journal article·2025-09

Synergistic enhancement on mechanical and cutting performances of Ti(C, N)-based cermets by tailoring raw WC particle size

Wen-Liang Jin, Sheng-Jian Zhou, Jia-Hao Li, Chen-Guang Xu, Jia-Hu Ouyang, Yu-Jin Wang, Lei Chen

Ceramics International· Volume 51· Issue 23
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Abrasion and erosion resistance of cermets: a review
2. The effect of Co particle structures on the mechanical properties and microstructure of TiCN-based cermets10.1016/j.msea.2016.08.050 ↗
3. Development of TiCN-based cermets: mechanical properties and wear mechanism10.1016/j.ijrmhm.2012.07.001 ↗
4. A critical review of high-temperature tribology and cutting performance of cermet and ceramic tool materials10.3390/lubricants11030122 ↗
5. Cutting performance and wear mechanism of submicron and ultrafine Ti(C, N)-based cermets10.1016/j.ceramint.2024.08.391 ↗
6. Effect of WC content on the microstructure and mechanical properties of Ti (C,N)-based cermets fabricated by in situ carbothermal reduction of TiO210.1016/j.msea.2019.138024 ↗
7. Physical properties and microstructure of Ti(CN)-based cermets with different WC particle size10.1016/j.msea.2014.06.115 ↗
8. Influence of WC addition on mechanical properties of (HfNbTaZrTiMo)C-Co cermet10.1111/ijac.14619 ↗
9. Effect of Mo addition mode on the microstructure and mechanical properties of TiC-high Mn steel cermets10.1016/j.ceramint.2019.11.023 ↗
10. The effects of Mo2C additions on the sintering response of TiC0.3N0.7-Ni3Al cermets10.1016/j.ijrmhm.2016.08.013 ↗
11. Influence of TaC content on microstructure and mechanical performance of Ti(C,N)-based cermets fabricated by mechanical activation and subsequent in situ carbothermal reduction10.1016/j.ceramint.2021.10.166 ↗
12. Effect of TaC addition on the microstructures and mechanical properties of Ti(C, N)-based cermets10.1016/j.matdes.2010.01.047 ↗
13. Insights into hardening and strengthening in ultrafine Ti(C, N)-based cermets10.1016/j.jallcom.2024.174843 ↗
14. Effect of Nb on microstructure and tribological properties of Ti(C, N)-based cermet10.1016/j.ijrmhm.2024.106958 ↗
15. Effect of Ta, Nb and Zr additions on the microstructures and mechanical properties of 70 vol% TiC/Al cermets10.1016/j.ceramint.2022.07.194 ↗
16. Effect of NbC on the microstructure, mechanical properties, and oxidation resistance of Ti(C,N)-based cermets10.3139/146.111907 ↗
17. Effects of VC additive on cutting compatibility of TiB2-based cermet cutting tools and Ti6Al4V alloy10.1007/s00170-022-09010-9 ↗
18. Effect of VC additions on the microstructure and mechanical properties of TiC-based cermets10.1088/2053-1591/abc2a1 ↗
19. Effect of VC addition on the microstructure and properties of Ti(C,N)-based nano cermets10.1007/s12598-011-0433-z ↗
20. Ti(C,N)-Based cermets: critical review of achievements and recent developments
21. Carbide/binder interfaces in Ti(CN)-(Ti, W)C/(Ti, W)(CN)-based cermets10.1016/j.jallcom.2015.10.121 ↗
22. Effect of submicron Ti(C,N) on the microstructure and the mechanical properties of Ti(C,N)-based cermets10.1016/j.ijrmhm.2011.05.007 ↗
23. Fracture behaviors of Ti(C, N)-based cermets with different contents of metal binder10.1016/j.ceramint.2022.07.183 ↗
24. Enhancement effects of FeCoNiCrMn high-entropy alloy doping on the Ti(C, N)-based cermets: microstructure and mechanical properties10.1016/j.ijrmhm.2024.106695 ↗
25. High-entropy alloys as an alternative binder to improve mechanical, tribological, and oxidation properties of cermets10.1016/j.matdes.2024.113431 ↗
26. TiCN cermets with MnFeCoNiCu High Entropy alloy binder
27. Fabrication and properties of Ti(C,N)-based cermets with multi-component AlCoCrFeNi high-entropy alloys binder10.1016/j.matlet.2013.08.087 ↗
28. TiC whisker reinforced ultra-fine TiC-based cermets: microstructure and mechanical properties10.1016/j.ceramint.2016.01.069 ↗
29. Effect of SiC nano-whisker addition on TiCN-based cermets prepared by spark plasma sintering10.1016/j.ijrmhm.2012.03.008 ↗
30. Effect of SiC whisker addition on the microstructures and mechanical properties of Ti(C, N)-based cermets10.1016/j.matdes.2010.07.028 ↗
