Abstract
Abstract The high-temperature tribological properties of bare 7075 Al – Zn – Mg – Cu alloy substrate and microarc oxidation (MAO) coating against ZrO2 ceramic ball were evaluated at 25 °C −300 °C. Coefficients of friction were recorded, and wear rates were determined. Surface morphology and wear scars on the ZrO2 ball were observed. Furthermore, wear mechanisms at three different temperatures were discussed. It was found that the MAO coating could maintain a low wear rate and a stable wear performance in an elevated temperature environment. At 300 °C, the wear rate of MAO coating was merely 1/11 of 7075 aluminium alloy substrate. MAO coating suffered mainly adhesive wear at ambient temperature, and both adhesive wear and abrasive wear at elevated temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. 2017 · vol. 1
2. Campbell · 2011
3. Progress in structural materials for aerospace systems10.1016/j.actamat.2003.08.023 ↗
4. Tribological behavior of diamond-like-carbon (DLC) coatings against aluminum alloys at elevated temperatures10.1016/j.surfcoat.2006.06.045 ↗
5. Structure, mechanical and tribological properties of diamond-like carbon films on aluminum alloy by arc ion plating10.1016/j.vacuum.2011.10.019 ↗
6. HVOF thermal sprayed coatings on aluminium alloys and aluminium matrix composites10.1016/j.surfcoat.2005.02.124 ↗
7. Wear of plasma-nitrided aluminum alloys10.1016/j.wear.2005.02.119 ↗
8. Plasma electrolysis for surface engineering10.1016/S0257-8972(99)00441-7 ↗
9. Analysis of phase distribution for ceramic coatings formed by microarc oxidation on aluminum alloy10.1111/j.1151-2916.1998.tb02493.x ↗
10. An elevated temperature infrared emissivity ceramic coating formed on 2024 aluminium alloy by microarc oxidation10.1016/j.ceramint.2012.09.060 ↗
11. Deposition of duplex Al2O3/TiN coatings on aluminum alloys for tribological applications using a combined microplasma oxidation (MPO) and arc ion plating (AIP)10.1016/j.wear.2005.01.029 ↗
12. Tribological behavior of microarc oxidation coatings on aluminum alloy10.2355/isijinternational.46.287 ↗
13. Structure and antiwear behavior of micro-arc oxidized coatings on aluminum alloy10.1016/S0257-8972(01)01671-1 ↗
14. The tribological performance of ultra-hard ceramic composite coatings obtained through microarc oxidation10.1016/S0257-8972(02)00646-1 ↗
15. An investigation into the mechanical and tribological properties of plasma electrolytic oxidation and hard-anodized coatings on 6082 aluminum alloy10.1016/j.msea.2011.06.032 ↗
16. Wear and corrosion resistant coatings on surface of cast A356 aluminum alloy by plasma electrolytic oxidation in moderately concentrated aluminate electrolytes10.1016/S1003-6326(17)60038-4 ↗
17. High temperature tribological behavior of microarc oxidation film on Ti-39Nb-6Zr alloy10.1016/j.surfcoat.2018.04.062 ↗
18. Microstructure and high temperature properties of two-step voltage-controlled mao ceramic coatings formed on Ti2AlNb alloy10.1016/j.apsusc.2014.03.148 ↗
19. High temperature wear behavior of aluminum oxide layers produced by AC micro arc oxidation10.1016/j.surfcoat.2009.09.057 ↗
20. Effects of evaluated temperature on tribological behaviors of micro-arc oxidated 2219 aluminum alloy and their field application10.1007/s00170-017-0919-4 ↗
21. Dry sliding wear of MAO-coated A356/20 vol.% SiCp composites in the temperature range 25-180 C10.1016/j.wear.2007.01.044 ↗
22. Pin on disk against ball on disk for the evaluation of wear improvement on cryo-treated metal cutting shears10.1063/1.4914239 ↗
23. Tribological coatings for aerospace applications and the case of WC-Co plasma spray coatings
24. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