journal article·2017-06

Interfacial structure and stability of a co-continuous SiC/Al composite prepared by vacuum-pressure infiltration

Jingbo Zhu, Fuchi Wang, Yangwei Wang, Bowen Zhang, Lu Wang

Ceramics International· Volume 43· Issue 8
Publisher page

Abstract

Abstract The interfacial structure of a SiC 3D /Al composite prepared by vacuum-pressure infiltration was investigated to determine whether interfacial reactions occur and specific orientation relationships exist between SiC and Al. The resulting SiC/Al interfaces were continuous and free of any precipitates and voids. There is no consensus for the orientation relationship between 6H-SiC and Al. In addition, the mismatch between the two phases at the interface was accommodated by mismatch dislocation. The stability of the SiC 3D /Al composite after annealing at 873 K for 10 h was determined. No Al 4 C 3 precipitated at the interface, although grain coarsening of Al occurred. Compared with the concentration gradients at the initial interfaces, those obtained at the interface after annealing were still steep, indicating that concurrent interdiffusion occurred between SiC and Al in a very narrow region near the interfaces. Theoretical calculations suggest similarly the chemical and structural stability of the SiC/Al interface during the annealing treatment.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Preparation of interpenetrating ceramic–metal composites10.1016/j.jeurceramsoc.2003.10.030 ↗
2. Preparation of C4 ceramic/metal composites by reactive metal penetration of commercial ceramics10.1016/j.compscitech.2005.04.046 ↗
3. Processing of ceramic-metal interpenetrating composites10.1016/j.jeurceramsoc.2008.07.034 ↗
4. Thermophysical properties of SiC/Al composites with three dimensional interpenetrating network structure10.1016/j.ceramint.2013.12.105 ↗
5. Friction behavior of co-continuous alumina/aluminum composites with and without SiC reinforcement10.1016/S0043-1648(01)00812-2 ↗
6. Thermal shock resistance of TiB2–Cu interpenetrating phase composites10.1016/j.compscitech.2005.02.010 ↗
7. Effects of particle size and properties on the microstructures, mechanical properties, and fracture mechanisms of 7075Al hybrid composites prepared by squeeze casting10.1007/s10853-014-8496-5 ↗
8. Co-continuous composite materials for friction and braking applications10.1007/s11837-006-0235-1 ↗
9. Thermophysical properties of SiC/Al composites with three dimensional interpenetrating network structure10.1016/j.ceramint.2013.12.105 ↗
10. High strain rate characteristics of 3-3 metal–ceramic interpenetrating composites10.1016/j.msea.2010.12.016 ↗
11. Effect of aluminum reinforcement on the dynamic fragmentation of SiC ceramics10.1016/S0734-743X(03)00034-4 ↗
12. Control of the interface in SiC/Al composites10.1016/S1359-6462(99)00227-4 ↗
13. Wettability of SiC by aluminium and Al-Si alloys10.1007/BF01160579 ↗
14. Anomalous penetration of Al into SiC10.1016/0956-7151(94)00250-L ↗
15. Diffusion of ion implanted aluminum in silicon carbide10.1063/1.444133 ↗
16. Influence of SiC surface polarity on the wettability and reactivity in an Al/SiC system10.1016/j.apsusc.2015.07.164 ↗
17. SiC-Al interface structure in squeeze cast SiCw/Al composite10.1016/0956-716X(95)00304-E ↗
18. Effects of surface-oxidation modification and heat treatment on silicon carbide 3D/AlCu5MgTi composites during vacuum-pressure infiltration10.1016/j.apsusc.2015.08.151 ↗
19. Microstructural aspects of aluminium-silicon carbide particulate composites produced by a casting method10.1016/0921-5093(89)90376-6 ↗
20. Al‒SiC interface structure studied by HREM10.1016/0956-7151(92)90287-O ↗
21. A comparison of interfacial arrangements of SiC/Al composites10.1016/0956-716X(95)00008-J ↗
22. Quantum chemical study of adhesion at the SiC/Al interface10.1063/1.342082 ↗
23. Limiting the development of Al4C3 to prevent degradation of Al/SiCp composites processed by pressureless infiltration10.1016/j.compscitech.2005.07.025 ↗
24. Kosolapova · 2012
25. Moisture effect on SiCP/6061 Al MMC: dissolution of interfacial Al4C310.1016/S1359-6462(97)00133-4 ↗
26. Interfacial structure of a SiC/Al composite10.1016/0921-5093(96)10168-4 ↗
27. Structure and mechanism of bonding at a diffusion-bonded Al/SiC interface10.1016/0956-7151(94)90276-3 ↗
28. Fiber and interface fracture in singlecrystal aluminum/SiC fiber composites10.1007/BF02646070 ↗
29. Y. Liang, Study on the Molding and Sintering Processes of Recrystallized SiC Porous Ceramic, in: School of Materials Science and Engineering, Master of Engineering, Beijing Institute of Technology, Beijing, 2015.
30. Effect of ductile agents on the dynamic behavior of SiC3D network composites10.1007/s10443-016-9497-0 ↗
31. The effect of surface oxidized modification on the mechanical properties of SiC3D/Al10.1016/j.apsusc.2015.01.205 ↗
32. Fine Ceramics (Advanced Ceramics, Advanced Technical Ceramics)-Determination of Density and Apparent Porosity, in: I.O.f. Standardization (Ed.), ISO 18754, 2003.
33. Test method for compressive strength of fine ceramics (advanced ceramics, advanced technial ceramics), in: C.N. Standards (Ed.), GB/T 8489, 2006.
34. Fine ceramics (advanced ceramics, advanced technial ceramics)-Test method for flexural strength of monolithic ceramics at room temperature, International Organization for Standardization, in: I.O.f. Standardization (Ed.), ISO 14704, 2000.
35. Cai · 2009
36. Diffusion of ion implanted aluminum in silicon carbide10.1063/1.444133 ↗
38. Nanocrystalline eutectic Al–Si alloy produced by cryomilling10.1016/j.msea.2008.12.017 ↗
39. Compatibility of carbon filaments with a carbide coating and an aluminum matrix10.1007/BF00779433 ↗
40. Interfacial reactions between SiC and aluminium during joining10.1007/BF00563067 ↗