Abstract

Abstract At present, the fixed-abrasive wire saw machining technology is widely used in the slicing process of SiC single crystal. And the subsurface microcrack damage depth of wire sawn SiC wafer is an important quality control parameter. In this paper, experimental and numerical analysis of the subsurface microcrack damage depth of single-crystal SiC in wire sawing is presented. A finite element model (FEM) which was used for simulation and calculation of subsurface microcrack damage depth in wire saw slicing SiC crystal wafer was established. The variations of maximum principal stress and stress change rate of sawn crystal and slice in wire sawing were analyzed, and the validity of the FEM was verified by sawing experiment. Further, microcrack damage depths under different ingot feed speeds and wire speeds were predicted and the influence of process parameters on microcrack damage depth was discussed. Research results show that the microcrack damage depth values of simulation are lower than the experimental measurement, but with a consistent change trend of a relative error is less than 15.92%. The subsurface microcrack damage depths of sawn wafer decrease with the increase of wire speed and decrease of feed speed. The research results can be helpful to develop precision and high quality slicing technology of SiC single crystal.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Advanced machining processes and optimization · Advanced Machining and Optimization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Fixed abrasive diamond wire saw slicing of single-crystal SiC wafers10.1081/AMP-120029960 ↗
2. Experimental investigation on the machining characteristics of single-crystal SiC sawing with the fixed diamond wire10.1007/s00170-015-7250-8 ↗
3. Prediction of sawing force for single-crystal silicon carbide with fixed abrasive diamond wire saw10.1016/j.mssp.2017.01.014 ↗
4. A scratching force model of diamond abrasive particles in wire sawing of single crystal SiC10.1016/j.mssp.2017.05.032 ↗
5. Surface roughness optimization in processing SiC monocrystal wafers by wire saw machining with ultrasonic vibration10.1177/0954405413508116 ↗
6. Indentation in single-crystal 6H silicon carbide: experimental investigations and finite element analysis10.1016/j.ijmecsci.2017.11.021 ↗
7. The mechanism of ductile deformation in ductile regime machining of 6H SiC10.1016/j.commatsci.2014.10.045 ↗
8. Investigation of subsurface damages and surface roughness in grinding process of Zerodur glass–ceramic10.1016/j.apsusc.2014.05.137 ↗
9. Effect of grinding wheel spindle vibration on surface roughness and subsurface damage in brittle material grinding10.1016/j.ijmachtools.2015.01.003 ↗
10. Determination of the impact of the wire velocity on the surface damage of diamond wire sawn silicon wafers10.1016/j.egypro.2015.07.124 ↗
11. Effect of wire speed on subsurface cracks in wire sawing process of single crystal silicon carbide10.1016/j.engfracmech.2017.09.002 ↗
12. Slicing large-diameter SiC single crystal by using diamond wire saw
13. Experiment study on electroplated diamond wire saw slicing single-crystal silicon10.1016/j.mssp.2016.08.003 ↗
14. Subsurface crack damage in silicon wafers induced by resin bonded diamond wire sawing10.1016/j.mssp.2016.10.021 ↗
15. Simple technique for observing subsurface damage in machining of ceramics10.1111/j.1151-2916.1994.tb05424.x ↗
16. Experimental investigation of surface/subsurface damage formation and material removal mechanisms in SiC grinding10.1016/j.ijmachtools.2007.10.013 ↗
17. Han · 2013 · 4
18. Coupling stress caused by thermal and slicing force in KDP crystal slicing with fixed abrasive wire saw10.1007/s00170-018-1893-1 ↗