journal article·2021-03

Effects of HfC/PyC core-shell structure nanowires on the microstructure and mechanical properties of Hf1-xZrxC coating

Jincui Ren, Yuting Duan, Chaofeng Lv, Jiyuan Luo, Yulei Zhang, Yanqin Fu

Ceramics International· Volume 47· Issue 6
Publisher page

Abstract

Abstract To elevate the mechanical and anti-ablation properties of Hf1-xZrxC coating on C/C composites, HfC/PyC core-shell structure nanowires (HfCnw/PyC) with different PyC layer thickness were synthesized by two steps of CVD. Influences of HfCnw/PyC on the microstructure and mechanical properties of Hf1-xZrxC coating were researched. Toughening mechanism of HfCnw/PyC was also investigated. PyC layer exhibited a lamellar structure and combined well with HfCnw. After incorporating HfCnw/PyC, Hf1-xZrxC coating structure converted from columnar crystal to isometric crystal. HfCnw improved H, E, Kc and bonding strength of Hf1-xZrxC coating, which is ascribed to the nanowire pullout, debonding, bridging and crack deflection mechanism. With the PyC layer thickness increasing, H and E of the coating reduced, Kc and bonding strength of the coating increased. Because of the moderate bonding strength between HfCnw/PyC and coating matrix, lamellar structure of PyC layer and higher Kc of PyC, toughening effectiveness of the core-shell structures gradually enhanced with the PyC layer thickness increasing.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Semiconductor materials and devices · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Mechanical enhancement of C/C composites via the formation of a machinable carbon nanofiber interphase10.1016/j.carbon.2007.10.040 ↗
2. Comparison of 2D and 3D carbon/carbon composites with respect to damage and fracture resistance10.1016/S0008-6223(02)00442-6 ↗
3. The role of CNT in improving the mechanical strength retention rate of C/C composites during heat treatment10.1016/j.compositesb.2020.107856 ↗
4. Self-generating high-temperature oxidation-resistant glass-ceramic coatings for C-C composites using UHTCs10.1111/jace.13017 ↗
5. Ablation behavior of nose-shaped HfB2-SiC modified carbon/carbon composites exposed to oxyacetylene torch10.1016/j.corsci.2019.02.015 ↗
6. Effect of combustion gas mass flow rate on carbon/carbon composite nozzle ablation in a solid rocket motor10.1016/j.carbon.2011.11.034 ↗
7. Fabrication of low-density carbon-bonded carbon fiber composites with an Hf-based coating for high temperature applications10.1039/C8RA01129J ↗
8. Ultra-high-temperature ceramic coatings for oxidation protection of carbon/carbon composites10.1111/j.1551-2916.2008.02331.x ↗
9. Design of a C/SiC functionally graded coating for the oxidation protection of C/C composites10.1016/j.carbon.2005.02.025 ↗
10. Ultrahigh temperature ceramic HfB2-SiC coating by liquid phase sintering method to protect carbon materials from oxidation10.1016/j.matchemphys.2018.07.018 ↗
11. Microstructure and ablation resistance of ZrCxNy-modified ZrC-SiC composite coating for carbon/carbon composites10.1016/j.jeurceramsoc.2018.05.043 ↗
12. Ablation behavior of HfC protective coatings for carbon/carbon composites in an oxyacetylene combustion flame10.1016/j.corsci.2012.08.064 ↗
13. Microstructure and growth behavior of Hf(Ta)C ceramic coating synthesized by low pressure chemical vapor deposition10.1016/j.jallcom.2017.02.101 ↗
14. Anti-oxidation modification behaviors and mechanisms of ZrB2 phase on Si-based ceramic coatings in aerobic environment with wider temperature region10.1016/j.jallcom.2018.07.300 ↗
