journal article·2016-05

TiC whisker reinforced ultra-fine TiC-based cermets: Microstructure and mechanical properties

Huiwen Xiong, Zhiyou Li, Kechao Zhou

Ceramics International· Volume 42· Issue 6
Publisher page

Abstract

Abstract TiC whisker reinforced ultra-fine TiC-based cermets were fabricated and their microstructures as well as mechanical properties were characterized and compared with microsized and ultra-fine cermets. The effects of high energy milling and subsequent annealing on the composition and microstructure of microsized TiC powders were studied. It was shown that the particle size distribution of TiC powders played a critical role in determining cermets׳ microstructure and properties. Inverse grain (White core with grey rim) only exists in ultra-fine cermet with a narrow size distribution of annealed TiC powders. Large discrepancy of larger TiC powders (microsized particles or whiskers) and ultra-fine particles in size resulted in a bimodal grain size feature. Additionally, mechanical property testing was conducted and was related to the microstructural features. The whisker reinforced cermets own much higher toughness of 12.43 Mpa m1/2 than the microsized and ultra-fine cermets, with a hardness (Hv30, 1620) between them.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Powder Metallurgy Techniques and Materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Effect of submicron Ti(C,N) on the microstructure and the mechanical properties of Ti(C,N)-based cermets10.1016/j.ijrmhm.2011.05.007 ↗
2. Microstructure and cutting performance investigation of Ti(C,N)-based cermets containing various types of secondary carbides10.1016/j.ijmachtools.2006.09.012 ↗
3. Effect of powder size on microstructure and mechanical properties of Ti(C,N) based cermets10.1179/174367607X202636 ↗
4. Effect of ultra- fine powders on the microstructure of Ti(C,N)–xWC–Ni cermets10.1016/j.actamat.2003.11.021 ↗
5. Preparation of Ni–Mo–C/Ti(C,N) coated powders and its influence on the microstructure and mechanical properties of Ti(C,N) -based cermets10.1016/j.ceramint.2015.03.062 ↗
6. Microstructure, hardness and toughness of nanostructured and conventional WC–Co composites10.1016/S0965-9773(98)00123-8 ↗
7. Microstructure and mechanical properties of ultrafine Ti(CN)-based cermets fabricated from nano/submicron starting powders10.1016/j.ceramint.2004.09.013 ↗
8. Effect of nano-size powders on the microstructure of Ti(C,N)–xWC–Ni cermets10.1111/j.1551-2916.2007.01654.x ↗
9. Effect of TiC/TiN powder size on microstructure and properties of Ti(C,N)-based cermets10.1016/j.msea.2006.10.003 ↗
10. Synthesis, sintering, and mechanical properties of nanocrystalline cemented tungsten carbide – a review10.1016/j.ijrmhm.2008.07.011 ↗
11. Fabrication of nanocomposite Ti(C,N)-based cermet by spark plasma sintering10.1016/j.matchemphys.2004.12.031 ↗
12. Microstructure, mechanical properties and thermal shock resistance of nano-TiN modified TiC-based cermets with different binders10.1016/j.ijrmhm.2008.01.008 ↗
13. Toughened ultrafine (Ti,W)(C,N)-based cermets10.1016/j.scriptamat.2004.09.017 ↗
14. Development and application of tool wear: a review of the characterization of TiC-based cermets with different binders10.1016/j.cej.2014.06.078 ↗
15. Hardening and toughening mechanisms of cemented carbides with plate-like WC grains prepared by seeding10.2320/matertrans.M2010380 ↗
16. High temperature strength of WC–Co base cemented carbide having highly oriented plate-like triangular prismatic WC grains10.2497/jjspm.49.299 ↗
17. Preparation of a highly toughened (Ti,W)C–20Ni cermet through in situ formation of solid solution and WC whiskers10.1016/j.ceramint.2014.11.031 ↗
18. Effect of SiC nano-whisker addition on TiCN-based cermets prepared by spark plasma sintering10.1016/j.ijrmhm.2012.03.008 ↗
19. Effect of SiC whisker addition on the microstructures and mechanical properties of Ti(C,N)-based cermets10.1016/j.matdes.2010.07.028 ↗
20. Synthesis and growth mechanism of TiC whiskers by carbothermal reduction of titania/microcrystalline cellulose10.1111/jace.13539 ↗
21. Large-scale synthesis of TiC whiskers by carbothermal reduction with microcrystalline cellulose as the carbon source10.1016/j.jcrysgro.2015.09.004 ↗
22. Effects of ball milling time on the synthesis and consolidation of nanostructured WC–Co composites10.1016/j.ijrmhm.2009.05.006 ↗
23. Hardness to toughness relationship of fine-grained WC–Co hard metals10.1016/S0263-4368(98)00028-6 ↗
24. Initial stages of oxidation of near-stoichiometric titanium carbide at low oxygen pressures10.1016/j.jallcom.2008.04.067 ↗
25. Effect of stoichiometry on the surface energies of {100}and {111} and the crystal shape of TiCx and TiNx10.1039/C2CE26419F ↗
26. Study on phase evolution during reaction synthesis of ultrafine (Ti, W, Mo, V)(CN)–Ni composite powders10.1016/j.matchemphys.2009.07.021 ↗
27. High-energy milling of nonstoichiometric carbides: Effect of nonstoichiometry on particle size of nanopowders10.1016/j.jallcom.2013.08.008 ↗
28. Effect of nonstoichimetry of NbCy and TaCy powders on their high-energy ball milling10.1016/j.ijrmhm.2014.05.018 ↗
29. Rim structure in Ti(C0.7N0.3)–WC–Ni cermets10.1111/j.1151-2916.2003.tb03551.x ↗
30. Inverse core-rim microstructure in (Ti,Ta)(C,N)-based cermets developed by a mechanically induced self-sustaining reaction10.1016/j.ijrmhm.2011.09.003 ↗
31. Microstructure characterization and mechanical properties of Ti(C, N)-based cermets with AlN addition10.1016/j.ceramint.2014.12.068 ↗
32. Correlation of transverse rupture strength of WC–Co with hardness10.1016/j.ijrmhm.2004.11.005 ↗