Abstract

Abstract Fine-grained and dense boron carbide ceramics are sintered by SPS process. The effect of the decrease of the impurities content by a heat-treatment of the starting powder is studied on the mechanical properties at room temperature ( i.e. Vickers hardness and fracture toughness) and at high temperature (up to 1600 °C) by bending tests ( i.e. elastic modulus, flexural strength). These properties are correlated with microstructural characteristics of both materials. It is shown that heat treatment of the powder decreases the contents of free carbon (exhibiting an “onion-like” structure) and of secondary oxide phases (silicon and boron-rich) at grain boundaries. It leads to a slight decrease of the hardness, fracture toughness and bending modulus, and an increase of the flexural strength. In addition, no brittle-to-plastic transition is noticed up to 1600 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Boron and Carbon Nanomaterials Research · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Additive-free superhard B4C with ultrafine-grained dense microstructures10.1016/j.jeurceramsoc.2013.10.006 ↗
2. Opportunities for advanced ceramics and composites in the nuclear sector10.1111/jace.12406 ↗
3. Boron carbide: structure, properties, and stability under stress10.1111/j.1551-2916.2011.04865.x ↗
4. The elastic modulus and fracture of boron carbide10.1111/j.1151-2916.1980.tb09845.x ↗
5. Structural modifications induced by ion irradiation and temperature in boron carbide B4C10.1016/j.nimb.2015.07.082 ↗
6. D. Gosset, 15 – Absorber materials for generation IV reactors A2 – Yvon, Pascal, in: Struct. Mater. Gener. IV Nucl. React., Woodhead Publishing, 2017, pp. 533–567, http://www.sciencedirect.com/science/article/pii/B978008100906200015X (accessed November 18, 2016).10.1016/B978-0-08-100906-2.00015-X ↗
7. Boron carbide—a comprehensive review10.1016/0955-2219(90)90048-K ↗
8. Structure and single-phase regime of boron carbides10.1103/PhysRevB.38.6041 ↗
9. Boron carbides from first principles10.1088/1742-6596/176/1/012002 ↗
10. The effect of stoichiometry on mechanical properties of boron carbide
11. Mechanical properties of hot-pressed B-B4C materials10.1111/j.1151-2916.1979.tb19042.x ↗
12. Microstructure and mechanical properties of B4C based ceramics with Fe3Al as sintering aid by spark plasma sintering10.1016/j.jeurceramsoc.2014.02.014 ↗
13. Microstructure and mechanical properties of B4C densified by spark plasma sintering with Si as a sintering aid10.1016/j.ceramint.2014.09.115 ↗
14. High temperature fracture of boron carbide: experiments and simple theoretical models10.1007/BF02403232 ↗
15. Strength and creep in boron carbide (B4C) and aluminum dodecaboride (α-AlB12)10.1006/jssc.2000.8834 ↗
16. Method for the determination of free graphite in boron carbide10.1016/0022-5088(81)90096-5 ↗
17. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
18. High temperature compressive creep of spark plasma sintered zirconium (oxy-)carbide10.1016/j.msea.2014.06.059 ↗
19. Graphite–hydrogen reactions and their implications in geochemistry10.1038/2121420a0 ↗
20. D. Bernache-Assollant, J.-P. Bonnet, Frittage: Aspects Physico-chimiques, Ed. Techniques Ingénieur, 2005.
21. High-temperature creep deformation of coarse-grained boron carbide ceramics10.1016/j.jeurceramsoc.2014.11.001 ↗
22. The effect of twins on the mechanical behavior of boron carbide10.1007/s11661-010-0548-0 ↗
23. Defects in boron carbide before and after neutron irradiation10.1016/0001-6160(71)90040-X ↗
24. Curling and closure of graphitic networks under electron-beam irradiation10.1038/359707a0 ↗
25. Direct observation of the tetrahedral bonding in graphitized carbon black by high resolution electron microscopy10.1016/0022-0248(80)90013-5 ↗
26. Marcoux · 2002
27. M. Colin, G. Nucléaire, Tech. Ing., 1989, 〈http://www.techniques-ingenieur.fr.ezproxy.unilim.fr/base-documentaire/archives-th12/archives-genie-nucleaire-tiabn/genie-nucleaire-b3720/〉 (accessed 21.07.16).