Fe2O3 solubility and structural investigation in simulated high-level liquid waste vitrified Na2O-TiO2-Fe2O3 -B2O3-SiO2 glass system
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Glass properties and applications · Pigment Synthesis and Properties · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. M.I. Ojovan, Vitrification as a key solution for immobilisation within nuclear Waste Manag., (n.d.). https://doi.org/10.1007/s13369-024-09292-z.10.1007/s13369-024-09292-z ↗
2. V.I. Malkovsky, S. V Yudintsev, M.I. Ojovan, V.A. Petrov, The influence of radiation on confinement properties of nuclear waste glasses, 2020 (n.d.) 1–14. https://doi.org/10.1155/2020/8875723.10.1155/2020/8875723 ↗
3. S. Manohar, G. Sugilal, R.K. Bajpai, C.P. Kaushik, K. Raj, Radioactive waste management, in: B.S. Tomar, P.R.V. Rao, S.B. Roy, J.P. Panakkal, K. Raj, A.N. Nandakumar (Eds.), Nuclear Fuel Cycle, Springer Nature Singapore, n.d.: pp. 255–331. https://doi.org/10.1007/978-981-99-0949-0_8.10.1007/978-981-99-0949-0_8 ↗
4. J.S. McCloy, B.J. Riley, M.C. Dixon Wilkins, J.S. Evarts, J. Bussey, J.D. Vienna, P.A. Bingham, D.J. Gregg, M. Ojovan, S. Schuller, K. Uruga, D. Perret, E. Regnier, I. Giboire, W. Um, K. Xu, A. Goel, A.A. Kruger, International perspectives on glass waste form development for low-level and intermediate-level radioactive waste, 80 (n.d.) 594–618. https://doi.org/10.1016/j.mattod.2024.08.025.10.1016/j.mattod.2024.08.025 ↗
5. 1992
6. J. Selvakumar, S. Rajasekaran, S. Chitra, B. Paul, Simulated studies on optimization and characterization of feed and product of melter for safe disposal of high-level radioactive liquid waste, 118 (n.d.) 103135. https://doi.org/10.1016/j.pnucene.2019.103135.10.1016/j.pnucene.2019.103135 ↗
7. Glass matrices for vitrification of radioactive waste – an update on R & D efforts10.1088/1757-899X/2/1/012002 ↗
8. A. Goel, J.S. McCloy, R. Pokorny, A.A. Kruger, Challenges with vitrification of hanford high-level waste (HLW) to borosilicate glass – an overview, 4 (n.d.) 100033. https://doi.org/10.1016/j.nocx.2019.100033.10.1016/j.nocx.2019.100033 ↗
9. Role of Ba(NO3) pretreatment in reducing the yellow phase formation during vitrification of nuclear waste10.1016/j.jnucmat.2021.153121 ↗
10. M.I. Ojovan, W.E. Lee, S.N. Kalmykov, Nuclear waste types and sources, in: An Introduction to Nuclear Waste Immobilisation, Elsevier, n.d.: pp. 119–143. https://doi.org/10.1016/B978-0-08-102702-8.00010-8.10.1016/B978-0-08-102702-8.00010-8 ↗
11. P. Hrma, B.J. Riley, J. V Crum, J. Matyas, The effect of high-level waste glass composition on spinel liquidus temperature, 384 (n.d.) 32–40. https://doi.org/10.1016/j.jnoncrysol.2013.02.014.10.1016/j.jnoncrysol.2013.02.014 ↗
12. J.G. Reynolds, Spinel Structure and Liquidus Temperature Relationships in Nuclear Waste Glass, vol. 40 (n.d.) 3987–3991. https://doi.org/10.1007/s10853-005-2007-7.10.1007/s10853-005-2007-7 ↗
13. M. Jiricka, P. Hrma, J.D. Vienna, The Effect of Composition on Spinel Crystals Equilibrium in low-silica high-level Waste Glasses, vol. 319 (n.d.) 280–288. https://doi.org/10.1016/S0022-3093(03)00010-3.10.1016/S0022-3093(03)00010-3 ↗
