journal article·2018-02

Ceramic nanoparticles addition in pure copper plate: FSP approach, microstructure evolution and texture study using EBSD

Akbar Heidarzadeh, Hesam Pouraliakbar, Soheil Mahdavi, Mohammad Reza Jandaghi

Ceramics International· Volume 44· Issue 3
Publisher page

Abstract

Abstract In this study, the effect of ceramic nanoparticles addition on the microstructure and texture of friction stir processed (FSP) copper has been investigated. For this purpose, two pure copper plates with and without Al2O3 nanoparticles were FSPed at rotational speed of 800 rpm and traverse speed of 100 mm min−1. Electron back scattered diffraction (EBSD) technique was employed in order to study the microstructure and texture of the fabricated samples. Based on the obtained results, considerable grain refinement by dynamic recrystallization (DRX) mechanism was observed in both specimens. However, Al2O3 inset led to evolution of ultrafine grained (UFG) structure with an average grain size of 0.7 µm. In addition, Al2O3 addition caused formation of lower twin boundaries and stronger texture components compared with the sample without ceramic reinforcements. The presence of nanoparticles increased the proportion of the continuous DRX mechanism (CDRX) compared to the discontinuous mechanism (DDRX) during grain structure formation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Prediction of grain size and mechanical properties in friction stir welded pure copper joints using a thermal model10.1007/s00170-014-6543-7 ↗
2. Microstructure, properties and wear behaviors of (Ni3Al)p reinforced Cu matrix composites10.1016/S1005-0302(11)60167-9 ↗
3. The influence of technological process on dry sliding wear behaviour of titanium carbide reinforcement copper matrix composites10.2320/matertrans.M2010270 ↗
4. Al-Mg-Si/SiC laminated composites: fabrication, architectural characteristics, toughness, damage tolerance, fracture mechanisms10.1016/j.compositesb.2017.05.055 ↗
5. Improvement of interfacial bonding and mechanical properties of Cu-Al2O3 composite by Cr-nanoparticle-induced interfacial modification10.1016/j.jallcom.2016.11.055 ↗
6. Effect of tool pin design on the microstructural evolutions and tribological characteristics of friction stir processed structural steel10.1016/j.measurement.2015.02.051 ↗
7. Elucidating of tool rotational speed in friction stir welding of 7020-T6 aluminum alloy10.1007/s00170-015-7252-6 ↗
8. Tensile behavior of friction stir welded AA 6061-T4 aluminum alloy joints10.1016/j.matdes.2011.12.022 ↗
9. Simulation of dynamic recrystallization process during friction stir welding of AZ91 magnesium alloy10.1007/s00170-015-7595-z ↗
10. 3 - Microstructural evolution
11. Effect of tool pin profile on distribution of reinforcement particles during friction stir processing of B4C/aluminum composites
12. Effect of friction stir processing on the microstructure and mechanical properties of Cu–TiC composite10.1016/j.ceramint.2014.04.158 ↗
13. Characterization of oxide dispersion strengthened copper based materials developed by friction stir processing10.1016/j.matdes.2014.04.012 ↗
14. Influence of tool rotational speed on microstructure and sliding wear behavior of Cu/B4C surface composite synthesized by friction stir processing10.1016/S1003-6326(15)63583-X ↗
15. Characterization of boron carbide particulate reinforced in situ copper surface composites synthesized using friction stir processing10.1016/j.matchar.2013.07.001 ↗
16. Prediction of mechanical and wear properties of copper surface composites fabricated using friction stir processing10.1016/j.matdes.2013.09.053 ↗
17. Microstructure and mechanical properties of a B4C particle-reinforced Cu matrix composite fabricated by friction stir welding10.1016/j.jallcom.2016.08.304 ↗
18. Effect of ceramic particulate type on microstructure and properties of copper matrix composites synthesized by friction stir processing10.1016/j.jmrt.2016.01.003 ↗
19. Friction and wear performance of copper–graphite surface composites fabricated by friction stir processing (FSP)10.1016/j.wear.2013.04.023 ↗
20. Microstructural, mechanical and tribological behavior of aluminum nitride reinforced copper surface composites fabricated through friction stir processing route10.1016/j.msea.2017.02.010 ↗
21. Microstructure and sliding wear characterization of Cu/TiB2 copper matrix composites fabricated via friction stir processing10.1016/j.jascer.2017.06.002 ↗
22. Microstructure and mechanical properties of Cu/SiC metal matrix composite fabricated via friction stir processing10.1016/j.matdes.2013.08.107 ↗
23. Fabrication of in situ Cu/SiC composites using multi-pass friction stir processing: evaluation of microstructural, porosity, mechanical and electrical behavior10.1016/j.compositesa.2011.06.010 ↗
24. On the role of processing parameters in producing Cu/SiC metal matrix composites via friction stir processing: investigating microstructure, microhardness, wear and tensile behavior10.1016/j.matchar.2010.11.005 ↗
25. Intrinsic high cycle fatigue behavior of ultrafine grained pure Cu with stable structure10.1007/s40843-016-5068-6 ↗
26. Microstructure and mechanical properties of friction stir processed Cu with an ideal ultrafine-grained structure10.1016/j.matchar.2016.10.009 ↗
27. Approach for fabrication of Cu-Al2O3 surface composites by friction stir processing10.1016/j.mspro.2014.07.286 ↗
28. Microstructure, texture, and mechanical properties of friction stir welded commercial brass alloy10.1016/j.matchar.2016.07.009 ↗
29. Constrained groove pressing and subsequent annealing of Al-Mn-Si alloy: microstructure evolutions, crystallographic transformations, mechanical properties, electrical conductivity and corrosion resistance10.1016/j.matdes.2017.03.053 ↗
30. Study on the post-rolling direction of severely plastic deformed Aluminum-Manganese-Silicon alloy10.1016/j.acme.2016.06.005 ↗
31. On the effect of non-isothermal annealing and multi-directional forging on the microstructural evolutions and correlated mechanical and electrical characteristics of hot-deformed Al-Mg alloy10.1016/j.msea.2016.01.056 ↗
32. Achieving ultrafine-grained ferrite structure in friction stir processed weld metal10.1016/j.matlet.2015.09.115 ↗
33. Particle refinement and fine-grain formation leading to enhanced mechanical behaviour in a hypo-eutectic Al–Si alloy subjected to multi-pass friction stir processing10.1016/j.matchar.2016.01.011 ↗
34. Achieving ultrafine-grained structure in a pure nickel by friction stir processing with additional cooling10.1016/j.matdes.2013.12.001 ↗
35. Achieving ultrafine grain size in Mg–Al–Zn alloy by friction stir processing10.1016/j.scriptamat.2007.04.007 ↗
36. Strategy for severe friction stir processing to obtain acute grain refinement of an Al–Zn–Mg–Cu alloy in three initial precipitation states10.1016/j.matchar.2015.12.014 ↗
37. Modification of mechanical properties of friction stir welded Cu joint by additional liquid CO2 cooling10.1016/j.matdes.2013.10.076 ↗
38. Microstructural evolution of pure copper during friction-stir welding10.1080/14786435.2015.1006293 ↗
39. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
40. A review of dynamic recrystallization phenomena in metallic materials10.1016/j.matdes.2016.09.012 ↗
41. Humphreys · 2004 · 285