journal article·2019-01

Microstructural evolution of SiC coating on C/C composites exposed to 1500 °C in ambient air

Wei Zhou, Peng Xiao, Wei Luo, Yang Li

Ceramics International· Volume 45· Issue 1
Publisher page

Abstract

Abstract Oxidation-resistant coatings are essentially required to improve oxidation resistance performance of carbon/carbon (C/C) composites for applications under oxygen-containing atmosphere at elevated temperatures. In this work, thick and loose SiC coating was prepared by pack cementation (PC) to offer protection for C/C composites. Coating thickness, phases, anti-oxidation properties, and failure behavior at 1500 °C were characterized in ambient air for the as-prepared SiC coated specimens. As-prepared loose SiC coating with 150 µm thickness shows good oxidation resistance due to outstanding self-heal ability of SiO2. Weight loss of SiC coated specimens exposed to 1500 °C in ambient air is about 2.1% after oxidation for 58 h. Microstructural observation of SiC coated specimens after long-term oxidation indicates that bubbles caused by immigration and expansion of CO2 gas introduce defects. These defects cannot be rapidly healed by SiO2, which is main reason for SiC coating failure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Bansal · 2005
2. Ablation of the carbon/carbon composite nozzle-throats in a small solid rocket motor10.1016/j.carbon.2010.11.037 ↗
3. Effect of combustion gas mass flow rate on carbon/carbon composite nozzle ablation in a solid rocket motor10.1016/j.carbon.2011.11.034 ↗
4. Oxidation kinetics and mechanisms of a 2D-C/C composite10.1016/j.carbon.2006.06.027 ↗
5. Oxidative attack of carbon/carbon substrates through coating pinholes10.1016/S0008-6223(98)00206-1 ↗
6. Oxidation protective multilayer coatings for carbon–carbon composites10.1016/S0008-6223(01)00151-8 ↗
7. Oxidation through coating cracks of SiC-protected carbon/carbon10.1016/j.surfcoat.2008.09.013 ↗
8. A Si–SiC oxidation protective coating for carbon/carbon composites prepared by a two-step pack cementation10.1016/j.ceramint.2009.01.005 ↗
9. Oxidation behavior of oxidation protective coatings for C/C-SiC composites at 1500 °C10.1016/S1003-6326(08)60229-0 ↗
10. A C/SiC gradient oxidation protective coating for carbon/carbon composites10.1016/j.surfcoat.2006.07.239 ↗
11. A mullite/SiC oxidation protective coating for carbon/carbon composites10.1016/j.jeurceramsoc.2012.08.009 ↗
12. Comparison of the oxidation behaviors of SiC coatings on C/C composites prepared by pack cementation and chemical vapor deposition10.1016/j.surfcoat.2016.05.071 ↗
13. LPCVD-based SiO2/SiC multi-layers coating on graphite for improved anti-oxidation at wide-ranged temperatures10.1016/j.compositesb.2018.03.035 ↗
14. Silicon carbide based plasma sprayed coatings10.1016/j.surfcoat.2012.06.062 ↗
15. Microstructure and property of SiC coating for carbon materials10.1016/j.fusengdes.2007.03.001 ↗
16. CVD and CVR Silicon-based functionally gradient coatings on C/C composites10.1016/0008-6223(94)00166-W ↗
17. Resistance to oxidation and ablation of SiC coating on graphite prepared by chemical vapor reaction10.1016/j.corsci.2013.05.009 ↗
18. Ultra-high-temperature ceramic coatings for oxidation protection of carbon–carbon composites10.1111/j.1551-2916.2008.02331.x ↗
19. Effect of Al2O3 on the densification and oxidation behavior of SiC coating for carbon/carbon composites10.1016/j.ceramint.2018.04.072 ↗
20. The anti-oxidation behavior and infrared emissivity property of SiC/ZrSiO4–SiO2 coating
21. Microstructure and oxidation behavior of sol–gel mullite coating on SiC-coated carbon/carbon composites10.1016/j.jeurceramsoc.2015.06.033 ↗
22. Oxidation behavior of C/C composites with SiC/ZrSiO4–SiO2 coating10.1016/S1003-6326(17)60045-1 ↗
23. Oxidation resistance of a gradient self-healing coating for carbon/carbon composites10.1016/j.carbon.2007.08.036 ↗
24. A glass coating prepared by pulse arc discharge deposition for oxidation protection of carbon/carbon composites10.1016/j.apsusc.2014.08.013 ↗
25. Mullite based oxidation protection for SiC–C/C composites in air at temperatures up to 1900 K10.1016/S0955-2219(98)00242-8 ↗
26. Probing surface structure via time-of-escape analysis of gas in Knudsen regime10.1016/j.ces.2006.08.069 ↗
27. Preparation of an anti-oxidative SiC/SiO2 coating on carbon fibers by a sol–gel method10.1016/j.carbon.2013.06.059 ↗
28. The improvement in oxidation resistance of carbon by a graded SiC/SiO2 coating10.1016/S0955-2219(03)00098-0 ↗
29. Preparation of anti-oxidative SiC/SiO2 coating on carbon fibers from vinyltriethoxysilane by sol–gel method10.1016/j.apsusc.2012.11.056 ↗
30. SiC-Si-ZrSiO4 multiphase oxidation protective coating for carbon/carbon composites
31. A ZrSiO4/SiC oxidation protective coating for carbon/carbon composites10.1016/j.surfcoat.2012.01.030 ↗
32. Influence of the preparation temperature on the phase, microstructure and anti-oxidation property of a SiC coating for C/C composites10.1016/j.carbon.2004.01.066 ↗