31. High-performance Ti(C,N)-based cermet with ZrO2 whiskers and Al0.3CoCrFeNi high-entropy alloy10.1016/j.ijrmhm.2022.105990 ↗
32. Properties of Ti(C,N)-based cermets reinforced with ZrO2 whiskers deposited via sulfate flux at high temperatures10.1016/j.vacuum.2021.110336 ↗
33. Effect of ZrO2 whiskers on the microstructure and mechanical properties of a Ti(C,N)-based cermet cutting tool material10.1111/ijac.13186 ↗
34. Preparation of a highly toughened (Ti,W)C-20Ni cermet through in situ formation of solid solution and WC whiskers10.1016/j.ceramint.2014.11.031 ↗
35. Microstructure and mechanical properties of (Ti,W)C-Ni cermet prepared using a nano-sized TiC-WC powder mixture10.1016/j.jallcom.2015.03.115 ↗
36. Evolution of microstructure and interfacial characteristics of complete solid-solution Ti(C,N)-based cermets fabricated by mechanical activation and subsequent in situ carbothermal reduction10.1016/j.ceramint.2021.02.251 ↗
37. The fabrication of multi-core structure cermets based on (Ti,W,Ta)CN and TiCN solid-solution powders10.1016/j.ijrmhm.2016.09.011 ↗
38. Enhancing mechanical properties of Ti(C, N)-based cermets via preparation with (Ti, W)(C, N) multi-component powder10.1016/j.ijrmhm.2022.105931 ↗
39. Effect of nano-TiB2 addition on the microstructure, mechanical properties and machining performance of TiCN cermet10.1007/s41779-018-0185-4 ↗
40. Mechanical properties and microstructures of TiCN/nano-TiB2/TiN cermets prepared by spark plasma sintering10.1016/j.ceramint.2018.02.154 ↗
41. Effects of nano-Al2O3 addition on microstructure, mechanical properties, and wear resistance of Ti(C, N)-based cermets10.1016/j.ijrmhm.2023.106290 ↗
42. TiC0.5N0.5-Based cermets with varied amounts of Si3N4 nanopowders prepared by spark plasma sintering10.1155/2015/626429 ↗
43. Effect of Si3N4 additive on microstructure and mechanical properties of Ti(C, N)-Based cermet cutting tools10.3390/ma17112586 ↗
44. Influences of ultrafine Ti(C, N) additions on microstructure and properties of micron Ti(C,N)-based cermets10.1016/j.matchemphys.2019.03.066 ↗
45. Effect of TiC/TiN powder size on microstructure and properties of Ti(C, N)-based cermets10.1016/j.msea.2006.10.003 ↗
46. Microstructural evolution and formation mechanism of liquid exudation induced surface metal capping on Ti(C, N)-based cermets10.1016/j.ijrmhm.2024.106679 ↗
47. Grain growth behavior in TaC-modified ultrafine Ti(C, N)-based cermets10.1016/j.ijrmhm.2024.106625 ↗
48. Enhanced densification of ultrafine Ti(C, N)-based cermets based on grain-growth induced liquid-phase pore filling mechanism10.1016/j.jallcom.2024.174141 ↗
49. Effect of WC content on the microstructures and corrosion behavior of Ti(C, N)-based cermets10.1016/j.ceramint.2012.06.055 ↗
50. Macro-gradient structures generated in Ti(C, N)-based cermets with supersaturated WC: an experimental and thermodynamic investigation10.1080/21663831.2022.2131371 ↗
51. Electron work function guided tailoring of (W4-x, Mx)C4/doped Ni matrix interfacial bonding: insights from first-principles calculations10.1016/j.actamat.2024.120511 ↗
52. Interfacial bonding between iron and Mo- and Cr-doped tungsten carbides10.1063/5.0134620 ↗
53. Work of adhesion analysis for metal-substituted W4C4 carbides in a cobalt matrix
54. Effects of WC content on core/rim phases and microstructure of TiB2-TiC-WC-(Co-Ni) cermets
55. Structures and properties of TiAlCrN coatings deposited on Ti(C,N)-based cermets with various WC contents10.1016/j.ijrmhm.2017.08.020 ↗
56. Effect of WC content on the microstructure and mechanical properties of Ti(C0.5N0.5)-WC-Mo-Ni cermets10.1016/j.ijrmhm.2009.10.005 ↗
57. Effect of WC content on the microstructure and mechanical properties of (Ti, W)(C, N)-Co cermets10.1016/j.ijrmhm.2007.01.003 ↗
58. Effect of W content in solid solution on properties and microstructure of (Ti,W)C-N3Al cermets10.1016/j.jallcom.2016.03.073 ↗
59. High-temperature compression tests of Ti(C, N)-70 wt% W cermet and isothermal forging of Inconel 718 alloys using cermet molds10.1016/j.jmrt.2023.04.237 ↗
60. Peters
61. Semi-empirical relationship between the hardness, grain size and mean free path of WC-Co10.1016/S0263-4368(01)00022-1 ↗