journal article·2017-05

Comparison of corrosion behavior of Ti 3 SiC 2 and Ti 3 AlC 2 in NaCl solutions with Ti

M. Zhu, R. Wang, C. Chen, H.B. Zhang, G.J. Zhang

Ceramics International· Volume 43· Issue 7
Publisher page

Abstract

Abstract Corrosion behavior of self-sintered, ternary-layered titanium silicon carbide (Ti 3 SiC 2 ) and titanium aluminum carbide (Ti 3 AlC 2 ) fabricated by an in-situ solid-liquid reaction/hot pressing process was investigated by potentiodynamic polarization, potentiostatic polarization and electrochemical impedance spectroscopy in a 3.5% NaCl solution. Commercially pure titanium (Ti) was selected for comparison through XRD, XPS, SEM and EDS examinations for elucidating both the passivation behavior and corrosion mechanism of the alloys. Both Ti 3 SiC 2 and Ti 3 AlC 2 exhibited significantly superior passivation characteristics compared to Ti; Ti 3 SiC 2 also showed better corrosion resistance. The silicon/aluminum site is prone to attack, and the difference in the diffusion rate between the A-site atoms and titanium decreases the passivation ability of the MAX phase. CP titanium exhibited a lower passivation current density and did not undergo breakdown in the test potential region while two MAX phases are destroyed. Nevertheless, the corrosion resistances of Ti 3 SiC 2 and Ti 3 AlC 2 are comparable to that of CP titanium.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. The MN+1AXN phases: a new class of solid; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
2. Structure and crystal chemistry of Ti3SiC210.1016/S0022-3697(98)00226-1 ↗
3. The M(N+1)AX(N) phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
4. Electronic properties of Ti3SiC2-based solid solutions10.1103/PhysRevB.58.16042 ↗
5. Ab into calculation of titanium silicon carbide10.1103/PhysRevB.60.1441 ↗
6. The MAX phases: unique new carbide and nitride materials-ternary ceramics turn out to be surprisingly soft and machinable, yet also heat-tolerant, strong and light weight10.1511/2001.28.736 ↗
7. Preliminary report on the electrochemical behavior of Ti3SiC210.1023/A:1006653806613 ↗
8. The corrosion behavior of Ti3SiC2 in common acids and dilute NaOH10.1016/S0010-938X(02)00227-5 ↗
9. Corrosion behavior and passive film characteristics formed on Ti, Ti3SiC2, and Ti4AlN3 in H2SO4 and HCl10.1149/1.1637897 ↗
10. Corrosion behavior of select MAX phases in NaOH, HCl and H2SO410.1016/j.corsci.2006.04.005 ↗
11. V.D. Jovic, M.W. Barsoum, Electrolytic Cell and Electrodes for use In Electrochemical Processes, US Patent 7001494B2, 2006.
12. Corrosion behavior of Ti3AlC2 in NaOH and H2SO410.1016/j.jeurceramsoc.2010.07.002 ↗
13. Experimental and thermodynamic study of the hydrothermal oxidation behavior of Ti3SiC2 powders10.1016/j.scriptamat.2008.06.005 ↗
14. Effect of Al dopant on the hydrothermal oxidation behavior of Ti3SiC2 powders10.1016/j.jeurceramsoc.2008.12.010 ↗
15. Mechanisms and kinetics of the hydrothermal oxidation of bulk titanium silicon carbide10.1111/j.1551-2916.2009.03570.x ↗
16. Hydrothermal oxidation behavior of bulk titanium aluminum carbide10.1111/j.1551-2916.2011.04590.x ↗
17. Corrosion behavior of selected Mn+1AXn phases in hot concentrated HCl solution: effect of A element and MX layer10.1016/j.corsci.2012.03.047 ↗
18. The formation of chlorine dioxide in the electrochemical treatment of drinking water for disinfection10.1016/j.electacta.2005.01.061 ↗
19. Study on pretreatment of seawater electrolysis for desalination10.1080/19443994.2013.782088 ↗
20. Water disinfection by electrochemical treatment10.1016/j.biortech.2003.11.021 ↗
21. Electrochemical technologies in wastewater treatment10.1016/j.seppur.2003.10.006 ↗
22. Passivity breakdown of titanium in LiBr solutions10.1149/2.035401jes ↗
23. Electrochemical stability of anodic titanium oxide films grown at potentials higher than 3V in a simulated physiological solution10.1016/j.corsci.2006.08.010 ↗
24. Characterisation of titanium oxide film grown in 0.9% NaCl at different sweep rates10.1016/j.electacta.2005.05.051 ↗
25. Characterization of anodized titanium for hydrometallurgical applications-evidence for the reduction of cupric on titanium dioxide10.1016/j.apsusc.2013.06.168 ↗
26. Modelling the formation and growth of anodic passive films on metals in concentrated acid solutions10.1007/s100080050041 ↗
27. The ability of a surface charge approach to describe barrier film growth on tungsten in acidic solutions10.1016/S0013-4686(97)00037-6 ↗
28. The stability of the passive state of iron chromium alloys in sulphuric acid solution10.1016/S0010-938X(99)00003-7 ↗
29. Evidence of coupling between film growth and metal dissolution in passivation processes10.1016/S0013-4686(03)00578-4 ↗
30. Passivity of titanium, Part 1: film growth model diagnostics10.1007/s10008-013-2334-6 ↗
31. Some personal adventures in passivity—a review of the point defect model for film growth10.1134/S1023193512030068 ↗
32. Passivity-the key to our metals-based civilization10.1351/pac199971060951 ↗
33. The stability of the passive state of iron chromium alloys in sulphuric acid solution10.1016/S0010-938X(99)00003-7 ↗
34. Evidence of coupling between film growth and metal dissolution in passivation processes10.1016/S0013-4686(03)00578-4 ↗
35. Determination of the sp3/sp2 ratio of a-C:H by XPS and XAES10.1016/S0022-3093(99)00388-9 ↗
36. XPS and laser Raman analysis of hydrogenated amorphous carbon films10.1016/S0925-9635(02)00374-6 ↗
37. Study of structure, tribological properties and growth mechanism of DLC and nitrogen-doped DLC films deposited by electrochemical technique10.1016/j.apsusc.2004.05.005 ↗