Enhanced thermal and structural performance of mesophase pitch-based C/C-SiC composites via pyrolytic graphite matrix modification

Xiaodong He, Ting Ouyang, Dong Huang, Xiaoyan Hu, Huafeng Quan, Chong Ye, Jinshui Liu, Yudi Zhang

Ceramics International· Volume 51· Issue 11
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Fiber-reinforced polymer composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Innovative thermal management concepts and material solutions for future space vehicles10.2514/1.A33501 ↗
2. Application of a high thermal conductivity C/C composite in a heat-redistribution thermal protection system
3. Ceramic matrix composite (CMC) thermal protection systems (TPS) and hot structures for hypersonic vehicles
4. Thermal protection systems for space vehicles: a review on technology development, current challenges and future prospects10.1016/j.actaastro.2020.06.047 ↗
5. Evolution of mechanical and electromagnetic interference shielding properties of C/SiC during oxidation at 700 °C10.1016/j.carbon.2019.09.088 ↗
6. New large-scale production method for C/C-SiC ceramics: investigating the influence of chopped and nonwoven CF10.1016/j.ceramint.2018.10.095 ↗
7. Designable density defect influencing the mechanical property of 3D needled C/SiC composites10.1016/j.jallcom.2019.07.163 ↗
8. Ablation behavior and mechanism analysis of C/SiC composites10.1016/j.jmrt.2015.10.004 ↗
9. Numerical investigation of the thermal benefit of using a high thermal conductivity CMC for the leading edge of hypersonic vehicles
10. Thermal conductivity of textile reinforcements for composites
11. Construction of continuous heat conductive channel, a double harvest strategy to enhance thermal conductance and bending strength of C/SiC composites10.1016/j.jmst.2021.06.063 ↗
12. Effect of diamond content on microstructure and properties of C/SiC-diamond composites10.1016/j.diamond.2020.107902 ↗
13. Effects of graphite filler on the thermophysical properties of 3D C/SiC composites10.1016/j.jallcom.2018.08.223 ↗
14. Preparation and properties of C/SiC composites reinforced by high thermal conductivity graphite films10.1016/j.diamond.2021.108376 ↗
15. Thermophysical properties of three-dimensional ceramic-filler-modified carbon/carbon composites10.1016/j.ceramint.2018.10.015 ↗
16. Efficacy of a ZrB2–SiC matrix in protecting C fibres from oxidation in novel UHTCMC materials10.1016/j.matdes.2016.09.104 ↗
17. Ablation behavior and thermal conduction mechanism of 3D ZrC–SiC-modified carbon/carbon composite having high thermal conductivity using mesophase-pitch-based carbon fibers and pyrocarbon as heat transfer channels10.1016/j.compositesb.2021.109201 ↗
18. Mechanical, thermophysical, and ablation properties of C/HfC–SiC composites with various SiC/HfC ratios
19. Microstructure of high thermal conductivity mesophase pitch-based carbon fibers10.1016/S1872-5805(21)60050-1 ↗
20. Preparation and properties of highly thermal conductive C/C-SiC
21. Thermal conductivity and bending strength of SiC composites reinforced by pitch-based
22. Preparation and properties of the three-dimensional highly thermal conductive carbon/carbon-silicon carbide composite using the mesophase-pitch-based carbon fibers and pyrocarbon as thermal diffusion channels10.1016/j.jeurceramsoc.2021.03.011 ↗
23. Tensile properties of ultrahigh strength PAN-based, ultrahigh modulus pitch-based and high ductility pitch-based carbon fibers10.1016/j.carbon.2007.11.001 ↗
24. Large diameter carbon fibres from mesophase pitch10.1016/S0008-6223(02)00060-X ↗
25. Origin and effect of fiber attack for the processing of C/SiC
26. Development of UHTCMCs via water based ZrB2 powder slurry infiltration and polymer infiltration and pyrolysis10.1016/j.jeurceramsoc.2020.05.054 ↗
27. Ablation behavior of Cf/ZrC-SiC-based composites fabricated by an improved reactive melt infiltration10.1016/j.jeurceramsoc.2019.07.007 ↗
28. A global approach to fiber nD architectures and self‐sealing matrices: from Research to production10.1111/j.1744-7402.2005.02011.x ↗
29. The effect of Z-yarn density on the in-plane shear property of three-dimensional stitched carbon fiber reinforced silicon carbide composites10.1016/j.compscitech.2014.11.008 ↗
30. A reconsideration of the relationship between the crystallite size La of carbons determined by X-ray diffraction and Raman spectroscopy10.1016/j.carbon.2006.06.029 ↗
31. Raman microprobe studies on carbon materials10.1016/0008-6223(94)90148-1 ↗
32. Measurements of thermal conductivity and electrical conductivity of a single carbon fiber10.1023/A:1006674510648 ↗
33. The correlation of thermal conductivity with electrical resistivity in mcsophase pitch-based carbon fiber10.1016/0008-6223(93)90207-Q ↗
34. Indirect measurement of thermal conductivity of pitch-based carbon fibers
35. Kinetics of mesophase formation in a stirred tank reactor and properties of the products—II. Discontinuous reactor10.1016/0008-6223(92)90099-I ↗
36. Kinetics of mesophase formation of petroleum pitch10.1016/0008-6223(94)90054-X ↗
37. Production of monodisperse spherical mesophase from coal tar pitch by solvent extraction10.1007/s42823-023-00481-8 ↗
38. Mesophase from anthracene oil-based pitches10.1021/ef800499x ↗
39. Effects of fabrication processes on the properties of SiC/SiC composites10.1016/j.ceramint.2021.04.281 ↗
40. Fabrication and performance of micro-diamond modified C/SiC composites via precursor impregnation and pyrolysis process10.1016/j.ceramint.2018.02.185 ↗
41. Three-dimensional micro-pipelines high thermal conductive C/SiC composites10.1016/j.ceramint.2021.08.346 ↗
42. Optimized ablation resistance behavior and mechanism of C/SiC composites with high thermal conductive channels10.1111/jace.19281 ↗
43. Effect of positioning impregnation on the oxidation behaviour of Ti3SiC2/SiC functionally graded materials at 1400 °C10.1016/j.jallcom.2018.01.310 ↗