Wear resistance of hybrid self-lubricating composites containing MoS2/WS2 and CaF2/BaF2
Source abstract
Abstract
: Powder metallurgy was used to produce hybrid self-lubricating nickel composites containing a different content of MoS 2 /WS 2 and CaF 2 /BaF 2 . The wear properties of the hybrid self-lubricating composites were investigated in temperatures up to 600°C. During the wear process, the samples were coated with a tribofilm, which caused a decrease in the coefficient of friction and improved the tribological properties of the samples. The properties of the tribofilm depended on the content of the high-and moderate-temperature solid lubricant. The presence of the tribofilm caused an improvement in the tribological properties of the samples and it was confirmed by the EDS and XPS techniques. The tribofilm protected the friction pair against oxidation wear, which was clearly seen during the investigation of the third body.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Tribology and Wear Analysis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Effect of Fe on the high-temperature tribological behavior of NiAl/WC-Fexself-lubricating composites produced by thermal explosion10.1088/2053-1591/aba5cf ↗
2. Diamond-like/graphite-like carbon composite films deposited by high-power impulse magnetron sputtering10.1016/j.diamond.2020.107818 ↗
3. Synthesis, microstructural and mechanical properties of self-lubricating Mo-Se-C coatings deposited by closed-field unbalanced magnetron sputtering10.1016/j.surfcoat.2020.125889 ↗
4. Synthesis, microstructure and mechanical properties of W–S–C self-lubricant thin films deposited by magnetron sputtering10.1016/j.triboint.2020.106363 ↗
5. Tribological properties of powder metallurgy - processed aluminium self lubricating hybrid composites with SiC additions10.1016/j.matdes.2012.09.015 ↗
6. Effect of counterbody on friction and wear properties of copper-MgP-graphite composites prepared by powder metallurgy
7. Effect of CaF2 surface layers on the friction behavior of copper-based composite10.1007/s11106-012-9441-2 ↗
8. Self-lubricating surface layers produced using laser alloying of bearing steel10.1016/j.wear.2017.01.102 ↗
9. Wear behavior of self-lubricating boride layers produced on Inconel 600-alloy by laser alloying
10. Self-lubricating laser claddings for reducing friction and wear from room temperature to 600 °C10.1016/j.wear.2018.05.001 ↗
11. Microstructure and wear properties of self-lubricating MoS2/Ni coating by laser cladding
12. Wear behaviors of TiN/WS2 + hBN/NiCrBSi self-lubricating composite coatings on TC4 alloy by laser cladding10.3390/coatings11010001 ↗
13. Laser cladding of Co-based alloy/TiC/CaF2 self-lubricating composite coatings on copper for continuous casting mold10.1016/j.surfcoat.2013.05.036 ↗
14. Effect of TiB 2 content on properties of nickel-coated graphite self-lubricating coating prepared by laser cladding10.3390/coatings11121501 ↗
15. Effects of aging treatment on microstructure and tribological properties of nickel-based high-temperature self-lubrication wear resistant composite coatings by laser cladding10.1016/j.matchemphys.2013.09.043 ↗
16. Development and characterization of composite Ni-Cr-C-CaF2 laser cladding on γ-TiAl intermetallic alloy10.1016/j.jallcom.2008.03.020 ↗
17. Influence of service temperature on tribological characteristics of self-lubricant coatings: a review10.1007/s11706-013-0190-z ↗
18. Friction and wear behavior of PTFE coatings modified with poly (methyl methacrylate)10.1016/j.compositesb.2019.04.047 ↗
19. Tribological properties of spark-plasma-sintered ZrO2(Y 2O3)-CaF2-Ag composites at elevated temperatures10.1016/j.wear.2004.10.007 ↗