14. A. Deshkar, M. Ahmadzadeh, A. Scrimshire, E. Han, P.A. Bingham, D. Guillen, J. McCloy, A. Goel, Crystallization Behavior of Iron‐ and Boron‐Containing Nepheline (Na_2 O·Al_2 O_3 ·2Sio_2) Based Model High‐Level Nuclear Waste Glasses, vol. 102 (n.d.) 1101–1121. https://doi.org/10.1111/jace.15936.10.1111/jace.15936 ↗
15. M. Ahmadzadeh, J. Marcial, J. McCloy, Crystallization of Iron‐Containing Sodium Aluminosilicate Glasses in the NaAlSiO_4 ‐Nafesio_4 Join, vol. 122 (n.d.) 2504–2524. https://doi.org/10.1002/2016JB013661.10.1002/2016JB013661 ↗
16. J. Marcial, J. Kabel, M. Saleh, N. Washton, Y. Shaharyar, A. Goel, J.S. McCloy, Structural Dependence of Crystallization in Glasses Along the Nepheline (Naalsio_4) ‐ Eucryptite (Lialsio_4) Join, vol. 101 (n.d.) 2840–2855. https://doi.org/10.1111/jace.15439.10.1111/jace.15439 ↗
17. Manaktala
18. P. Hrma, Crystallization During Processing of Nuclear Waste Glass, vol. 356 (n.d.) 3019–3025. https://doi.org/10.1016/j.jnoncrysol.2010.03.039.10.1016/j.jnoncrysol.2010.03.039 ↗
19. R. Pokorny, P. Hrma, Model for the Conversion of Nuclear Waste Melter Feed to Glass, vol. 445 (n.d.) 190–199. https://doi.org/10.1016/j.jnucmat.2013.11.009.10.1016/j.jnucmat.2013.11.009 ↗
20. P. Fauvet, Corrosion issues in nuclear fuel reprocessing plants, in: Nuclear Corrosion Science and Engineering, Elsevier, n.d.: pp. 679–728. https://doi.org/10.1533/9780857095343.5.679.10.1533/9780857095343.5.679 ↗
21. G. Shit, S. Ningshen, Effect of Metallic Redox Ions on the Corrosion Behavior of GTAW Weldment of Type 304L Stainless Steel in Simulated Non-radioactive PUREX and HLLW Medium, vol. 168 (n.d.) 105039. https://doi.org/10.1016/j.pnucene.2023.105039.10.1016/j.pnucene.2023.105039 ↗
22. P. Fauvet, F. Balbaud, R. Robin, Q.-T. Tran, A. Mugnier, D. Espinoux, Corrosion Mechanisms of Austenitic Stainless Steels in Nitric Media Used in Reprocessing Plants, vol. 375 (n.d.) 52–64. https://doi.org/10.1016/j.jnucmat.2007.10.017.10.1016/j.jnucmat.2007.10.017 ↗
23. G. Suneel, C.P. Kaushik, P.M. SatyaSai, J.K. Gayen, K. V Ravi, Remote start-up of Joule Heated Ceramic Melter – Optimization of Design Parameters Based on Experimental and Numerical Investigations, vol. 57 (n.d.) 243–252. https://doi.org/10.1080/00223131.2019.1667922.10.1080/00223131.2019.1667922 ↗
24. J. Selvakumar, S. Maity, G. Suneel, S. Srinivasan, N.R. Jawahar, J.K. Gayen, Assessment of SiO2-B2O3-Na2O-TiO2-Fe2O3 glass system for the vitrification of high-level acidic radioactive liquid waste, in: A.R. Molla, A. Kalyandurg, J.M. Parker (Eds.), Advances in Glass and Glass-Ceramics, Springer Nature Singapore, n.d.: pp. 1–12. https://doi.org/10.1007/978-981-97-2969-2_1.10.1007/978-981-97-2969-2_1 ↗
25. Cassingham J. Nathan; Bingham A. Paul; Hand J. Russell; Forder D. Sue, Property modification of a high level nuclear waste borosilicate glass through the addition of Fe2O3, 49 (n.d.) 21–26. https://www.ingentaconnect.com/contentone/sgt/gta/2008/00000049/00000001/art00004.
