Abstract

Abstract In this research, a Copper-based composite was fabricated by TiC reinforcement via friction stir processing. Holes with the diameter and depth of 2 mm were made on the surface of a pure copper specimen and filled by TiC powders. Friction srir processing was carried out with transverse and rotational speeds of 50 mm/min and 1000 rpm, respectively. Optical and scanning electron microscope observations revealed that FSP produced a fine grain microstructure with a homogeneous distribution of particles on the surface. Reinforcing particles showed a good bonding with the base metal. Mechanical test results also proved that FSP increased the microhardness and the wear resistance of specimen as a result of grain refinement and the existence of TiC particles in the FSP zone. Maximum hardness in the stir zone was 117 Vickers, while the hardness of pure copper was 65 Vickers. X-Ray analysis proved no intermetallic compounds in the stir zone.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. On the role of processing parameters in producing Cu/SiC metal matrix composites via friction stir processing: investigating microstructure, microhardness, wear and tensile behavior10.1016/j.matchar.2010.11.005 ↗
2. Microstructure, properties and wear behaviors of (Ni3Al)p reinforced Cu matrix composites10.1016/S1005-0302(11)60167-9 ↗
3. The influence of technological process on dry sliding wear behaviour of titanium carbide reinforcement copper matrix composites10.2320/matertrans.M2010270 ↗
4. Characterization of boron carbide particulate reinforced in situ copper surface composites synthesized using friction stir processing10.1016/j.matchar.2013.07.001 ↗
5. Wear transitions in particulate reinforced copper matrix composites10.2320/matertrans.45.2332 ↗
6. Friction stir processing: a novel technique for fabrication of surface composite10.1016/S0921-5093(02)00199-5 ↗
7. Microscopic and spectroscopic analyses of TiC powder synthesized by thermal plasma technique10.1016/j.powtec.2013.01.018 ↗
8. High strain rate superplasticity in a friction stir processed 7075 Al alloy10.1016/S1359-6462(99)00329-2 ↗
9. The microstructure and mechanical properties of TiC and TiB2-reinforced cast metal matrix composites10.1023/A:1004519306186 ↗
10. Plasma transferred arc surface alloying of a construction steel to produce a metal matrix composite tool steel with TiC as reinforcing particles10.1016/S0257-8972(02)00744-2 ↗
11. Weldability of metal matrix composite plates by friction stir weldin at low welding parameters
12. Preparation of ultrafine TiC±Ni cermet powders by mechanical alloying10.1016/S0924-0136(00)00529-X ↗
13. Formation of metal matrix composite layer on aluminum alloy with TiC–Cu powder by laser surface alloying process10.1016/S0257-8972(01)01172-0 ↗
14. Friction stir processing of particle reinforced composite materials10.3390/ma3010329 ↗
15. A novel way to produce bulk SiCp reinforced aluminum metal matrix composites by friction stir processing10.1016/j.jmatprotec.2008.05.001 ↗
16. Characterization of the effects of friction stir processing on microstructural changes in DRA composites10.1016/j.msea.2006.04.106 ↗
17. Effect of tool pin profile on microstructure and mechanical properties of friction stir welded pure copper joints10.1016/j.matdes.2012.09.010 ↗
18. Microstructure and mechanical properties of steel/TiC nano-composite surface layer produced by friction stir processing10.1016/j.surfcoat.2012.08.005 ↗
19. Mg based nano-composites fabricated by friction stir processing10.1016/j.scriptamat.2005.11.056 ↗
20. Friction stir processing for enhancement of wear resistance of ZM21 magnesium alloy10.1007/s12666-012-0163-4 ↗
21. Effect of friction stir processing with SiC particles on microstructure and hardness of AZ3110.1016/j.msea.2006.06.089 ↗
22. Characterization of boron carbide particulate reinforced in situ copper surface composites synthesized using friction stir processing10.1016/j.matchar.2013.07.001 ↗
23. Friction and wear performance of copper–graphite surface composites fabricated by friction stir processing (FSP)10.1016/j.wear.2013.04.023 ↗
24. The microstructure and mechanical properties of an Al–CuO insitu composite produced using friction stir processing10.1016/j.matlet.2012.09.028 ↗
25. Mishra · 2011
26. Investigation of mechanical properties of Cu/SiC composite fabricated by FSP: effect of SiC particles׳ size and volume fraction10.1016/j.msea.2010.11.006 ↗
27. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
28. Recent advances in friction-stir welding – process, weldment structure and properties10.1016/j.pmatsci.2008.05.001 ↗
29. Investigating effects of process parameters on microstructural and mechanical properties of Al5052/SiC metal matrix composite fabricated via friction stir processing10.1016/j.matdes.2011.09.035 ↗
30. Fabrication of in situ Cu/SiC composites using multi-pass friction stir processing: evaluation of microstructural, porosity, mechanical and electrical behavior10.1016/j.compositesa.2011.06.010 ↗
31. Microstructure and sliding wear behavior of AA6360/(TiC+B4C) hybrid surface composite layer synthesized by friction stir processing on aluminum substrate10.1016/j.msea.2012.05.049 ↗
32. The challenge of ceramic/metal microcomposites and nanocomposites10.1016/j.pmatsci.2006.09.003 ↗
33. Effect of friction stir processing (FSP) on microstructure and properties of Al–TiC in situ composite10.1016/j.msea.2011.02.085 ↗
34. Effects of SiC particle size and process parameters on the microstructure and hardness of AZ91/SiC composite layer fabricated by FSP10.1007/s11665-011-9855-x ↗
35. Microstructure and mechanical properties of Cu/SiC metal matrix composite fabricated via friction stir processing10.1016/j.matdes.2013.08.107 ↗