journal article·2021-11

Selective laser melting of SiCp/Al composites: Densification, microstructure, and mechanical and tribological properties

Houbo Xie, Jialian Zhang, Faliang Li, Gaoqian Yuan, Qing Zhu, Quanli Jia, Haijun Zhang, Shaowei Zhang

Ceramics International· Volume 47· Issue 21
Publisher page

Abstract

Abstract In this paper, SiCp/Al composites were successfully fabricated by selective laser melting (SLM), and the dependence of phase composition, densification behavior, and mechanical properties of the composites on laser power was researched and discussed. The results showed that the density, microhardness and friction resistance of the SLM formed SiCp/Al composites were enhanced with increasing the laser power density, which may be caused by the higher molten pool temperature at higher laser power density. When SiCp/Al composites were prepared at 400 W with a scanning speed of 300 mm/s, the highest relative density of approximately 91.1 % and microhardness of approximately 191 HV0.1 (more than six times higher than that of the selective laser melted pure Al specimens, 191 HV0.1 vs 31 HV0.1) were obtained, and the minimum wear rate and friction coefficient were 1.31 × ×10−5 mm3 N−1 m−1 and 0.38, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. PZT ceramics fabricated based on stereolithography for an ultrasound transducer array application10.1016/j.ceramint.2018.09.055 ↗
2. 3D printing of BaTiO3 piezoelectric ceramics for a focused ultrasonic array
3. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders:processing, microstructure, and properties10.1016/j.pmatsci.2015.03.002 ↗
4. Mechanical properties of AlSi10Mg produced by selective laser melting10.1016/j.phpro.2012.10.059 ↗
5. New developments of laser processing Aluminium Alloys via additive manufacturing technique10.1016/j.phpro.2011.03.050 ↗
6. Laser additive manufacturing of metallic components: materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
7. Thermal behavior and densification mechanism during selective laser melting of copper matrix composites: simulation and experiments10.1016/j.matdes.2013.10.006 ↗
8. Fabrication of porous Ti-6Al-4V with designed structure by rapid prototyping technology10.4028/www.scientific.net/KEM.330-332.1293 ↗
9. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
10. On the precipitation hardening of selective laser melted AlSi10Mg10.1007/s11661-015-2980-7 ↗
11. Microstructural and mechanical approaches of the selective laser melting process applied to a nickel-base superalloy10.1016/j.msea.2011.11.092 ↗
12. Novel selective laser melting processed in-situ TiC particle-reinforced Ni matrix composite with excellent processability and mechanical properties10.1016/j.msea.2020.140145 ↗
13. Multi-material selective laser melting of Fe/Al-12Si components10.1016/j.mfglet.2017.01.002 ↗
14. Simultaneously enhanced strength and ductility for 3D-printed stainless steel 316L by selective laser melting10.1038/s41427-018-0018-5 ↗
15. Microstructure and properties of intermetallic composite coatings fabricated by selective laser melting of Ti-SiC powder mixtures10.1016/j.intermet.2013.11.012 ↗
16. Ductility of a Ti-6Al-4V alloy produced by selective laser melting of prealloyed powders10.1108/13552541011083371 ↗
17. Effect of SiC particle size on the physical and mechanical properties of extruded Al matrix nanocomposites10.1016/j.matdes.2013.08.049 ↗
18. Interface formation and bonding control in high-volume-fraction (TiC+TiB2)/Al composites and their roles in enhancing properties10.1016/j.compositesb.2021.108605 ↗
19. Selective laser melting of in-situ titanium-titanium boride composites: processing, microstructure and mechanical properties10.1016/j.actamat.2014.05.022 ↗
20. Evaluation of microstructure and mechanical properties of Al-TiC metal matrix composite prepared by conventional, microwave and spark plasma sintering methods
21. Synthesis and characterisation of advanced ball-milled Al-Al2O3 nanocomposites for selective laser melting10.1016/j.powtec.2016.04.015 ↗
22. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
23. Modification of microstructure and superficial properties of A356 and A356/10% SiCp by selective laser surface melting (SLSM)10.1016/j.surfcoat.2016.10.046 ↗
24. Laser processing of SiC-particle-reinforced coating on titanium10.1016/j.scriptamat.2010.04.044 ↗
25. Overview of wear performance of aluminium matrix composites reinforced with ceramic materials under the influence of controllable variables10.1016/j.ceramint.2015.08.150 ↗
26. Dynamic softening mechanism of 2 vol.% nano-sized SiC particle reinforced Al-12Si matrix composites during hot deformation
27. Fabrication, microstructure and properties of the mid-fraction SiC particles/6061Al composites using an optimized powder metallurgy technique10.3103/S1067821219030076 ↗
28. High strength and good ductility at elevated temperature of nano-SiCp/Al2014 composites fabricated by semi-solid stir casting combined with hot extrusion10.1016/j.msea.2014.12.089 ↗
29. Study of the microstructure and ring element segregation zone of spray deposited SiCp/7055Al10.3390/ma12081299 ↗
30. Selective laser melting of in-situ Al4SiC4+SiC hybrid reinforced Al matrix composites: influence of starting SiC particle size10.1016/j.surfcoat.2015.04.029 ↗
31. On the breakdown of SiC during the selective laser melting of aluminum matrix composites10.1002/adem.201600835 ↗
