journal article·2013-04

Influence of grain size on high temperature oxidation behavior of Cr2AlC ceramics

Shibo Li, Xiaodong Chen, Yang Zhou, Guiming Song

Ceramics International· Volume 39· Issue 3
Publisher page

Abstract

Abstract The influence of grain size on the oxidation behavior of Cr 2 AlC at 1100 °C and 1200 °C for different times was investigated using fine grained (2 μm) and coarse grained (60 μm) samples. The two materials show a good oxidation resistance owing to the formation of a dense and continuous Al 2 O 3 layer. The oxidation rate of the fine grained Cr 2 AlC is relatively faster than that of the coarse grained Cr 2 AlC. The microstructure and phase composition of scale was characterized. After oxidation at 1100 °C and 1200 °C for long times up to 100 h, only a dense and continuous α -Al 2 O 3 oxide layer formed on both the fine grained and coarse grained Cr 2 AlC. However, after oxidation at 1100 °C for a relatively short 2 h period, a Cr 7 C 3 compound was detected beneath the α -Al 2 O 3 oxide layer on the coarse grained Cr 2 AlC, yet no Cr 7 C 3 was found in the fine grained Cr 2 AlC. The oxidation mechanism of the fine and the coarse grained Cr 2 AlC was discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. The M n+1AXn phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
2. Current Status in layered ternary Carbide Ti3SiC2, a review
3. Elastic and mechanical properties of the MAX phases10.1146/annurev-matsci-062910-100448 ↗
4. Layered machinable and electrically conductive Ti2AlC and Ti3AlC2 ceramics: a review10.1016/S1005-0302(10)60064-3 ↗
5. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
6. Recent progress in theoretical prediction, preparation, and characterization of layered ternary transition-metal carbides10.1146/annurev-matsci-082908-145340 ↗
7. The Mn+1AXn phases: materials science and thin-film processing10.1016/j.tsf.2009.07.184 ↗
8. Multiple crack healing of a Ti2AlC ceramic10.1016/j.jeurceramsoc.2012.01.017 ↗
9. Ultra-high temperature ablation of Ti2AlC ceramics under an oxyacetylene flame10.1016/j.jeurceramsoc.2010.11.035 ↗
10. Effect of temperature, strain rate and grain size on the mechanical response of Ti3SiC2 in tension10.1016/S1359-6454(01)00424-4 ↗
11. Processing and mechanical properties of Ti3SiC2. II. Effect of grain size and deformation temperature10.1111/j.1151-2916.1999.tb02167.x ↗
12. Fatigue-crack growth and fracture properties of coarse and fine-grained Ti3SiC210.1016/S1359-6462(99)00427-3 ↗
13. Effect of grain size, notch width, and testing temperature on the fracture toughness of Ti3Si(Al)C2 and Ti3AlC2 using the chevron-notched beam (CNB) method10.1016/j.jeurceramsoc.2007.07.011 ↗
14. Synthesis and mechanical properties of fully dense Ti2SC10.1111/j.1551-2916.2007.01999.x ↗
15. Mechanical properties of low temperature synthesized dense and fine grained Cr2AlC ceramics10.1016/j.jeurceramsoc.2010.08.014 ↗
16. Effect of grain size on friction and wear behavior of Ti3SiC210.1016/S0043-1648(99)00348-8 ↗
17. Tensile creep of coarse-grained (100–300μm) Ti3SiC2 in the 1000–1200°C temperature range10.1016/S0925-8388(03)00435-3 ↗
18. Tensile creep of fine-grained (3–5μm) Ti3SiC2 in the 1000–1200°C temperature range10.1016/S1359-6454(01)00243-9 ↗
19. Compressive creep of fine and coarse-grained Ti3SiC2 in air in the 1000–1200°C temperature range10.1016/j.actamat.2005.05.037 ↗
20. High-temperature oxidation and hot corrosion of Cr2AlC10.1016/j.actamat.2007.07.024 ↗
21. Oxidation behavior of Cr2AlC ceramics at 1100 and 1250°C10.1007/s10853-008-2516-2 ↗
22. Oxidation of Cr2AlC between 900 and 1200°C in air10.1007/s11085-007-9071-0 ↗
23. Cyclic oxidation of Cr2AlC between 1000 and 1300°C in air10.1016/j.jallcom.2007.10.018 ↗
24. S.B. Li, L.O. Xiao, G.M. Song, W.G. Sloof, S. van der Zwaag, Oxidation and self-healing behavior of a fine-grained Cr2AlC ceramic, Submitted for publication.
25. Synthesis and thermal stability of Cr2AlC10.1016/j.jeurceramsoc.2011.01.009 ↗
26. A first-principles investigation of the phase stability of Ti2AlC with Al vacancies10.1016/j.scriptamat.2007.09.048 ↗
27. High-temperature oxidation behavior of Ti2AlC in air10.1023/A:1023092027697 ↗
28. High temperature healing of Ti2AlC: on the origin of inhomogeneous oxide scale10.1016/j.scriptamat.2011.03.031 ↗
29. High temperature oxidation behavior of Ti2AlC ceramic at 1200°C10.3184/096034012X13348496462140 ↗
30. Multiple crack healing of a Ti2AlC ceramic10.1016/j.jeurceramsoc.2012.01.017 ↗
31. Insight into high temperature oxidation of Al2O3-forming Ti3AlC210.1016/j.corsci.2012.01.011 ↗
32. Alloy design of intermetallics for protective scale formation and for use as precursors for complex ceramic phase surfaces10.1016/j.intermet.2004.02.019 ↗