20. Wear mechanism of Ag as solid lubricant for wide range temperature application in micro-beam plasma cladded Ni60 coatings10.1016/j.triboint.2021.107402 ↗
21. Phase analysis and microstructure study of sintered Ni-Cr composites containing MoS2, Ag and CaF2 additives as solid lubricants10.15282/jmes.14.2.2020.02.0514 ↗
22. Wear mechanism of Ag as solid lubricant for wide range temperature application in micro-beam plasma cladded Ni60 coatings10.1016/j.triboint.2021.107402 ↗
23. Tailoring self-lubricating, wear-resistance, anticorrosion and antifouling properties of Ti/(Cu, MoS2)-DLC coating in marine environment by controlling the content of Cu dopant10.1016/j.triboint.2019.106029 ↗
24. Structural design of MoS2-based coatings toward high humidity and wide temperature10.1007/s10853-019-03754-8 ↗
25. Solid lubrication with MoS2: a review10.3390/lubricants7070057 ↗
26. Tribological behavior of a Ni-WS2 composite coating across wide temperature ranges10.1007/s12598-018-1152-5 ↗
27. Study on the effectiveness of WS2 and CaF2 on the performances of self-lubricating micro impregnated diamond bits10.1016/j.ijrmhm.2019.105021 ↗
28. Microstructure and properties of HVOF sprayed Ni-based submicron WS2/CaF2 self-lubricating composite coating10.1016/S1003-6326(08)60233-2 ↗
29. Synthesis and tribological properties of WS2/MoS2 micro-nano composite lubricant10.1016/j.triboint.2025.110506 ↗
30. A novel design by constructing MoS2/WS2 multilayer film doped with tantalum toward superior friction performance in multiple environment10.1007/s10853-021-06217-1 ↗
31. The mechanism of wear reduction in the Ni-CaF2 composite material: Raman and confocal microscopy insights10.3390/ma15165501 ↗
32. Dry sliding wear behavior of Al2O3-TiC ceramic composites added with solid lubricant CaF2 by cold pressing and sintering10.1080/10402004.2014.962206 ↗
33. Wear behavior and self tribofilm formation of hot-pressed Al2O3/TiC/CaF2 ceramic composites sliding against cemented carbide10.1016/j.ceramint.2005.09.008 ↗
34. Structure design of Al2O3/TiC/CaF2 multicomponent gradient self-lubricating ceramic composite and its tribological behaviors10.1016/j.ceramint.2017.12.199 ↗
35. Effect of TiO2 nanoparticles on the tribological properties of lubricating oil: an experimental investigation10.1038/s41598-022-09245-2 ↗
36. Tribological properties of TiAl matrix self-lubricating composites incorporated with tungsten disulfide and zinc oxide10.1039/C5RA04420K ↗
37. Microstructure and tribological properties of ZrO2(Y2O3) matrix composites doped with different solid lubricants from room temperature to 800 °C10.1016/j.wear.2008.11.017 ↗
38. Tribological performance of TiAl matrix self-lubricating composites containing Ag, Ti3SiC2 and BaF2/CaF2 tested from room temperature to 600°C10.1016/j.matdes.2013.07.053 ↗
39. Low humidity-sensitivity of MoS2/Pb nanocomposite coatings10.1016/j.wear.2015.12.008 ↗
40. Effect of coating prepared using CuNiIn mixed with graphite and MoS2 on fretting wear behaviour of Ti6Al4V10.1016/j.matlet.2022.132816 ↗
41. High-temperature tribological properties of Al2O3, Ni-20 mass% Cr and NiAl spark-plasma-sintered composites containing BaF 2-CaF2 phase10.1016/j.wear.2004.12.019 ↗
42. Friction coefficient study of nanocomposite Al2O3–NbC obtained by spark plasma sintering-SPS10.1108/ILT-08-2019-0356 ↗
43. Microstructural evolution and wear mechanism of Ti3AlC2 – Ti2AlC dual MAX phase composite consolidated by spark plasma sintering (SPS)
44. The mechanism of wear reduction in the Ni-CaF2 composite material: Raman and confocal microscopy insights10.3390/ma15165501 ↗
45. The influence of solid lubricant on tribological properties of sintered Ni–20%CaF2 composite material10.1016/j.ceramint.2019.05.262 ↗