journal article·2012-04

Evaluation of mechanical reliability of zirconia-toughened alumina composites for dental implants

Dongxu Tang, Hyung-Bong Lim, Ki-Ju Lee, Chi-Hoon Lee, Won-Seung Cho

Ceramics International· Volume 38· Issue 3
Publisher page

Abstract

Abstract Zirconia-toughened alumina composites containing 0–30 vol% of 3Y-TZP were fabricated by sintering at 1600 °C for 2 h in air. The effect of the 3Y-TZP content on the mechanical properties and microstructure of the alumina ceramics was investigated. The fracture toughness and biaxial flexural strength increased as the 3Y-TZP content increased. The Young's modulus decreased with 3Y-TZP content according to the rule of mixture, while the hardness showed the contrary tendency. The Weibull modulus of the Al 2 O 3 with 20 vol% 3Y-TZP composite is higher than that of alumina. The residual hoop compressive stress developed in ZTA ceramic composites probably accounts for the enhancement of strength and fracture toughness, as well as for the higher tendency of crack deflection. No monoclinic phase and strength degradation were found after low temperature degradation (LTD) testing. The excellent LTD resistance can be explained by the increased constraining force on zirconia embedded in alumina matrix.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Mechanical properties and cytotoxicity of 3Y-TZP bioceramics reinforced with Al2O3 particles10.1016/j.ceramint.2008.02.004 ↗
2. On the wide range of mechanical properties of ZTA and ATZ based dental ceramic composite by varying the Al2O3 and ZrO2 content10.1016/j.ijrmhm.2009.06.001 ↗
3. Crack growth resistance of alumina zirconia and zirconia toughened alumina ceramics for joint prostheses10.1016/S0142-9612(01)00206-X ↗
4. Transformation toughening. Part 4. Fabrication, fracture toughness and strength of Al2O3–ZrO2 composites10.1007/BF00809060 ↗
5. Strength-toughness relations in sintered and isostatically hot-pressed ZrO2-toughened Al2O310.1111/j.1151-2916.1986.tb07401.x ↗
6. Perspective on the development of high-toughness ceramics10.1111/j.1151-2916.1990.tb06493.x ↗
7. Contributions of t–m phase transformation to the toughening of ZTA10.1111/j.1151-2916.1991.tb07166.x ↗
8. Fracture toughness of zirconia–alumina composites10.1016/S0263-4368(98)00064-X ↗
9. Zirconia-toughened alumina (ZTA) ceramics10.1007/BF02385721 ↗
10. Low-temperature ageing of zirconia-toughened alumina ceramics and its implication in biomedical implants10.1016/S0955-2219(03)00313-3 ↗
11. Powder characteristics sintering behavior and microstructure of sol–gel derived ZTA composites10.1016/S0955-2219(99)00165-X ↗
12. Mechanical properties of alumina–zirconia composites for ceramic abutments10.1590/S1516-14392004000400021 ↗
13. DIN 51109 · 1991
14. Numerical simulation of zener pinning with growing second-phase particles10.1111/j.1151-2916.1998.tb02370.x ↗
15. Hindrance of grain growth in Al2O3 by ZrO2 inclusions10.1111/j.1151-2916.1984.tb19734.x ↗
16. Effects of particle size on inhibited grain growth10.1016/0956-716X(90)90574-Z ↗
17. Rice · 1977
18. Perspective on the development of high-toughness ceramics10.1111/j.1151-2916.1990.tb06493.x ↗
19. ISO 6872.2008 (E), Third Edition, 2008-09-01.
20. Chawla · 1993
21. Strengthening contribution arising from residual stresses in Al2O3/ZrO2 composites: a piezo-spectroscopy investigation10.1016/S0955-2219(98)00195-2 ↗
22. Fracture statistics of ceramics – Weibull statistics and deviations from Weibull statistics10.1016/j.engfracmech.2006.05.028 ↗
23. On the spacing of dispersed obstacles10.1016/0001-6160(66)90185-4 ↗
24. Thermal stability of Y2O3-partially stabilized zirnonia (Y-PSZ) and Y-PSZ/Al2O3 composites10.1007/BF00720523 ↗
25. Young's modulus, flexural strength, and fracture of yttria-stabilized zirconia versus temperature10.1111/j.1151-2916.1997.tb02920.x ↗
26. William · 2007
27. Low temperature degradation of a Y-TZP dental ceramic10.1016/j.actbio.2010.09.020 ↗
28. Low temperature aging of Y-TZP ceramics10.1111/j.1151-2916.1999.tb02055.x ↗