Microstructure and mechanical properties of B4C–TiB2–SiC composites fabricated by spark plasma sintering
Source abstract
Abstract
Abstract Boron carbide ceramics have broad application prospects due to their excellent performance. However, their poor sinterability and low fracture toughness limit their application, especially in the field of bulletproof armor. In this work, B4C–TiB2–SiC composites were successfully prepared by spark plasma sintering (SPS) with B4C, TiB2, and SiC powder mixtures. The effects of different SiC contents on the mechanical properties and microstructure of B4C–TiB2–SiC composites were investigated. The B4C–TiB2–SiC composites with 15 wt% SiC combined a relative density of 98.43%, a fracture toughness of 4.17 MPa m1/2, as well as Vickers hardness of 30.07 GPa. The addition of SiC can increase the toughness of B4C–TiB2–SiC composites while maintaining high hardness. The main reason for this behavior is grain refinement of B4C and TiB2 due to the pinning effect of the SiC phase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Boron and Carbon Nanomaterials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Boron carbide—a comprehensive review10.1016/0955-2219(90)90048-K ↗
2. High strength B4C–TiB2 composites fabricated by reaction hot-pressing10.1016/S0955-2219(02)00274-1 ↗
3. Synthesis and consolidation of boron carbide: a review10.1179/095066009X12506721665211 ↗
4. Comparing the effects of different sintering methods for ceramics on the physical and mechanical properties of B4C–TiB2 nanocomposites10.1016/j.ijrmhm.2015.04.003 ↗
5. In situ synthesis and sintering of B4C/ZrB2 composites from B4C and ZrH2 mixtures by spark plasma sintering10.1016/j.jeurceramsoc.2014.10.013 ↗
6. Analytical and experimental investigation of the effect of SPS and hot rolling on the microstructure and flexural behavior of Ti6Al4V matrix reinforced with in-situ TiB and TiC10.1016/j.jallcom.2016.09.026 ↗
7. Microstructure and mechanical properties of pulsed electric current sintered B4C–TiB2 composites10.1016/j.msea.2010.10.022 ↗
8. Boron carbide and nitride as reactants for in situ syntheses of boride-containing ceramic composites10.1016/S0955-2219(03)00607-1 ↗
9. Processing and mechanical properties of boron carbide sintered with TiC10.1016/S0955-2219(98)00071-5 ↗
10. Han · 2007 · 917
11. Preparation and abrasive properties of eutectic compositions in the system B4C-SiC-TiB2
12. Preparation of directionally solidified B4C–TiB2–SiC ternary eutectic composites by a floating zone method and their properties10.2320/matertrans.46.2067 ↗
13. Spark plasma sintering of B4C-TiB2-SiC composite ceramics using B4C, Ti3SiC2 and Si as starting materials10.1016/j.ceramint.2018.08.245 ↗
14. Microstructure and mechanical properties of B4C-TiB2-SiC composites toughened by composite structural toughening phases10.1111/jace.14815 ↗
15. High toughness and electrical discharge machinable B4C-TiB2-SiC composites fabricated at the low sintering temperature10.1016/j.msea.2017.06.100 ↗
16. Combined carbothermal synthesis of powders in the B4C–SiC–TiB2 system10.1007/s11148-017-0076-1 ↗
17. Microstructures and mechanical properties of B4C-TiB2-SiC composites fabricated by ball milling and hot pressing10.1016/j.jeurceramsoc.2018.02.020 ↗
18. Additive-free superhard B4C with ultrafine-grained dense microstructures10.1016/j.jeurceramsoc.2013.10.006 ↗
19. High strength-high toughness B4C-TiB2 composites10.1023/A:1006766910536 ↗
20. Processing, microstructure, and mechanical properties of B4C―TiB2 particulate sintered composites. Part II. Fracture and mechanical properties10.1023/A:1011378825628 ↗
21. Microstructural development and mechanical properties of hot-pressed SiC reinforced TiB2 based composite10.1016/j.ijrmhm.2015.03.014 ↗
22. Mechanical properties and fracture behavior of B4C-nano/micro SiC composites produced by pressureless sintering10.1016/j.ijrmhm.2017.10.001 ↗
23. Microstructure and properties of B4C-SiC composites prepared by polycarbosilane-coating/B4C powder route10.1016/j.jeurceramsoc.2013.10.039 ↗
24. Microstructure and properties of (SiC, TiB2)/B4C composites by reaction hot pressing10.1016/j.ceramint.2005.05.022 ↗
25. In situ platelet-toughened TiB2–SiC composites prepared by reactive pulsed electric current sintering10.1016/j.scriptamat.2011.03.015 ↗
26. Effect of TiB2 content on microstructure and mechanical properties of in-situ fabricated TiB2/B4C composites10.1016/S1003-6326(11)61608-7 ↗
27. Toughening of super-hard ultra-fine grained B4C densified by spark-plasma sintering via SiC addition10.1016/j.jeurceramsoc.2013.01.018 ↗
28. Microstructure and properties of B4C-SiC composites prepared by polycarbosilane-coating/B4C powder route10.1016/j.jeurceramsoc.2013.10.039 ↗