-8 ↗
2. Complex carbide powders for plasma spraying10.1016/0040-6090(77)90262-0 ↗
3. Improving wear-resistance of high speed steel tools by carbide coating10.1016/0041-2678(74)90033-5 ↗
4. Deposition and characterization of WC-Co hard-metal coatings by high velocity oxy-fuel process combined with dry-ice blasting10.1016/j.ijrmhm.2016.12.007 ↗
5. Lovelock, powder/processing/structure relationships in WC-Co thermal spray coatings: a review of the published literature10.1361/105996398770350846 ↗
6. Microstructure and mechanical properties of TiC-Ni coating on AISI304 steel produced by TIG cladding process10.1016/j.jmatprotec.2016.09.018 ↗
7. Two-body abrasive wear of nano- and microcrystalline TiC–Ni-based thermal spray coatings10.1016/j.surfcoat.2005.05.007 ↗
8. Effect of Ni contents on the microstructure and mechanical properties of TiC–Ni cermets obtained by direct laser fabrication10.1016/j.ijrmhm.2008.07.006 ↗
9. Effect of additions of TiC and Re on high temperature corrosion performance of cold sprayed Ni–20Cr coatings10.1016/j.surfcoat.2015.08.002 ↗
10. Ti–Ni–C nanocomposite coatings evaluated in a sliding electrical contact application10.1016/j.surfcoat.2015.06.016 ↗
11. Friction and contact resistance of nanocomposite Ti–Ni–C coatings10.1016/j.wear.2010.12.006 ↗
12. Thermal stability of Ti-C-Ni-Cr and Ti-C-Ni-Cr-Al-Si nanocomposite coatings10.1088/1742-6596/652/1/012057 ↗
13. The prospects of nanodispersive powders application in surface engineering technologies10.1016/j.surfcoat.2003.10.086 ↗
14. R.N. Johnson, ElectroSpark deposition: principles and applications, in: Proceedings of the 45th Annual Technical Conference Proceedings. Society of Vacuum Coaters, 2002, pp. 87 – 92.
15. Adhesion behavior of WC coating deposited on titanium alloy by electrospark deposition10.4028/www.scientific.net/SSP.127.325 ↗
16. Advances in the electrospark deposition coating process10.1116/1.573672 ↗
17. Surface modification by electrical discharge machining: a review10.1016/j.jmatprotec.2008.09.032 ↗
18. A. Goto, M. Akiyoshi, H. Ochiai, M. Watanabe, Development of micro spark coating, in: Proceedings of the 24th Congress of International Council of the Aeronautical Sciences, 29 August-3, September, Yokohama, Japan, Paper ICAS 2004-5.5.2, 2004.
19. Erosion testing of coatings for V-22 aircraft applications
20. Mechanical and tribological properties of the TiC–TiB2 composite coating deposited on 40Cr-steel by electro spark deposition10.1016/j.apsusc.2015.12.198 ↗
21. Improving oxidation resistance of Ti3Al and TiAl intermetallic compounds with electro-spark deposit coatings10.1016/S0921-5093(02)00595-6 ↗
22. Protection of a Ti3Al–Nb alloy by electro-spark deposition coating10.1016/S1359-6462(01)01146-0 ↗
23. Investigation and characterization of electrospark deposited chromium carbide-based coating on the steel10.1016/j.surfcoat.2015.04.033 ↗
24. Corrosion behavior of TiZrNiCuBe metallic glass coatings synthesized by electrospark deposition10.1016/j.corsci.2014.03.017 ↗
25. Surface modification of resistance welding electrode by electro-spark deposited composite coatings: part I. Coating characterization10.1016/j.surfcoat.2006.02.015 ↗
26. Surface hardening of metallic alloys by electrospark deposition followed by plasma nitriding10.1016/j.jmatprotec.2006.03.162 ↗
27. Laser treatment of electro-spark coatings deposited in the carbon steel substrate with using nanostructured WC-Cu electrodes10.1016/j.phpro.2012.10.041 ↗
28. Large area smoothing of surfaces by ion bombardment: fundamentals and applications
29. Effect of deposition parameters on properties of TiO2 films deposited by reactive magnetron sputtering10.1016/j.ceramint.2017.05.139 ↗
30. Magnetron sputtering preparation and properties of SiC/MoSi2 oxidation protective coating for carbon/carbon composites prepared10.1016/S1875-5372(17)30031-0 ↗
31. Mechanical properties of decellularized extracellular matrix coated with TiCaPCON film10.1088/1748-605X/aa6fc0 ↗
32. Modification of polytetrafluoroethylene implants by depositing TiCaPCON films with and without stem cells10.1016/j.surfcoat.2011.08.029 ↗
33. The use of PVD coating on natural textile fibers10.1016/j.proeng.2016.01.220 ↗
34. Morphology and mechanical properties of TiN coatings prepared with different PVD methods10.1016/S1875-5372(17)30057-7 ↗
35. Enhanced wear resistance of the Cr-based thin film coating on micro drill by doping with W–C–N10.1016/j.tsf.2009.03.052 ↗
36. The influence of Si concentrations on the oxidation resistance of Mo–Si–B–(N) coatings10.3103/S106782121406011X ↗
37. Effects of magnetic field strength and deposition pressure on the properties of TiN films produced by high power pulsed magnetron sputtering (HPPMS)10.1016/j.surfcoat.2017.02.051 ↗
38. Hard Cr–Al–Si–B–(N) coatings deposited by reactive and non-reactive magnetron sputtering of CrAlSiB target10.1016/j.apsusc.2014.06.160 ↗
39. TiC-Ni-based composite materials dispersion-strengthened by nanoparticles for electrospark deposition10.3103/S1067821208050167 ↗
40. Analysis of elemental composition by high-frequency glow dicharge optial emission spectroscopy10.1134/S207020511205005X ↗
41. On the generality of the relationship among contact stiffness, contact area, and elastic modulus during indentation10.1557/JMR.1992.0613 ↗
42. Influence of oxygen flow rate on the structural and mechanical properties of reactively magnetron sputter-deposited Zr–B–O coatings10.1016/S0040-6090(98)01732-5 ↗
43. Influence of Zr and O on the structure and properties of TiC(N) coatings deposited by magnetron sputtering of composite TiC0.5 + ZrO2 and (Ti, Zr)C0.5 + ZrO2 targets10.1016/j.surfcoat.2011.10.057 ↗
44. Stresses in coatings obtained by electro-spark alloying and laser processing (review)10.1007/BF02355555 ↗
45. Hague · 1964 · 1
46. Comparative investigation of TiAlC(N), TiCrAlC(N), and CrAlC(N) coatings deposited by sputtering of МАХ-phase Ti2 − хCrхAlC targets10.1016/j.surfcoat.2009.05.036 ↗
47. Effect of Al addition on structure and properties of sputtered TiC films10.1002/ppap.200730102 ↗
48. Investigation of the influence of Ni doping on the structure and hardness of Ti-Ni-C coatings10.1155/2017/6368927 ↗
49. Comparative study of sliding, scratching, and impact-loading behavior of hard CrB2 and Cr–B–N films10.1007/s11249-016-0729-0 ↗
50. Influences of bias voltage on mechanical and tribological properties of Ti–Al–C films synthesized by magnetron sputtering10.1016/j.surfcoat.2008.12.003 ↗