26. M.I. Ojovan, W.E. Lee, S.N. Kalmykov, Immobilisation of radioactive wastes in glass, in: An Introduction to Nuclear Waste Immobilisation, Elsevier, n.d.: pp. 319–368. https://doi.org/10.1016/B978-0-08-102702-8.00019-4.10.1016/B978-0-08-102702-8.00019-4 ↗
27. N.O. Dantas, W.E.F. Ayta, A.C.A. Silva, N.F. Cano, S.W. Silva, P.C. Morais, Effect of Fe2O3 Concentration on the Structure of the SiO2–Na2O–Al2O3–B2O3 Glass System, vol. 81 (n.d.) 140–143. https://doi.org/10.1016/j.saa.2011.05.074.10.1016/j.saa.2011.05.074 ↗
28. Infrared studies of Na2O–B2O3–SiO2 and Al2O3–Na2O–B2O3–SiO2 glasses10.1016/S0921-4526(02)01547-8 ↗
29. The influence of local structure and surface morphology on the antibacterial activity of silver-containing calcium borosilicate glasses10.1016/j.jnoncrysol.2014.08.004 ↗
30. On the connectivity of borate tetrahedra in borate and borosilicate glasses
31. Structural, dielectric, and optical properties of yttrium calcium borate glasses10.1063/1.3115796 ↗
32. Characterization of novel CeO2–B2O3 glasses, structure and properties10.1016/S0921-4526(00)00593-7 ↗
33. Zinc borate glasses: properties, structure and modelling of the composition-dependence of borate speciation10.1039/D2CP05517A ↗
34. Structure of CaO–B2O3–SiO2–TiO2 glasses: a raman spectral study10.2355/isijinternational.51.1021 ↗
35. Fe-oxidation state in alkali-trisilicate glasses - a Raman spectroscopic study10.1016/j.jnoncrysol.2017.04.033 ↗
36. Effect of Fe2O3 concentration on the structure of the SiO2–Na2O–Al2O3–B2O3 glass system10.1016/j.saa.2011.05.074 ↗
37. Thermo-physical behavior of borosilicate glasses in the presence of high-level radioactive liquid waste constituents10.1007/s10973-019-09130-7 ↗
38. Non-isothermal crystallization kinetic studies on MgO–Al2O3–SiO2–TiO2 glass10.1016/j.jnoncrysol.2007.04.008 ↗
39. The effect of TiO2 addition on the crystallization and phase formation in lithium aluminum silicate (LAS) glasses nucleated by P2O510.1016/j.jpcs.2008.06.003 ↗
40. Effect of different additions on the crystallization behavior and magnetic properties of magnetic glass–ceramic in the system Fe2O3–ZnO–CaO–SiO210.1016/j.jare.2011.07.001 ↗
41. Preparation and characterization of some ferromagnetic glass–ceramics contains high quantity of magnetite10.1016/j.ceramint.2008.08.021 ↗
42. Devitrification of defense nuclear waste glasses: role of melt insolubles10.1016/0022-3093(86)90789-1 ↗
43. Structure of NaFeSiO4, NaFeSi2O6, and NaFeSi3O8 glasses and glass-ceramics10.2138/am-2020-7285 ↗
44. The system Na2O-Al2O3-Fc2O3-SiO2 at 1 atmosphere, and the petrogenesis of alkaline rocks10.1093/petrology/7.1.114 ↗
45. Morphological and structural investigations on iron borosilicate glasses10.4236/njgc.2017.72002 ↗
46. Magnetic nanoparticles with enhanced γ-Fe 2 O 3 to α-Fe 2 O 3 phase transition temperature10.1088/0957-4484/17/23/023 ↗
47. Property modification of a high level nuclear waste borosilicate glass through the addition of Fe2O3
48. Development of mica glass‐ceramic glazes10.1111/j.1551-2916.2004.00819.x ↗
49. Structure of borosilicate glassy materials with high concentrations of sodium, iron, and aluminum oxides10.1134/S1087659609030031 ↗
50. Raman spectra and structure of BaO·SiO2 SrO·SiO2 and CaO·SiO2 melts to 1600°C10.1016/0009-2541(94)00127-T ↗
51. Effect of Fe2O3 on the structure and properties of mo‐containing borosilicate glasses for nuclear waste immobilization10.1111/ijag.16680 ↗
52. Structural investigation of sodium borate glasses and melts by raman spectroscopy. II. Conversion between BO4 and BO2O− units at high temperature10.1016/S0022-3093(03)00159-5 ↗
53. Structural study of antimony borate glass system doped with transition metal ions using infrared and Raman spectroscopy10.4028/www.scientific.net/AMR.501.51 ↗
54. The environment of Fe3+/Fe2+ cations in a sodium borosilicate glass10.13036/17533562.58.3.016 ↗
55. Melting behaviour of simulated radioactive waste as functions of different redox iron-bearing raw materials10.1016/j.jnucmat.2022.153946 ↗
56. The effect of Fe on the structure and electrical conductivity of sodium borosilicate glasses10.1039/C7CP02042B ↗
57. Structural changes in borosilicate glasses as a function of Fe2O3 content: a multi-technique approach10.1016/j.jnoncrysol.2023.122664 ↗
58. Nuclear magnetic resonance and FTIR structural studies on borosilicate glasses containing iron oxide10.4236/njgc.2016.64006 ↗
59. Insights into the Iron- and phosphorus-induced structural rearrangements in sodium aluminoborosilicate glasses and their impact on melt rheology and crystallization behavior10.1021/acs.jpcc.2c06717 ↗
60. Effects of the iron content and redox state on the structure of sodium borosilicate glasses: a R aman, M össbauer and boron K‐edge XANES spectroscopy study10.1111/j.1551-2916.2011.05020.x ↗
61. Iron-induced structural rearrangements and their impact on sulfur solubility in borosilicate-based nuclear waste glasses10.1021/acs.jpcc.4c02085 ↗