Abstract

Abstract The reactive wetting behavior of zirconia with SnAgCu-x%Ti (SAC-x%Ti, wt%, x = 1, 4) alloy was investigated via the sessile drop method in isothermal experiments. As temperatures elevated, the final contact angle decreased and the minimum contact angle of 21° and 7° were obtained at 1000 °C for SAC-1%Ti and SAC-4%Ti droplets, respectively. Kinetic calculations indicated that the spreading of SAC-Ti droplets on zirconia was controlled by interfacial reaction and the wetting activation energy was 108.8 kJ/mol. The reaction products distribution and morphology in droplets were influenced vastly by the addition of Ti. Along with the increase of Ti content from 1% to 4%, a great deal of Ti-Sn intermetallic compounds (IMCs) were generated in droplets, thereby the outline of droplets were transformed from hemispherical into similar trapezoidal due to the limited spreading and fluidity of droplets. Owing to the interfacial reaction between active elements Ti and zirconia and the subsequent formation of the Ti-O layer, the wettability of SAC-Ti/zirconia was greatly promoted. According to transmission electron microscopy (TEM) analysis, the thin Ti-O reaction layer consisted of the Ti 2 O, Ti 4 O 7 , Ti 7 O 13 and TiO 2 phase.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: ZnO doping and properties · Semiconductor materials and devices · Catalytic Processes in Materials Science

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Active metal brazing of zirconia10.1016/S1359-6454(00)00256-1 ↗
2. Improving the hot corrosion resistance of plasma sprayed ceria–yttria stabilized zirconia thermal barrier coatings by laser surface treatment10.1016/j.matdes.2013.12.075 ↗
3. Electroconductive ceramic tooling for dry deep drawing10.1016/j.jmatprotec.2009.08.020 ↗
4. Braze oxidation behavior and joint microstructure in YSZ/steel joints made using palladium brazes for SOFC applications10.1016/j.msea.2007.08.032 ↗
5. Microstructural and mechanical properties of jointed ZrO2/Ti–6Al–4V alloy using Ti33Zr17Cu50 amorphous brazing filler10.1016/j.matdes.2012.12.023 ↗
6. An insight into microstructural evolution during plastic deformation in AA6061 alloy after friction welding with alumina-YSZ composite10.1016/j.mechmat.2015.07.010 ↗
7. Actively brazed alumina to alumina joints using CuTi, CuZr and eutectic AgCuTi filler alloys10.1016/j.ceramint.2010.07.029 ↗
8. Brazing copper to alumina using reactive CuAgTi alloys10.1016/j.actamat.2009.10.029 ↗
9. Review article: recent advances in metal-ceramic brazing10.1590/S0366-69132003000400002 ↗
10. Active metal brazing of silicon nitride ceramics using a Cu-based alloy and refractory metal interlayers10.1016/j.ceramint.2015.12.087 ↗
11. Initial stages of wetting of alumina by reactive CuAgTi alloys10.1016/j.scriptamat.2011.03.026 ↗
12. Progress in understanding and modeling reactive wetting of metals on ceramics10.1016/j.cossms.2006.04.004 ↗
13. Effect of Cr on the wetting in Cu/graphite system10.1016/j.apsusc.2011.02.060 ↗
14. Interface reaction in ultrasonic vibration-assisted brazing of aluminum to graphite using Sn–Ag–Ti solder foil10.1016/j.jmatprotec.2015.02.028 ↗
15. Bonding mechanisms in silicon nitride brazing10.1111/j.1151-2916.1990.tb06552.x ↗
16. Wetting and interfacial reactivity in Ag–Zr/sintered AlN system10.1016/S1359-6462(02)00449-9 ↗
17. Wetting of B4C, TiC and graphite substrates by molten Mg10.1016/j.matchemphys.2011.07.040 ↗
18. Factors governing interfacial reactions in liquid metal/non-oxide ceramic systems: ni-based alloy–Ti/sintered AlN system10.1016/j.jeurceramsoc.2008.06.004 ↗
19. Wetting and interfacial behavior of Sn–Ti alloys on zirconia
20. Reactive wetting of TiC-Ni cermet by Ag-Cu-Zn alloy during evaporation10.1016/j.vacuum.2017.01.014 ↗
21. Reactive wetting of tin/steel and tin/aluminum at 350–450 °C10.1016/j.jallcom.2017.05.036 ↗
22. Dynamics of wetting in reactive metal/ceramic systems
23. Influence of interfacial reaction on reactive wettability of molten Ag-Cu-X wt%Ti filler metal on SiC ceramic substrate and mechanism analysis10.1016/j.apsusc.2017.12.106 ↗
24. Brazing of stainless steel to Yttria-stabilized zirconia using gold-based brazes for solid oxide fuel cell applications10.1111/j.1744-7402.2007.02126.x ↗
25. Characterization of yttria-stabilized-zirconia/stainless steel joint interfaces with gold-based interlayers for solid oxide fuel cell applications10.1016/j.jeurceramsoc.2013.08.036 ↗
26. Brazing of zirconia with AgCuTi and SnAgTi active filler metals10.1007/s11661-000-0169-0 ↗
27. Wetting and low temperature bonding of zirconia metallized with Sn0.3Ag0.7Cu-Ti alloys10.1016/j.ceramint.2018.03.207 ↗
28. Brazing ZrO2 ceramic to Ti–6Al–4V alloy using NiCrSiB amorphous filler foil: interfacial microstructure and joint properties10.1016/j.matchar.2013.04.009 ↗
29. Effects of fabrication parameters on interface of zirconia and Ti-6Al-4V joints using Zr55Cu30Al10Ni5 amorphous filler10.1007/s11665-013-0534-y ↗
30. Effect of short-term aging on interfacial and mechanical properties of yttria stabilized zirconia (YSZ)/stainless steel joints10.1016/j.jeurceramsoc.2014.10.001 ↗
31. Interfacial and mechanical characterization of yttria-stabilized zirconia (YSZ) to stainless steel joints fabricated using Ag–Cu–Ti interlayers10.1016/j.ceramint.2013.07.119 ↗
32. Bonding of zirconia to super alloy with the active brazing technique10.1016/S0955-2219(00)00162-X ↗
33. Brazing of yttria-stabilized zirconia (YSZ) to stainless steel using Cu, Ag, and Ti-based brazes10.1007/s10853-007-1985-z ↗
34. Wettability and interfacial reactions in the systems NiYSZ and Ni/Ti-TiO2/YSZ10.1016/1359-6454(96)00019-5 ↗
35. Effect of Ti content on the metallization layer and copper/alumina brazed joint10.1016/j.ceramint.2017.07.016 ↗
36. Chemical reaction-limited spreading: the triple line velocity versus contact angle relation10.1016/S1359-6454(02)00309-9 ↗
37. Massalski · 1990
38. The effect of solid particles on liquid viscosity10.1002/srin.201000207 ↗