15. Influence of the ZrB2 content on the anti-oxidation ability of ZrB2-SiC coatings in aerobic environments with broad temperature range10.1016/j.jeurceramsoc.2019.10.006 ↗
16. Microstructure and anti-ablation performance of HfC-TaC and HfC-ZrC coatings synthesized by CVD on C/C composites10.1016/j.ceramint.2020.01.006 ↗
17. Diffusion and solid solution formation between the binary carbides of TaC, HfC and ZrC10.1016/j.ijrmhm.2013.03.009 ↗
18. Microstructures and ablation resistance of WSi2/ZrSi2/ZrxHf1-xC/SiC coating based on a pattern strengthening one-step method10.1016/j.jeurceramsoc.2020.09.011 ↗
19. Oxidative protection of a carbon-bonded carbon fiber composite with double-layer coating of MoSi2-SiC whisker and TaSi2-MoSi2-SiC whisker by slurry method10.1016/j.ceramint.2017.04.140 ↗
20. HfC nanowire-toughened TaSi2-TaC-SiC-Si multiphase coating for C/C composites against oxidation10.1016/j.corsci.2014.10.048 ↗
21. UHTC coating reinforced by HfC nanowires against ablation for C/C composites10.1016/j.surfcoat.2017.01.014 ↗
22. Ablation resistance of HfC coating reinforced by HfC nanowires in cyclic ablation environment10.1016/j.jeurceramsoc.2017.02.057 ↗
23. Influence of HfC nanowires on the growth behavior, microstructure and ablation resistance of CVD-HfC coating10.1016/j.ceramint.2018.11.230 ↗
24. SiCnw/PyC core-shell networks to improve the bonding strength and oxyacetylene ablation resistance of ZrB2-ZrC coating for C/C-ZrB2-ZrC-SiC composites10.1016/j.carbon.2017.09.019 ↗
25. CNT–PyC–SiC/SiC double-layer oxidation-protection coating on C/C composite10.1016/j.carbon.2008.07.014 ↗
26. Single-crystal SiC nanowires with a thin carbon coating for stronger and tougher ceramic composites10.1002/adma.200500104 ↗
27. Influence of fiber coating thickness on microstructure and mechanical properties of carbon fiber-reinforced zirconium diboride based composites10.1016/j.ceramint.2013.07.040 ↗
28. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
29. SiC/SiC minicomposites with nanoscale multilayered fibre coatings10.1016/S0266-3538(00)00131-7 ↗
30. Mechanical properties of SiCf/SiC composites with PyC and the BN interface10.1016/j.ceramint.2015.02.041 ↗
31. Effect of interface type on the static and dynamic mechanical properties of 3D braided SiCf/SiC composites10.1016/j.msea.2016.05.080 ↗
32. Effect of PyC interphase thickness on mechanical behaviors of SiBC matrix modified C/SiC composites fabricated by reactive melt infiltration
33. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
34. Fracture toughness and crack morphologies in eroded WC-Co-Cr thermally sprayed coatings10.1016/S0167-577X(98)00092-5 ↗
35. Effects of deposition temperature and time on HfC nanowires synthesized by CVD on SiC-coated C/C composites10.1016/j.ceramint.2015.12.078 ↗
36. Microstructural investigations of the pyrocarbon interphase in SiC fiber-reinforced SiC matrix composites10.1016/j.matlet.2009.06.040 ↗
37. Magnetic susceptibility of solid solutions of hafnium and tantalum monocarbides
38. Hierarchical, seamless, edge-rich nanocarbon hybrid foams for highly efficient electromagnetic-interference shielding10.1016/j.jmst.2020.07.020 ↗
39. HfC/ZrC ablation protective coating for carbon/carbon composites10.1016/j.corsci.2013.06.042 ↗
40. Action mechanism of hydrogen gas on deposition of HfC coating using HfCl4-CH4-H2-Ar system10.1016/j.apsusc.2016.08.169 ↗
41. Effect of carbon nanotubes on the toughness, bonding strength and thermal shock resistance of SiC coating for C/C-ZrC-SiC composites10.1016/j.jallcom.2015.04.223 ↗