journal article·2025-06

Effects of high-temperature pre-oxidation treatment on the wave-absorbing properties of SiC fibers

Zelin Ye, Ruiying Luo, Lianyi Wang, Huiyong Yang, Zehao Ye, Jinsen Wang, Xiaohui Dong, Xiaotian Yang, Jiangshun Huang

Ceramics International· Volume 51· Issue 15
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Electromagnetic wave absorption materials · Glass properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. Excellent microwave absorbing and electromagnetic shielding performance of grown MWCNT on activated carbon bifunctional composite10.1016/j.carbon.2022.07.024 ↗
3. Effect and mechanism analysis of free carbon on the oxidation behavior of SiC fibers10.1016/j.ceramint.2023.08.227 ↗
4. Self-healing mechanisms of a SiC fiber reinforced multi-layered ceramic matrix composite in high pressure steam environments10.1016/j.jeurceramsoc.2006.06.007 ↗
5. Research advances in composition, structure and mechanisms of microwave absorbing materials10.1016/j.compositesb.2021.109173 ↗
6. Additive manufacturing of fiber reinforced ceramic matrix composites: advances, challenges, and prospects10.1016/j.ceramint.2022.04.146 ↗
7. Emerging continuous SiC fibers for high-temperature applications10.1016/j.ceramint.2024.06.100 ↗
8. Effects of SiC fibers on microwave absorption and electromagnetic interference shielding properties of SiCf/SiCN composites10.1016/j.ceramint.2016.09.089 ↗
9. Effect of heat treatment on interface failure behavior in SiCf/PyC/SiC composites reinforced with Cansas-3 fibers10.1016/j.ceramint.2024.05.108 ↗
10. Fabrication of scalable, aligned and low density carbon nanotube/silicon carbide hybrid foams by polysilazane infiltration and pyrolysis10.1016/j.jeurceramsoc.2020.12.035 ↗
11. Oxidation and mechanical properties of SiC fibers after high temperature exposure in air and steam10.1016/j.jeurceramsoc.2024.04.076 ↗
12. Effect of CVI SiC interphase on tensile properties of SiC fibers with different surfaces10.1016/j.vacuum.2023.112435 ↗
13. Synthesis, characterization and growth mechanism of SiC fibers10.1016/j.matchemphys.2022.126703 ↗
14. Evaluation of heat resistance of SiC-based ceramic fibers via in situ elastic modulus and electrical conductivity measurement at elevated temperatures10.1016/j.jeurceramsoc.2023.10.008 ↗
15. Texture control of pyrolytic carbon coatings and effects of coating thickness on the tensile properties of SiC fibers10.1016/j.matchemphys.2022.126234 ↗
16. Effect of long-time annealing at high temperature on the microstructure and mechanical properties of different types of SiC fibers10.1016/j.compositesa.2024.108291 ↗
17. In-situ TEM investigations on the microstructural evolution of SiC fibers under ion irradiation: amorphization and grain growth10.1016/j.jeurceramsoc.2022.11.029 ↗
18. The effect of deposition temperature of BN interphase on the tensile properties of SiC fibers10.1016/j.ceramint.2023.10.043 ↗
19. Effects of PyC coating on SiC fibers after ultra-high temperature annealing10.1016/j.ceramint.2021.11.234 ↗
20. Evolution of the structure and mechanical performance of Cansas-II SiC fibers after thermal treatment10.1016/j.ceramint.2021.06.144 ↗
21. The effect of temperature and atmospheric-pressure on mechanical and electrical properties of polymer-derived SiC fibers10.1016/j.oceram.2023.100431 ↗
22. Effects of the Ar flow rate on the composition, structure, and properties of near-stoichiometric SiC fibers that were annealed at 1600°C10.1016/j.ceramint.2022.05.101 ↗
23. Mechanical properties and microstructural evolution of Cansas-III SiC fibers after thermal exposure in different atmospheres10.1016/j.ceramint.2022.07.206 ↗
24. The effects of annealing atmosphere and intrinsic component on high temperature evolution behaviors of SiC fibers10.1016/j.msea.2022.143363 ↗
25. Effects of corrosion in liquid fluoride salt on the tensile strength of domestic SiC fibers10.1016/j.ceramint.2021.07.303 ↗
26. Microstructure and corrosion behavior of in-situ grown Y3Si2C2 coated SiC fibers exposed to air and wet-oxygen at 1400 °C10.1016/j.jeurceramsoc.2022.02.020 ↗
27. Structural evolution and mechanical properties of Cansas-III SiC fibers after thermal treatment up to 1700 °C10.1016/j.jeurceramsoc.2020.12.003 ↗
28. Evolution of microstructure and tensile strength of Cansas-II SiC fibers under air oxidizing atmosphere10.1016/j.jeurceramsoc.2021.07.067 ↗
29. Long-time oxidation behavior of the nearly stoichiometric polycrystalline SiC fibers under air atmosphere at different temperatures10.1016/j.jeurceramsoc.2024.01.001 ↗
30. Tuning dielectric and electromagnetic absorption properties of SiC fiber by in-situ grown polycrystalline carbon nanowires10.1016/j.matchemphys.2023.128793 ↗
31. Influence of fiber surface properties of SiCf/SiC composites on the interfacial debonding behavior10.1016/j.jeurceramsoc.2023.09.081 ↗
32. SiC fibers with different diameters exhibiting excellent high-temperature resistance and oxidation resistance10.1016/j.jmrt.2023.01.129 ↗
33. The fiber structure evolution and performance changes of SiC–ZrC fibers after 1600 °C heat treatment10.1016/j.ceramint.2023.09.109 ↗
34. An analytical model for the high temperature fracture strength of SiC fiber reinforced ceramic matrix composites considering oxidation and residual thermal stresses10.1016/j.compositesa.2023.107668 ↗
35. Oxidation embrittlement of SiC fibers at intermediate temperatures10.1016/j.jeurceramsoc.2024.01.066 ↗
36. Enhanced microwave absorbance of oxidized SiCf/AlPO4 composites via the formation of a carbon layer on the SiC fibre surface10.1016/j.jeurceramsoc.2018.05.038 ↗
37. The effects of phase interfaces in SmFeN/YSZ composite thermal barrier materials on electromagnetic wave-absorbing properties10.1016/j.ceramint.2024.05.059 ↗
38. Raman spectroscopy studies of the high-temperature evolution of the free carbon phase in polycarbosilane derived SiC ceramics10.1016/j.ceramint.2010.08.003 ↗
39. Measurement of interfacial residual stress in SiC fiber reinforced Ni-Cr-Al alloy composites by Raman spectroscopy10.1016/j.jmst.2018.09.023 ↗
40. Effects of the fiber surface characteristics on the interfacial microstructure and mechanical properties of the KD SiC fiber reinforced SiC matrix composites10.1016/j.msea.2009.07.018 ↗
41. Silicon carbide fiber manufacturing: cost and technology10.1016/j.compositesb.2023.111101 ↗
42. Fabrication of SiC fibers from yttrium-containing polycarbosilane10.1016/S1003-6326(11)61260-0 ↗
43. Low-pressure oxidation for improving interface properties and voltage instability of SiO2/4H-SiC MOS capacitor10.1016/j.apsusc.2024.161604 ↗
44. Oxidation behavior and mechanism of 4H-SiC surface by holes in electrochemical and photoelectrochemical systems10.1016/j.apsusc.2024.162010 ↗
45. Effects of thermal oxidation on microwave-absorbing and mechanical properties of SiCf/SiC composites with PyC interphase10.1016/S1003-6326(15)63749-9 ↗