Porous SiC ceramics fabricated by reactive infiltration of gaseous silicon into charcoal
Source abstract
Abstract
Abstract Basswood has been converted to a porous biocarbon template by carbonizing under vacuum at 1200 °C. Subsequent reactive infiltration of gaseous silicon at 1500–1700 °C for 0.5–8 h in inert atmosphere resulted in the formation of a porous, cellular β-SiC ceramic. X-ray diffraction (XRD) studies show the resulting SiC, obtained at 1600 °C for 6 h in static argon atmosphere, is β-SiC. Scanning electron microscopy (SEM) reveals the resulting SiC ceramic reproduces the biomorphic cellular morphology of basswood tissue with high precision. Gaseous Si diffuses into charcoal through its continuous tracheidal cell channels, and reacts with carbon in the cell wall to form SiC. Growth of SiC layer is dependent of the diffusion of Si vapor through the primary porous SiC layer and further gas–solid reaction of Si(g) and C(s) at C/SiC interface. The densification of SiC strut material may occur at moderate temperatures and holding time.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced Cellulose Research Studies · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Effect of microstructure on the fracture behavior of biomorphous silicon carbide ceramics10.1016/S0955-2219(02)00135-8 ↗
2. Silicon/silicon carbide composites fabricated by infiltration of a silicon melt into charcoal10.1111/j.1151-2916.1999.tb02234.x ↗
3. Porous titania ceramic prepared by mimicking silicified wood10.1111/j.1151-2916.2000.tb01421.x ↗
4. Wood: a natural fibre reinforced composite
5. Biomorphic cellular silicon carbide ceramics from wood. I. Processing and microstructure; II. Mechanical properties10.1016/S0955-2219(98)00156-3 ↗
6. Effect of carbonizing speed on the property changes of woodceramics impregnated with liquefacient wood10.1016/S0167-577X(01)00399-8 ↗
7. Dry sliding friction and wear behavior of woodceramics/Al–Si composites
8. High temperature compressive mechanical behavior of joined biomorphic silicon carbide ceramics10.1016/S0955-2219(02)00138-3 ↗
9. Biomorphic SiC-ceramic prepared by Si-vapor phase infiltration of wood10.1016/S0955-2219(02)00131-0 ↗
10. Porous TiC ceramics derived from wood template10.1023/A:1021652930124 ↗
11. High temperature compressive mechanical behavior of biomorphic silicon carbide ceramics10.1016/S1359-6462(00)00494-2 ↗
12. Mechanical properties and microstructure of Si/SiC materials derived from native wood10.1016/S0921-5093(01)01387-9 ↗
13. Preparation of macroporous SiC from Si and wood powder using infiltration-reaction process10.1016/S0921-5093(03)00281-8 ↗
14. Conversion of oak to cellular silicon carbide ceramic by gas-phase reaction with silicon monoxide10.1111/j.1151-2916.2001.tb00822.x ↗
15. Low density biomorphic silicon carbide: microstructure and mechanical properties10.1016/S0955-2219(02)00137-1 ↗
16. Biomimetic process for producing SiC wood10.1111/j.1151-2916.1995.tb07988.x ↗
17. Near net shape manufacturing of ceramics10.1016/S0254-0584(99)00115-7 ↗
18. Silicon carbide coating by reactive pack cementation-part I: silicon carbide/silica interaction10.1002/(SICI)1521-3862(200002)6:1<33::AID-CVDE33>3.0.CO;2-Z ↗
19. A. Kaindl, Cellular SiC Ceramics from Wood, Ph.D. Thesis, University of Erlangen-Nuernberg, Erlangen, German, 2000.