Abstract

Magnesium oxide (MgO) presents excellent refractoriness and high resistance to basic slag. However, in the presence of water, MgO undergoes an expansive hydration reaction generating Mg(OH)2, which can lead to swelling and cracking. In this work, additives called chelants were added to dead burnt magnesia suspensions in order to check their effectiveness as inhibitors of the magnesium oxide hydration. Zeta potential, ionic conductivity, pH and temperature measurements were used to provide information related to the magnesia surface and the chelant adsorption. Assessment of the hydration degree and volumetric expansion provided indications of the amount of Mg(OH)2 formed, as well as its likelihood to damage the ceramic bodies. The results showed that citric acid can inhibit hydration to some extent, whereas ethylenediamine tetraacetic acid (EDTA) was more effective in preventing volume expansion. An addition of 0.3 wt% of these chelants was sufficient to prevent hydration and avoid expansion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Layered Double Hydroxides Synthesis and Applications · Magnesium Oxide Properties and Applications · Holomorphic and Operator Theory

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Hydration characteristics of magnesia
2. A novel approach for magnesia hydration assessment in refractory castables10.1016/j.ceramint.2006.01.004 ↗
3. Spinel forming castables: physical and chemical mechanisms during drying
4. Ceramic hydration with expansion: the structure and reaction of water layers on magnesium oxide. A cyclic cluster study
5. Magnesia sinter hydration–dehydration behavior in refractory castables10.1016/j.ceramint.2007.06.009 ↗
6. Dissolution and hydration kinetics of MgO10.1016/0376-4583(85)90080-9 ↗
7. The role of reactivity in syntheses and the properties of magnesium oxide10.1016/S0167-2738(97)00364-0 ↗
8. On the kinetics of magnesia hydration in magnesium acetate solutions10.1002/(SICI)1097-4660(199904)74:4<322::AID-JCTB35>3.0.CO;2-L ↗
9. The effect of magnesite calcinations conditions on magnesia hydration10.1016/S0892-6875(00)00146-1 ↗
10. Kinetics and mechanistic analysis of caustic magnesia hydration10.1002/jctb.1038 ↗
11. G. Huazhi, J. Ouyang, H. Wang, W. Zhang, J. Sun, C. Lu, Y. Hong, The hydration resistance of CaO–MgO clinker treated by H2C2O4 solution. in: Proceedings of UNITECR 2003, Technical Association of Refractories (TARJ), Osaka, Japan, 2003.
12. Improved hydration resistance of synthesized magnesia–calcia clinker by surface modification10.1111/j.1151-2916.2004.tb07485.x ↗
13. Microsilica addition as an antihydration technique for magnesia-containing refractory castables
14. The role of hydraulic binders on magnesia containing refractory castables: calcium aluminate cement and hydratable alumina10.1016/j.ceramint.2009.04.023 ↗
15. Temperature and common-ion effect on magnesium oxide (MgO) hydration10.1016/j.ceramint.2009.12.009 ↗
16. Mechanisms of reaction of hydratable aluminas10.1111/j.1551-2916.1999.tb20085.x ↗
17. Yatsimirskii · 1960