Abstract
Abstract To improve ablation resistance of carbon/carbon (C/C) composites at high temperature, ZrB2–SiC coating was prepared on surface of SiC-coated C/C composites by supersonic atmosphere plasma spray. The coated C/C composites were pre-oxidized in air at 1373 K. In the present work, the influence of pre-oxidation treatment on the microstructure and ablation resistance of ZrB2–SiC coating was investigated. Ablation resistance of coated C/C composites was tested in oxyacetylene torch environment with the heat flux of 2400 kW/m2. Results show that the liquid glass phase seals defects in the as-sprayed coating after pre-oxidation for 15 min and a dense coating is obtained. The pre-oxidation coating can protect C/C composites for 90 s, which is due to the formation of a dense oxides layer and the molten ZrO2 layer.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Oxidation-resistant carbon–carbon composites up to 1700°C10.1016/0008-6223(94)00173-W ↗
2. Ablation behavior of TaC coating on SiC coated C/C composites at different temperature10.1016/j.ceramint.2012.06.034 ↗
3. Microstructure and oxidation resistance of Si–Mo–B coating for C/SiC coated carbon/carbon composites10.1016/j.corsci.2013.03.015 ↗
4. Oxidation and ablation of 3D carbon–carbon composite at up to 3000°C10.1016/0008-6223(94)00172-V ↗
5. Effects of TaC addition on the ablation resistance of C/SiC10.1016/j.matlet.2010.04.051 ↗
6. Ablation behavior and mechanism of C/C–ZrC–SiC composites under an oxyacetylene torch at 3000°C10.1016/j.ceramint.2012.10.273 ↗
7. ZrC ablation protective coating for carbon/carbon composites10.1016/j.carbon.2009.07.047 ↗
8. Microstructure and ablation resistance of ZrC coating for SiC coated carbon/carbon composites prepared by supersonic plasma spraying10.1007/s11666-011-9676-3 ↗
9. Ablative property of HfC-based multilayer coating for C/C composites under oxyacetylene torch10.1016/j.apsusc.2010.11.020 ↗
10. Anti-oxidation and ablation properties of carbon/carbon composites infiltrated by hafnium boride10.1016/j.carbon.2012.09.053 ↗
11. Advances in microstructure and mechanical properties of zirconium10.1016/S0921-5093(02)00520-8 ↗
12. Effects of heat treatments on oxidation resistance and mechanical properties10.1016/j.surfcoat.2008.04.015 ↗
13. Evaluation of ultra-high temperature ceramics for aeropropulsion use10.1016/S0955-2219(02)00140-1 ↗
14. Oxidation mechanism and resistance of ZrB2–SiC composites10.1016/j.corsci.2009.07.005 ↗
15. The ZrB2 volatility diagram10.1111/j.1551-2916.2005.00599.x ↗
16. Mechanical, thermal, and oxidation properties of refractory hafnium and zirconium compounds, J.A. Zaykoski, S.J. Causey10.1016/S0955-2219(99)00129-6 ↗
17. Oxidation of ZrB2-based ceramics in dry air10.1149/1.1618226 ↗
18. Oxidation-resistance ZrB2–SiC composites at 2200°C10.1016/j.compscitech.2007.08.017 ↗
19. Plasma spray deposition of ultra high temperature ceramics10.1016/j.surfcoat.2006.04.053 ↗
20. High-temperature chemistry and oxidation of ZrB2 ceramics containing SiC, Si3N4, Ta5Si3, and TaSi210.1111/j.1551-2916.2008.02420.x ↗
21. Rare-earth modified zirconium diboride high emissivity coatings for hypersonic applications10.1016/j.jeurceramsoc.2013.07.016 ↗
22. Plasma spray deposition and high temperature characterization of ZrB2–SiC protective coatings10.1016/S0257-8972(02)00058-0 ↗
23. MoSi2-based oxidation protective coatings for SiC-coated carbon/carbon composites prepared by supersonic plasma spraying10.1016/j.jeurceramsoc.2010.06.007 ↗
24. Ablation behavior of ZrB2-based coating prepared by supersonic plasma spraying for SiC-coated C/C composites under oxyacetylene torch10.1007/s11666-013-9913-z ↗
25. Thermogravimetric study of the oxidation of ZrB2 in the temperature range of 800–1500°C10.1149/1.2408279 ↗
26. Si–W–Mo coating for SiC coated carbon/carbon composites against oxidation10.1016/j.surfcoat.2007.04.062 ↗
27. National Standard Committee of China, GJB323A-96: Measurement Standard of Ablation Properties of Materials, Beijing, 1996.
28. Oxidation of zirconium diboride–silicon carbide at 1500°C at a low partial pressure of oxygen10.1111/j.1551-2916.2006.01229.x ↗
29. Oxidation of ZrB2–SiC10.1002/9780470294680.ch27 ↗
30. Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500°C10.1016/j.jeurceramsoc.2006.10.012 ↗
31. Oxidation of ZrB2–SiC: influence of SiC content on solid and liquid oxide phase formation10.1111/j.1551-2916.2008.02874.x ↗
32. Thermodynamic analysis of ZrB2–SiC oxidation: formation of a SiC-depleted region10.1111/j.1551-2916.2006.01329.x ↗