32. Formation of Cu2FeAl7 phase in friction-stir-welded SiCp/Al-Cu-Mg composite10.1016/j.scriptamat.2007.08.020 ↗
33. Abnormal deformation behavior and particle distribution during hot compression of fine-grained 14 vol% SiCp/2014Al composite10.1016/j.jallcom.2018.01.397 ↗
34. Stable and metastable phase equilibria in the chemical interaction between aluminium and silicon carbide10.1007/BF01045395 ↗
35. Formation mechanisms of TiB2 tracks on Ti6Al4V alloy during selective laser melting of ceramic-metal multi-material10.1016/j.powtec.2020.04.027 ↗
36. Stability and response to rolling of the interfaces in cast Al-SiCp and Al-Mg alloy-SiCp composites10.1016/j.msea.2004.03.024 ↗
37. Moisture effect on SiCp/6061 Al MMC: dissolution of interfacial Al4C310.1016/S1359-6462(97)00133-4 ↗
38. Effect of active gas on weld shape and microstructure of advanced A-TIG-welded stainless steel
39. A study of the microstructural evolution during selective laser melting of Ti-6Al-4V10.1016/j.actamat.2010.02.004 ↗
40. Sintering of commercially pure titanium powder with a Nd:YAG laser source10.1016/S1359-6454(02)00567-0 ↗
41. Wetting of ceramics by liquid metals10.1111/j.1151-2916.1971.tb12307.x ↗
42. Wetting of pure aluminium on graphite, SiC and Al2O3 in aluminium filtration10.1016/S1003-6326(11)61410-6 ↗
43. The wettability and the reaction for SiC particle/Al alloy system10.1007/BF01151245 ↗
44. Particulate migration behavior and its mechanism during selective laser melting of TiC reinforced Al matrix nanocomposites10.1016/j.matdes.2015.05.041 ↗
45. Effects of laser sintering processing parameters on the microstructure and densification of iron powder10.1016/S0921-5093(03)00341-1 ↗
46. Grain refinement in a single titanium powder particle impacted at high velocity10.1016/j.scriptamat.2008.06.020 ↗
47. Selective laser melting additive manufacturing of TiC/AlSi10Mg bulk-form nanocomposites with tailored microstructures and properties10.1016/j.phpro.2014.08.153 ↗
48. Nanocrystalline TiC-reinforced H13 steel matrix nanocomposites fabricated by selective laser melting10.1016/j.matdes.2016.02.022 ↗
49. Rapid fabrication of bulk-form TiB2/316L stainless steel nanocomposites with novel reinforcement architecture and improved performance by selective laser melting10.1016/j.jallcom.2016.04.156 ↗
50. Microstructure development, tribological property and underlying mechanism of laser additive manufactured submicro-TiB2 reinforced Al-based composites
51. Selective laser melting of TiB2/316L stainless steel composites: the roles of powder preparation and hot isostatic pressing post-treatment10.1016/j.powtec.2016.12.073 ↗
52. Thermal behavior and densification mechanism during selective laser melting of copper matrix composites: simulation and experiments10.1016/j.matdes.2013.10.006 ↗
53. Particle reinforced aluminium and magnesium matrix composites10.1179/imr.1994.39.1.1 ↗
54. Thermodynamic assessments of the Al2O3-Al4C3-AlN and Al4C3-AlN-SiC systems10.1007/s11669-012-0073-5 ↗
55. Reactions between Ti2AlC, B4C, and Al and phase equilibria at 1000 °C in the Al-Ti-B-C quaternary system10.1007/s11669-015-0371-9 ↗
56. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
57. Density improvement of metal parts directly fabricated via selective laser melting
58. Influence of the second-phase particle size on grain growth based on computer simulation10.1016/S0921-5093(99)00177-X ↗
59. Microstructure evolution and wear properties of in-situ synthesized TiB2 and TiC reinforced steel matrix composites10.1016/j.jallcom.2007.05.018 ↗
60. Sliding wear behaviour of Al 6063/TiB2 in-situ composites at elevated temperatures10.1016/j.matdes.2008.09.037 ↗
61. Mechanisms of sliding wear of metals and alloys at elevated temperatures10.1016/j.triboint.2007.10.003 ↗
62. Dry sliding wear behavior of cast SiC-reinforced Al MMCs10.1016/S0921-5093(03)00408-8 ↗
63. Selective laser melting of TiC reinforced 316L stainless steel matrix nanocomposites: influence of starting TiC particle size and volume content10.1016/j.matdes.2016.05.018 ↗
64. AA2024/SiC metal matrix composites simultaneously improve ductility and cracking resistance during elevated temperature deformation10.1016/j.msea.2020.139697 ↗
65. Ceramic waste SiC particle-reinforced Al matrix composite brake materials with a high friction coefficient
66. Dry sliding wear behavior of SiC and B4C-reinforced AA6351 metal matrix composite produced by stir casting process
67. Effect of SiC addition on the mechanical properties and wear behavior of Al-SiC nanocomposites produced by accumulative roll bonding10.1088/2053-1591/ab9d53 ↗
68. Effect of SiC particle size and weight % on mechanical properties of AA7075 SiC composite[J]
69. Effects of particle size and surface modification of SiC on the wear behavior of high volume fraction Al/SiCp composites10.1016/j.jallcom.2020.154647 ↗
70. Enhanced strengthening of Al-SiC nanocomposites containing a uniform dispersion of dense nanoparticles fabricated by a hybrid accumulative roll-bonding process
71. Influence of reinforcing particle distribution on the casting characteristics of Al-SiCp composites10.1016/j.jmatprotec.2019.116580 ↗
72. Superior mechanical performance of inductively sintered Al/SiC nanocomposites processed by novel milling route10.1038/s41598-020-67198-w ↗
73. Tribological properties of spark plasma sintered Al-SiC composites10.3390/ma13214969 ↗